Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Storage Temperature = 25.0 °C Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Permabond ET500 Epoxy Resin
PERMABOND ET500 is a two-part fast-setting epoxy adhesive which bonds to a wide variety of substrates such as wood, metal, ceramics and some plastics and composites. It cures rapidly at room tempera..
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Permabond ET5401 Epoxy Resin
PERMABOND® ET5401 is a two-part, 2:1 mixable, semi-flexible toughened no slump epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and compo..
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Permabond HH131 High Temperature Threadlocker
Permabond® HH131 is a very high temperature resistant, high strength anaerobic threadlocker and sealant. This material cures in the absence of air between tight fitting metal parts. It is used for ..
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Permabond HH167 Anaerobic Retainer
Permabond® HH167 is a high viscosity gap filling silver paste, which can be used for repairing metal machinery parts. It is ideal for repairing worn shafts, broken threads, damaged keyways and spli..
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Permabond HM128 Anaerobic Threadlocker
Permabond® HM128 Threadlocker is a high strength adhesive for permanent assembly. It is typically used for preventing vibration loosening of bolts, studs and cap screws. Full cure to a cross-linked..
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Permabond HM165 Anaerobic Retainer
Permabond® HM165 is a high viscosity anaerobic retaining compound that cures when confined between metal parts to form a tough bond. It is best suited for cylindrical parts and where high temperatu..
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Permabond LH054 Anaerobic Threadsealant
Permabond® LH054 is an anaerobic curing, calibrated strength pipe sealant that allows for easier disassembly – especially of larger diameter pipes. It cures anaerobically when in contact with meta..
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Permabond LH056 Anaerobic Threadsealant
Permabond LH056 is a thread sealant designed for use in sealing metal pipes and fittings in sprinkler systems which may also contain CPVC piping. Permabond LH056 prevents leaks even on pipes that ar..
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Permabond LM113 Anaerobic Threadlocker
Permabond® LM113 Threadlocker is a medium viscosity product for locking small threaded fasteners, such as screws and bolts or hydraulic fittings that might require disassembly. Due to its thixotrop..
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Permabond UV640 UV-curable Adhesive
PERMABOND UV640 is a single part, fast setting, and UV curable adhesive designed specifically for bonding plastics. This material has excellent adhesion to a variety of plastics including polycarbon..
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Permabond UV649 UV-curable Adhesive
PERMABOND UV649 is a single part, fast setting, and UV curable adhesive designed specifically for bonding plastics. This material has excellent adhesion to a variety of plastics including polycarbon..
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Permabond UV7141 UV-curable Adhesive
Permabond UV7141 is a UV-curable adhesive with a secondary anaerobic cure mechanism. This makes it ideal for bonding materials such as ceramic-coated glass, mirrors, etc. where UV-light cannot penet..
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Victrex® Vicote® F804 Black Polyetheretherketone (PEEK) Liquid Dispersion
EVICOTE® is the brand name for the Victrex range of coatings. VICOTE Coatings are available through Victrex or its preferred coater network. VICOTE F804Blk has been specifically formulated to provi..
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Victrex® Vicote® F805 Polyetheretherketone (PEEK) Liquid Dispersion
The VICOTE F805 natural, F806 natural and F807Blk grades have been specifically formulated to provide a tough, resilient, high wear resistant coating with varying levels of lubricants on ferrous and..
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Victrex® Vicote® F806 Polyetheretherketone (PEEK) Liquid Dispersion
The VICOTE F805 natural, F806 natural and F807Blk grades have been specifically formulated to provide a tough, resilient, high wear resistant coating with varying levels of lubricants on ferrous and..
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Victrex® Vicote® F808 Polyetheretherketone (PEEK) Liquid Dispersion
The VICOTE F808 natural, F809 natural and F810Blk grades have been specifically formulated to provide a resilient coating with high wear and abrasion resistance combined with excellent release prope..
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Permabond F201 Anaerobic Retainer
Permabond® F201 is an anaerobic adhesive which has been developed to give excellent resistance to peel and impact forces. This toughening, combined with good adhesion to aluminum and copper alloys,..
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Permabond MM115 Anaerobic Threadlocker
Permabond® MM115 Threadlocker is an excellent general purpose threadlocker and sealant. It is used for locking metal bolts, nuts and screws that may require disassembly for service and maintenance...
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Permabond MM115P Pure Anaerobic Threadlocker
Permabond® MM115 PURE Threadlocker is an excellent general purpose threadlocker and sealant. It is used for locking metal bolts, nuts and screws that may require disassembly for service and mainten..
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Permabond TA4246 Toughened Acrylic Adhesive
PERMABOND® TA4246 is a 2-part, no-mix, room temperature curing structural adhesive. It is ideal for use on a wide variety of substrate materials and forms a very high strength structural bond with ..
Storage Temperature 15.0 - 25.0 °C
59.0 - 77.0 °F
Lubrizol Advanced Materials Pearlbond® D1160 Thermoplastic Polyurethane
Pearlbondâ„¢ D1160 is a linear, aromatic polyurethane, supplied in form of small white granules, which combines a high crystallization rate and high thermoplasticity level. Applications: Pearlbo..
Storage Temperature 0.000 - 25.0 °C
32.0 - 77.0 °F
Akzo Nobel Trigonox® C-C75 Polymerization Initiator
Initiator for the (co)polymerization of ethylene, styrene, acrylonitrile, acrylates and methacrylates.Chemical Description: tert-Butyl peroxybenzoate, 75% solution in odorless mineral spiritsCAS Num..
Storage Temperature 10.0 - 25.0 °C
50.0 - 77.0 °F
Akzo Nobel Trigonox® C Polymerization Initiator
Initiator for the (co)polymerization of ethylene, styrene, acrylonitrile, vinylacetate, acrylates and methacrylates. Trigonox C is a monofunctional peroxide which is used for the crosslinking of pol..
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Permabond A011 Anaerobic Threadlocker
Permabond® A011 is an anaerobic adhesive designed for locking and sealing threaded or coaxially fitting metal parts where subsequent dismantling is required. Its controlled strength ensures fatigue..
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Permabond A025 Anaerobic Retainer
Permabond® A025 is an anaerobic adhesive formulated to provide permanent locking and sealing of metal parts such as bearings, gears, studs and other threaded components. It has been designed for ap..
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Permabond HM135 Anaerobic Retainer
Permabond® HM135 is a fast curing, medium viscosity anaerobic adhesive for locking and sealing threads and retaining cylindrical components. It gives maximum torque strength on brass or plated bras..
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Permabond MH052 Anaerobic Threadsealant
Permabond® MH052 is ideal for the sealing of threaded joints. It is approved for use with natural gas and LPG for working pressure up to 20 bar (290 psi) and also for gaseous oxygen up to 10 bar (1..
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Victrex® Vicote® F815 Polyetheretherketone (PEEK) Liquid Dispersion
VICOTE® is the brand name for the Victrex range of coatings. VICOTE Coatings are available through Victrex or its preferred coater network. The VICOTE F815 and F816Blk grades have been specificall..
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Permabond A134 Anaerobic Retainer
Permabond® A134 is a high-strength anaerobic product designed for the permanent locking and sealing of metal parts. Its 'non-drip' formulation makes it suitable for use on larger fittings, coarse t..
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Victrex® Vicote® F810 Black Polyetheretherketone (PEEK) Liquid Dispersion
Eco-friendly VICOTE Coatings were developed to fill the performance gap found in many existing coating technologies today. Whether applied to industrial, automotive, food processing, semiconductor, ..
Copyright © lookpolymers.com All Rights Reserved