| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Storage Temperature | 2.00 - 7.00 °C | 35.6 - 44.6 °F | |
|
Permabond 101 Cyanoacrylate, Wicking Viscosity
PERMABOND® 101 is a low viscosity product useful in wicking or penetrating applications or bonding closely fitting parts. It is fast setting and suitable for use on plastics, rubber and metals. Cya..
|
|||
| Storage Temperature | 2.00 - 7.00 °C | 35.6 - 44.6 °F | |
|
Permabond 105 Cyanoacrylate, for difficult rubbers
PERMABOND® 105 is a low viscosity high purity cyanoacrylate adhesive. It is ideal for use on hard-to-bond plastics and rubbers such as natural rubber, EPDM and butyl rubber. Cyanoacrylate adhesives..
|
|||
| Storage Temperature | 2.00 - 7.00 °C | 35.6 - 44.6 °F | |
|
Permabond 170 Cyanoacrylate, gap filling
PERMABOND® 170 is a methyl cyanoacrylate adhesive. It is a single part, high viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. Permabond 170 w..
|
|||
| Storage Temperature | 2.00 - 7.00 °C | 35.6 - 44.6 °F | |
|
Permabond 2010 Cyanoacrylate, gap filling
PERMABOND 200 is a high viscosity product with good flow control useful in wire tacking applications or bonding components. It is fast setting and suitable for use on plastics, rubber and metals. Cy..
|
|||
| Storage Temperature | 2.00 - 7.00 °C | 35.6 - 44.6 °F | |
|
Permabond 2011 Cyanoacrylate, gel
PERMABOND® 2011 is a thixotropic, fast-setting cyanoacrylate particularly suitable for use on vertical and porous substrates. This material can be used on metals, plastics, elastomers, ceramics and..
|
|||
| Storage Temperature | 2.00 - 7.00 °C | 35.6 - 44.6 °F | |
|
Permabond 2050 Cyanoacrylate, flexible
PERMABOND® 2050 is a flexible cyanoacrylate adhesive, exhibiting improved peel strengths when compared to other grades. It has excellent impact and vibration resistance, and is suitable for bonding..
|
|||
| Storage Temperature | 2.00 - 7.00 °C | 35.6 - 44.6 °F | |
|
Permabond 268 Cyanoacrylate, General purpose
PERMABOND® 268 is a medium-high viscosity cyanoacrylate for large gap fill applications. Permabond® 268 provides faster set times and improved gap-filling capability compared to conventional cyano..
|
|||
| Storage Temperature | 2.00 - 7.00 °C | 35.6 - 44.6 °F | |
|
Permabond 737 Cyanoacrylate, toughened
PERMABOND® 737 is a toughened cyanoacrylate with improved impact and peel strength for maximum flexibility. Its increased temperature resistance and dark color make 737 suitable for a wide range of..
|
|||
| Storage Temperature | 2.00 - 7.00 °C | 35.6 - 44.6 °F | |
|
Permabond 738 Cyanoacrylate, toughened
PERMABOND 738 is a toughened cyanoacrylate with improved impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable over..
|
|||
| Storage Temperature | 2.00 - 7.00 °C | 35.6 - 44.6 °F | |
|
Permabond 940 Cyanoacrylate, low odor
PERMABOND 940 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad..
|
|||
| Storage Temperature | 2.00 - 7.00 °C | 35.6 - 44.6 °F | |
|
Permabond ES550 Epoxy Resin
PERMABOND ES550 is a single-part epoxy paste which is slump-resistant (does not flow) during cure. The adhesive is toughened for maximum impact resistance, along with excellent peel and shear streng..
|
|||
| Storage Temperature | 2.00 - 7.00 °C | 35.6 - 44.6 °F | |
|
Permabond ES562 Epoxy Resin
PERMABOND® ES562 is a single-part epoxy adhesive which flows like solder when heated during curing. The adhesive has excellent adhesion to metal surfaces and composites. The high bond strength of t..
|
|||
| Storage Temperature | 2.00 - 7.00 °C | 35.6 - 44.6 °F | |
|
Permabond ES578 Epoxy Resin
PERMABOND® ES578 is a single-part heat cured epoxy adhesive with excellent adhesion to metal surfaces, ceramics as well as composite materials. ES578 provides excellent thermal conductivity and bon..
|
|||
| Storage Temperature | 2.00 - 7.00 °C | 35.6 - 44.6 °F | |
|
Permabond TA4202 Toughened Acrylic Adhesive
PERMABOND® TA4202 is a 2-part, 1:1 toughened acrylic adhesive. It can be used to bond a wide variety of materials including metals, plastics, GRP, ceramics, wood and other substrates. It is conveni..
|
|||
| Storage Temperature | 2.00 - 7.00 °C | 35.6 - 44.6 °F | |
|
Permabond TA4300 Toughened Acrylic Adhesive
PERMABOND® TA4300 is a 2-part, 1:1 toughened acrylic adhesive. Its toughening makes it ideal for bonding dissimilar materials where differential thermal expansion and contraction could be an issue...
