Polymer Property : Viscosity Test = 150 cm³/g Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Viscosity Test 150 cm³/g
150 cm³/g
Average value: 150 cm³/g Grade Count:3
Overview of materials for Nylon 6, Glass Filled, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu..
Viscosity Test 150 - 250 cm³/g
150 - 250 cm³/g
Average value: 203 cm³/g Grade Count:9
Overview of materials for Nylon 66/6
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb ..
Viscosity Test 150 - 205 cm³/g
150 - 205 cm³/g
Average value: 178 cm³/g Grade Count:4
Overview of materials for Nylon 66, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum ..
Viscosity Test 150 cm³/g
<br>@Temperature 30.0 °C
150 cm³/g
<br>@Temperature 86.0 °F
Inherent Viscosity in DMF Solution
Kureha KF Polymer 1550 High Viscosity PVDF Homopolymer
KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p..
Viscosity Test 150 cm³/g
150 cm³/g
H&lt;sub&gt;2&lt;/sub&gt;SO&lt;sub&gt;4&lt;/sub&gt;; ISO 307
Sax Polymers SAXAMID 126F4MW4 Nylon 6, 40% Glass Fiber and Mineral Reinforced
SAXAMID 126F4MW4 is a 40% glass fibers/ mineral reinforced polyamide 6 injection-molding-grade. It has dimensional stability and high strength.Information provided by SAX Polymers
Viscosity Test 150 cm³/g
150 cm³/g
H&lt;sub&gt;2&lt;/sub&gt;SO&lt;sub&gt;4&lt;/sub&gt;; ISO 307
Sax Polymers SAXAMID 126F6T3 Nylon 6, 30% Glass Fiber and PTFE
SAXAMID 126F6T3 is a polyamide 6 injection-molding-grade reinforced with 30% glass fibers and 15% PTFE. Because of its high strength and stiffness this grade is often used for stressed parts requiri..
Viscosity Test 150 cm³/g
150 cm³/g
H&lt;sub&gt;2&lt;/sub&gt;SO&lt;sub&gt;4&lt;/sub&gt;; ISO 307
Sax Polymers SAXAMID 126H Nylon 6, Injection Molding Grade
SAXAMID 126H is a general purpose polyamide 6 injection-molding-grade. Benefits are short cycle times and good release properties. Additionally it has a higher content of heat stabilizer which is p..
Viscosity Test 150 cm³/g
150 cm³/g
H&lt;sub&gt;2&lt;/sub&gt;SO&lt;sub&gt;4&lt;/sub&gt;; ISO 307
Sax Polymers SAXAMID 126K6 Nylon 6, 30% Glass Filled
SAXAMID 126K6 is a 30% glass beads filled polyamide 6 injection-molding-grade. It is characterized by dimensional stability, low warpage and good surface quality.Information provided by SAX Polymers..
Viscosity Test 150 cm³/g
150 cm³/g
H&lt;sub&gt;2&lt;/sub&gt;SO&lt;sub&gt;4&lt;/sub&gt;; ISO 307
Sax Polymers SAXAMID 136F3Q32 Nylon 6, 15% Glass Fiber
SAXAMID 136F3Q32 is a high-impact-modified polyamide 6 injection-molding-grade reinforced with 15% glass fibers with very high impact properties. Beside the high impact strength at low temperatures ..
Viscosity Test 150 cm³/g
150 cm³/g
H&lt;sub&gt;2&lt;/sub&gt;SO&lt;sub&gt;4&lt;/sub&gt;; ISO 307
Sax Polymers SAXAMID 226 Nylon 6.6
SAXAMID 226 is a general purpose polyamide 6.6 injection-molding-grade. Benefits are short cycle times and good release properties.Information provided by SAX Polymers
Viscosity Test 150 cm³/g
150 cm³/g
H&lt;sub&gt;2&lt;/sub&gt;SO&lt;sub&gt;4&lt;/sub&gt;; ISO 307
Sax Polymers SAXAMID 226F4 Nylon 6.6, 20% Glass Fiber
SAXAMID 226F4 is a polyamide 6.6 injection-molding-grade reinforced with 20% glass fibers.Information provided by SAX Polymers
Viscosity Test 150 cm³/g
150 cm³/g
H&lt;sub&gt;2&lt;/sub&gt;SO&lt;sub&gt;4&lt;/sub&gt;; ISO 307
Sax Polymers SAXAMID 226F4RY01 Nylon 6.6, 20% Glass Fiber
SAXAMID 226F4RY01 is a polyamide 6.6 injection-molding-grade reinforced with 20% glass fibers. It has a halogen-free flame retardant.Information provided by SAX Polymers
Viscosity Test 150 cm³/g
150 cm³/g
H&lt;sub&gt;2&lt;/sub&gt;SO&lt;sub&gt;4&lt;/sub&gt;; ISO 307
Sax Polymers SAXAMID 226F6RY01 Nylon 6.6, 30% Glass Fiber
SAXAMID 226F6RY01 is a polyamide 6.6 injection-molding-grade reinforced with 30% glass fibers. It has a halogen-free flame retardant.Information provided by SAX Polymers
Viscosity Test 150 cm³/g
150 cm³/g
H&lt;sub&gt;2&lt;/sub&gt;SO&lt;sub&gt;4&lt;/sub&gt;; ISO 307
Sax Polymers SAXAMID 226K6 Nylon 6.6, 30% Glass Beads
SAXAMID 226K6 is a polyamide 6.6 injection-molding-grade filled with 30% glass beads. It is characterized by optimized shrinkage properties.Information provided by SAX Polymers
