| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Storage Temperature | 4.44 - 29.4 °C | 40.0 - 85.0 °F | |
|
Aremco Corr-Paint™ CP3015-BL High Temperature Protective Coating Inorganic, Mixed Oxides Filled
These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. High emissivity, inorganic black pigmented coating to 15..
|
|||
| Storage Temperature | 4.44 - 29.4 °C | 40.0 - 85.0 °F | |
|
Aremco Corr-Paint™ CP3015-GR High Temperature Protective Coating Inorganic, Mixed Oxides Filled
These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. Gray-ceramic inorganic coating to 1400°F.
|
|||
| Storage Temperature | 4.44 - 29.4 °C | 40.0 - 85.0 °F | |
|
Aremco Corr-Paint™ CP3015-SS High Temperature Protective Coating Inorganic, Mixed Oxides Filled
These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. Stainless steel filled, inorganic coating to 1400°F.
|
|||
| Storage Temperature | 4.44 - 29.4 °C | 40.0 - 85.0 °F | |
|
Aremco Corr-Paint™ CP3015-WH High Temperature Protective Coating Inorganic, Mixed Oxides Filled
These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. White-ceramic inorganic coating to 1500°F.
|
|||
| Storage Temperature | 12.8 - 29.4 °C | 55.0 - 85.0 °F | |
|
Aremco Corr-Paint™ CP4000 High Temperature Protective Silicone Coating, Metal Oxide Filled
This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a..
|
|||
| Storage Temperature | 12.8 - 29.4 °C | 55.0 - 85.0 °F | |
|
Aremco Corr-Paint™ CP4050 High Temperature Protective Coating Silicone
Low viscosity, green coating for power resistors to 1100°F (593°C)
|
|||
| Storage Temperature | 12.8 - 29.4 °C | 55.0 - 85.0 °F | |
|
Aremco Corr-Paint™ CP4060 High Temperature Protective Coating Silicone, Aluminum Filled
This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a..
|
|||
| Storage Temperature | 12.8 - 29.4 °C | 55.0 - 85.0 °F | |
|
Aremco Corr-Paint™ CP4080 High Temperature Protective Coating Silicone, Aluminum Filled
This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a..
|
|||
| Storage Temperature | 12.8 - 29.4 °C | 55.0 - 85.0 °F | |
|
Aremco Corr-Paint™ CP4090 High Temperature Protective Coating Silicone, Aluminum Filled
This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a..
|
|||
| Storage Temperature | 12.8 - 29.4 °C | 55.0 - 85.0 °F | |
|
Aremco Corr-Paint™ CP5000 High Temperature Protective Coating Inorganic, Zinc Filled
CP5000 is a two part, water-based, inorganic zinc rich primer which provides superior resistance to salt-fog, immersion, impact and abrasion. This primer system is compatible with all CP-Series prod..
|
|||
| Storage Temperature | 12.8 - 29.4 °C | 55.0 - 85.0 °F | |
|
Aremco Quartz-Coat™ 845 High Temperature Ceramic-Inorganic Coating
Single part, waterborne, silicon-filled, phosphate-bonded, brown-black coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps..
|
|||
| Storage Temperature | 12.8 - 29.4 °C | 55.0 - 85.0 °F | |
|
Aremco Aremco-Seal™ 4030 High Temperature Specialty Coatings Silicone, Ceramic Filled
Translucent-white, low-viscosity sealer for porous materials to 900°F (482°C)
|
|||
| Storage Temperature | 12.8 - 29.4 °C | 55.0 - 85.0 °F | |
|
Aremco Ceramacoat™ 845-BLK High Temperature Ceramic-Inorganic Coating
Single part, waterborne, silicon-filled, phosphate-bonded, Jet Black coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, s..
|
|||
| Storage Temperature | 12.8 - 29.4 °C | 55.0 - 85.0 °F | |
|
Aremco Ceramacoat™ 845-BLU High Temperature Ceramic-Inorganic Coating
Single part, waterborne, silicon-filled, phosphate-bonded, blue coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, stadiu..
|
|||
| Storage Temperature | 12.8 - 29.4 °C | 55.0 - 85.0 °F | |
|
Aremco Ceramacoat™ 845-GDK High Temperature Ceramic-Inorganic Coating
Single part, waterborne, silicon-filled, phosphate-bonded, dark green coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, ..
|
|||
| Storage Temperature | 12.8 - 29.4 °C | 55.0 - 85.0 °F | |
|
Aremco Ceramacoat™ 845-GLT High Temperature Ceramic-Inorganic Coating
Single part, waterborne, silicon-filled, phosphate-bonded, light-green coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps,..
|
|||
| Storage Temperature | 12.8 - 29.4 °C | 55.0 - 85.0 °F | |
|
Aremco Ceramacoat™ 845-GRY High Temperature Ceramic-Inorganic Coating
Single part, waterborne, silicon-filled, phosphate-bonded, gray coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, stadiu..
|
|||
| Storage Temperature | 12.8 - 29.4 °C | 55.0 - 85.0 °F | |
|
Aremco Ceramacoat™ 845-SIL High Temperature Ceramic-Inorganic Coating
Single part, waterborne, silicon-filled, phosphate-bonded, matte silver coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps..
|
|||
| Storage Temperature | 12.8 - 29.4 °C | 55.0 - 85.0 °F | |
|
Aremco Ceramacoat™ 845-WHT High Temperature Ceramic-Inorganic Coating
Single part, waterborne, silicon-filled, phosphate-bonded, white coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, stadi..
|
|||
| Storage Temperature | 12.8 - 29.4 °C | 55.0 - 85.0 °F | |
|
Aremco Cerama-Dip™ 538-N High Temperature Specialty Ceramic-Inorganic Coating
Low viscosity, light gray coating for powder resistors and rheostats to 2600°F (1427°C). black and green pigments also available.
|
|||
| Storage Temperature | 4.44 - 29.4 °C | 40.0 - 85.0 °F | |
|
Aremco Corr-Paint™ CP3015-AL High Temperature Protective Coating Inorganic, Mixed Oxides Filled
These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. Aluminum-ceramic filled coating to 1200°F.
|
|||
| Storage Temperature | 12.8 - 29.4 °C | 55.0 - 85.0 °F | |
|
Aremco Corr-Paint™ CP4010 High Temperature Protective Silicone Coating, Aluminum Filled
Single part, silicone-based, low viscosity, heat-curable, aluminum-filled sealer offering exceptional moisture resistance to 1100°F (593°C).
|
|||
| Storage Temperature | 12.8 - 29.4 °C | 55.0 - 85.0 °F | |
|
Aremco Corr-Paint™ CP4020 High Temperature Protective Coating Silicone, Aluminum Filled
This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4010 adheres to metals, ceramics, refractories, and quartz, a..
|
|||
| Storage Temperature | 12.8 - 29.4 °C | 55.0 - 85.0 °F | |
|
Aremco Corr-Paint™ CP4040 High Temperature Protective Coating Silicone
Low viscosity, white coating for motor windings to 1100°F (593°C)
|
|||
| Storage Temperature | 12.8 - 29.4 °C | 55.0 - 85.0 °F | |
|
Aremco Corr-Paint™ CP4070 High Temperature Protective Coating Silicone, Aluminum Filled
This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a..
|
|||
| Storage Temperature | 12.8 - 29.4 °C | 55.0 - 85.0 °F | |
|
Aremco Corr-Paint™ CP4095 High Temperature Protective Coating Silicone, Aluminum Filled
This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a..
|
|||