Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Storage Temperature = 40.0 °C Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Storage Temperature 0.000 - 40.0 °C
32.0 - 104 °F
Silikony Polskie Polsil Gum 100/40 HTV Silicone Rubber
Polsil Gum is a general purpose master batch compound, vulcanizing at high temperature after addition of vulcanizing agent. Silicone rubber obtained from Polsil® GUM shows useful properties: agei..
Storage Temperature 0.000 - 40.0 °C
32.0 - 104 °F
Silikony Polskie Polsil Gum 100/50 HTV Silicone Rubber
Polsil Gum is a general purpose master batch compound, vulcanizing at high temperature after addition of vulcanizing agent. Silicone rubber obtained from Polsil® GUM shows useful properties: agei..
Storage Temperature 0.000 - 40.0 °C
32.0 - 104 °F
Silikony Polskie Polsil Gum 100/60 HTV Silicone Rubber
Polsil Gum is a general purpose master batch compound, vulcanizing at high temperature after addition of vulcanizing agent. Silicone rubber obtained from Polsil® GUM shows useful properties: agei..
Storage Temperature 0.000 - 40.0 °C
32.0 - 104 °F
Silikony Polskie Polsil Gum 410/30 HTV Silicone Rubber
Polsil Gum is a general purpose master batch compound, vulcanizing at high temperature after addition of vulcanizing agent. Silicone rubber obtained from Polsil® GUM shows useful properties: agei..
Storage Temperature 10.0 - 40.0 °C
50.0 - 104 °F
Akzo Nobel Trigonox® 301 Polymerization Initiator
Initiator for the production of controlled rheology polypropylene (CR-PP).Chemical description: 3,6,9-Triethyl-3,6,9-trimethyl-1,4,7-triperoxonane, 41% solution in isoparaffinic hydrocarbonsCAS Numb..
Storage Temperature 0.000 - 40.0 °C
32.0 - 104 °F
Akzo Nobel Trigonox® A-W70 Polymerization Initiator
Initiator for the (co)polymerization of styrene, acrylonitrile, vinylchloride, vinylidenechloride, acrylates and methacrylates. Trigonox A-W70 may also be used as an initiator for the room temperatu..
Storage Temperature -30.0 - 40.0 °C
-22.0 - 104 °F
Akzo Nobel Trigonox® B-C50 Polymerization Initiator
Initiator for the (co)polymerization of ethylene.Chemical Description: Di-tert-butyl peroxide, 50% solution in odorless mineral spirits CAS Number: 110-05-4Acronym: DTBP; Tx BInformation provided by..
Storage Temperature 10.0 - 40.0 °C
50.0 - 104 °F
Akzo Nobel Trigonox® T Polymerization Initiator
Initiator for the (co)polymerization of ethylene, styrene, acrylates and methacrylates. Trigonox T may also be used for the crosslinking of polyolefins as well as natural rubber and synthetic rubber..
Storage Temperature 0.000 - 40.0 °C
32.0 - 104 °F
Akzo Nobel Trigonox® A-80 Polymerization Initiator
Initiator for the (co)polymerization of styrene, butadiene, acrylonitrile, acrylates and methacrylates.Chemical Description: tert-Butyl hydroperoxide, 80% solution in waterCAS Number: 75-91-2Acronym..
Storage Temperature -30.0 - 40.0 °C
-22.0 - 104 °F
Akzo Nobel Trigonox® B Polymerization Initiator
Initiator for the (co)polymerization of ethylene, styrene, acrylates and methacrylates. Trigonox B is a monofunctional peroxide which is used for the crosslinking of polyolefins as well as natural r..
Storage Temperature -30.0 - 40.0 °C
-22.0 - 104 °F
Akzo Nobel Trigonox® K-80 Polymerization Initiator
Initiator for the (co)polymerization of styrene, butadiene, acrylonitrile, vinylacetate, acrylates and methacrylates. Trigonox K-80 may also be used for the room temperature cure of promoted unsatur..
Storage Temperature 0.000 - 40.0 °C
32.0 - 104 °F
Silikony Polskie Polsil Gum 213/60 HTV Silicone Rubber
Polsil Gum is a general purpose master batch compound, vulcanizing at high temperature after addition of vulcanizing agent. Silicone rubber obtained from Polsil® GUM shows useful properties: ageing..
Copyright © lookpolymers.com All Rights Reserved