Viscosity Test 150 cm³/g
150 cm³/g
H&lt;sub&gt;2&lt;/sub&gt;SO&lt;sub&gt;4&lt;/sub&gt;; ISO 307
Sax Polymers SAXAMID 126F2K4 Nylon 6, Glass Fiber/Bead Filled
SAXAMID 126F2K4 is a 10% glass fibers and 20% glass beads filled polyamide 6 injection-molding-grade.Information provided by SAX Polymers
Viscosity Test 150 cm³/g
150 cm³/g
H&lt;sub&gt;2&lt;/sub&gt;SO&lt;sub&gt;4&lt;/sub&gt;; ISO 307
Sax Polymers SAXAMID 126F3 Nylon 6, 15% Glass Fiber
SAXAMID 126F3 is a polyamide 6 injection-molding-grade reinforced with 15% glass fibers.Information provided by SAX Polymers
Viscosity Test 150 cm³/g
150 cm³/g
H&lt;sub&gt;2&lt;/sub&gt;SO&lt;sub&gt;4&lt;/sub&gt;; ISO 307
Sax Polymers SAXAMID 126F5 Nylon 6, 25% Glass Fiber
SAXAMID 126F5 is a polyamide 6 injection-molding-grade reinforced with 25% glass fibers.Information provided by SAX Polymers
Viscosity Test 150 cm³/g
150 cm³/g
H&lt;sub&gt;2&lt;/sub&gt;SO&lt;sub&gt;4&lt;/sub&gt;; ISO 307
Sax Polymers SAXAMID 226F5 Nylon 6.6, 25% Glass Fiber
SAXAMID 226F5 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 25% glass fibers. It has high mechanical strength in combination with good flow properties.Information provid..
Viscosity Test 150 cm³/g
150 cm³/g
DAM; ISO 307 1157 1628
DuPont Performance Polymers Minlon® 22C NC010 Nylon 66 &nbsp;(Unverified Data**)
38% Mineral/Glass Reinforced Polyamide 66 Minlon 22C NC010 is a 38% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polym..
Viscosity Test 150 cm³/g
150 cm³/g
DAM; ISO 307 1157 1628
DuPont Performance Polymers Zytel® 70G35HSRX BK099 Nylon 66 &nbsp;(Unverified Data**)
35% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G35HSRX BK099 a 35% glass reinforced heat stabilized hydrolysis resistant PA66 for injection molding. Developed for applications designed fo..
Viscosity Test 150 cm³/g
150 cm³/g
DAM; ISO 307 1157 1628
DuPont Performance Polymers Zytel® 73G30HSL NC010 Nylon 6 &nbsp;(Unverified Data**)
30% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G30HSL NC010 is a 30% glass fiber reinforced heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performan..
Viscosity Test 150 cm³/g
150 cm³/g
DAM; ISO 307 1157 1628
DuPont Performance Polymers Zytel® FG408L NC010 Nylon 66 &nbsp;(Unverified Data**)
Unreinforced Toughened Polyamide 66 with Developed for Food Contact Applications Zytel FG408L NC010 is a general purpose lubricated impact modified polyamide 66 resin with superior toughness for inj..
Viscosity Test 150 cm³/g
150 cm³/g
Viscosity Number; ISO 307, 1157, 1628
DSM EcoPaXX® Q150-D PA410
Low/Medium Viscosity
Viscosity Test 150 cm³/g
150 cm³/g
DAM; ISO 307 1157 1628
DuPont Performance Polymers Zytel® 70G13HS1L NC010 Nylon 66 &nbsp;(Unverified Data**)
13% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G13HS1L NC010 is a 13% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perfor..
Viscosity Test 150 cm³/g
150 cm³/g
0.5% in 96% H2SO4; ISO 307
Azoty Tarnow™ Alphalon™ 27 Nylon 6
A bright polyamide 6 grade of low viscosity suited for the production of carpet yarns.Information provided by ATT Polymers™
Viscosity Test 150 cm³/g
150 cm³/g
0.5% in 96% H2SO4; ISO 307
Azoty Tarnow™ Alphalon™ 27D Nylon 6
A bright polyamide 6 grade of low viscosity suited for the production of compounds.Information provided by ATT Polymers™
Viscosity Test 150 cm³/g
150 cm³/g
Viscosity number
BASF Ultramid® A27 E 01 PA66 (Dry)
Ultramid A27 E 01 is a low-viscosity, general-purpose PA66 grade for compounding. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendation "..
Viscosity Test 150 cm³/g
150 cm³/g
Viscosity number
BASF Ultramid® B3S Q661 PA6 (Dry)
Ultramid B3S Q661 is a general purpose, PA6 resin for injection molding.
Viscosity Test 150 cm³/g
150 cm³/g
Viscosity number; ISO 307
BASF Ultramid® B3K PA6 (Dry)
Ultramid B 3K is an easy flowing, stabilized for fast processing, grade of nylon 6.
Viscosity Test 150 cm³/g
150 cm³/g
DAM; ISO 307 1157 1628
DuPont Performance Polymers Zytel® 70G30HSL BK039B Nylon 66 &nbsp;(Unverified Data**)
30% Glass Reinforced Heat Stabilized Polyamide 66 Information provided by DuPont Performance Polymers