|
|||
| Storage Temperature | 2.00 - 7.00 °C | 35.6 - 44.6 °F | |
|
Permabond TA4310 Toughened Acrylic Adhesive
PERMABOND® TA4310 is a 2-part, 1:1 toughened acrylic adhesive. Its toughening makes it ideal for bonding dissimilar materials where differential thermal expansion and contraction could be an issue...
|
|||
| Storage Temperature | 2.00 - 7.00 °C | 35.6 - 44.6 °F | |
|
Permabond 240 Cyanoacrylate, gap filling
PERMABOND® 240 is a high viscosity product useful in large gap applications. It is ideal for porous substrates. It is fast setting and suitable for use on plastics, rubber and metals. Cyanoacrylate..
|
|||
| Storage Temperature | 2.00 - 7.00 °C | 35.6 - 44.6 °F | |
|
Permabond 260 Cyanoacrylate
PERMABOND 260 is a low viscosity cyanoacrylate ideal for wicking type application. PERMABOND 260 provides faster set times and improved gap-filling capability compared to conventional cyanoacrylates..
|
|||
| Storage Temperature | 2.00 - 7.00 °C | 35.6 - 44.6 °F | |
|
Permabond 265 Cyanoacrylate
PERMABOND 265 is a medium viscosity cyanoacrylate ideal for intermediate gap fill application. PERMABOND 265 provides faster set times and improved gap-filling capability compared to conventional cy..
|
|||
| Storage Temperature | 2.00 - 7.00 °C | 35.6 - 44.6 °F | |
|
Permabond 791 Cyanoacrylate, Surface insensitive
PERMABOND® 791 is a low viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastomers ar..
|
|||
| Storage Temperature | 2.00 - 7.00 °C | 35.6 - 44.6 °F | |
|
Permabond 799 Cyanoacrylate, Surface insensitive
PERMABOND® 799 is a high viscosity cyanoacrylate that combines fast cure with the ability to cure through a large gap. Plastics, metals, ceramics and elastomers are also rapidly bonded. The fast cu..
|
|||
| Storage Temperature | 2.00 - 7.00 °C | 35.6 - 44.6 °F | |
|
Permabond 801 Cyanoacrylate, High Temperature
PERMABOND® 801 is a low viscosity modified ethyl cyanoacrylate suitable for applications where high temperature resistance is required. This material is fast setting and has good adhesion to rubber..
|
|||
| Storage Temperature | 2.00 - 7.00 °C | 35.6 - 44.6 °F | |
|
Permabond 919 Cyanoacrylate, High temperature
Features & Benefits: Rapid development of high strength; Ease of use – no mixing or heat cure; Bonds most materials; 100% reactive, no solvents.PERMABOND® 919 is an allyl cyanoacrylate adhesive. I..
|
|||
| Storage Temperature | 2.00 - 7.00 °C | 35.6 - 44.6 °F | |
|
Permabond 930 Cyanoacrylate
PERMABOND 930 is a low odor, nonfogging, nonfrosting cyanoacrylate. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate adhesives on hot and humid days, is eliminated. The ..
|
|||
| Storage Temperature | 2.00 - 7.00 °C | 35.6 - 44.6 °F | |
|
Permabond ES569 Epoxy Resin
PERMABOND® ES569 is a single-part heat cured epoxy adhesive with excellent adhesion to metal surfaces as well as composite materials. The high bond strength of this adhesive allows it to replace me..
|
|||
| Storage Temperature | 2.00 - 7.00 °C | 35.6 - 44.6 °F | |
|
Permabond TA4302 Toughened Acrylic Adhesive
PERMABOND® TA4302 is a 2-part, 1:1 toughened acrylic adhesive. It can be used to bond a wide variety of materials including metals, plastics, GRP, ceramics, wood and other substrates. It is conveni..
|
|||
| Storage Temperature | 2.00 - 7.00 °C | 35.6 - 44.6 °F | |
|
Permabond 792 Cyanoacrylate, Surface insensitive
PERMABOND® 792 is a low viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastomers ar..
|
|||
| Storage Temperature | 2.00 - 7.00 °C | 35.6 - 44.6 °F | |
|
Permabond 943 Cyanoacrylate, low odor
PERMABOND 943 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad..
|
|||
| Storage Temperature | 2.00 - 7.00 °C | 35.6 - 44.6 °F | |
|
Permabond 262 Cyanoacrylate
PERMABOND 262 is a low viscosity cyanoacrylate ideal for wicking type application. PERMABOND 262 provides faster set times and improved gap-filling capability compared to conventional cyanoacrylates..
|
|||
| Storage Temperature | 2.00 - 7.00 °C | 35.6 - 44.6 °F | |
|
Permabond 947 Cyanoacrylate, low odor
PERMABOND 947 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad..
|
|||