| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Storage Temperature | 0.000 - 30.0 °C | 32.0 - 86.0 °F | |
|
Silikony Polskie Polimer MV 0.07 Methylvinylsilicone Gum
POLIMER MV is the main starting material for production of HTV silicone rubber. Methylvinylsilicone gum should be compounded with crosslinking agents (peroxides), fillers and other additives. Methyl..
|
|||
| Storage Temperature | 0.000 - 30.0 °C | 32.0 - 86.0 °F | |
|
Silikony Polskie Polimer MV 1.0 Methylvinylsilicone Gum
POLIMER MV is the main starting material for production of HTV silicone rubber. Methylvinylsilicone gum should be compounded with crosslinking agents (peroxides), fillers and other additives. Methyl..
|
|||
| Storage Temperature | 5.00 - 30.0 °C | 41.0 - 86.0 °F | |
|
Silikony Polskie Polsil E5S Silicone Emulsion
POLSIL® E – water emulsions of POLSIL® OM methylsilicone fluid. These are milky-white liquids easily mixed with water, smooth to touch, with a specific smell. They are chemically inert. ..
|
|||
| Storage Temperature | 5.00 - 30.0 °C | 41.0 - 86.0 °F | |
|
Silikony Polskie Polsil E1 Silicone Emulsion
POLSIL® E – water emulsions of POLSIL® OM methylsilicone fluid. These are milky-white liquids easily mixed with water, smooth to touch, with a specific smell. They are chemically inert. ..
|
|||
| Storage Temperature | 5.00 - 30.0 °C | 41.0 - 86.0 °F | |
|
Silikony Polskie Polsil E2 Silicone Emulsion
POLSIL® E – water emulsions of POLSIL® OM methylsilicone fluid. These are milky-white liquids easily mixed with water, smooth to touch, with a specific smell. They are chemically inert. ..
|
|||
| Storage Temperature | 5.00 - 30.0 °C | 41.0 - 86.0 °F | |
|
Silikony Polskie Polsil E3 Silicone Emulsion
POLSIL® E – water emulsions of POLSIL® OM methylsilicone fluid. These are milky-white liquids easily mixed with water, smooth to touch, with a specific smell. They are chemically inert. ..
|
|||
| Storage Temperature | 5.00 - 30.0 °C | 41.0 - 86.0 °F | |
|
Silikony Polskie Polsil E5 Silicone Emulsion
POLSIL® E – water emulsions of POLSIL® OM methylsilicone fluid. These are milky-white liquids easily mixed with water, smooth to touch, with a specific smell. They are chemically inert. ..
|
|||
| Storage Temperature | 23.0 - 30.0 °C | 73.4 - 86.0 °F | |
|
Chengdu Polyster 10 LPI Lenticular Lens Sheet, Acrylic
10 LPI lenticular lens sheet has wider viewing range. It is of high impact resistance and UV resistance. It has been specially designed for outdoor billboards, signboards and shop displays. The sui..
|
|||
| Storage Temperature | 23.0 - 30.0 °C | 73.4 - 86.0 °F | |
|
Chengdu Polyster 10 LPI Lenticular Lens Sheet, PS
10 LPI lenticular lens sheet has wider viewing range. It is of high impact resistance and UV resistance. It has been specially designed for outdoor billboards, signboards and shop displays. The sui..
|
|||
| Storage Temperature | 23.0 - 30.0 °C | 73.4 - 86.0 °F | |
|
Chengdu Polyster 100 LPI Lenticular Lens Sheet, APET
Good for ink adhesion. The image is sharp and clear. It is specially designed for advertisement and packaging with high definition and clearness requirement. The suitable graphic effects: flip, 3D, ..
|
|||
| Storage Temperature | 23.0 - 30.0 °C | 73.4 - 86.0 °F | |
|
Chengdu Polyster 161 LPI Lenticular Lens Sheet, APET
Good for ink adhesion. The image is sharp and clear. It is specially designed for advertisement and packaging with high definition and clearness requirement. The suitable graphic effects: flip, 3D, ..
|
|||
| Storage Temperature | 23.0 - 30.0 °C | 73.4 - 86.0 °F | |
|
Chengdu Polyster 161 LPI Lenticular Lens Sheet, PP
Good for ink adhesion. The image is sharp and clear. It is specially designed for advertisement and packaging with high definition and clearness requirement. The suitable graphic effects: flip, 3D, ..
|
|||
| Storage Temperature | 23.0 - 30.0 °C | 73.4 - 86.0 °F | |
|
Chengdu Polyster 20 LPI Lenticular Lens Sheet, Acrylic
The image printed by this sheet material is being separated into layers clearly. It has the 3D effect, and has high UV resistance. It has been designed for posters, outdoor billboards, signboards, ..
|
|||
| Storage Temperature | 23.0 - 30.0 °C | 73.4 - 86.0 °F | |
|
Chengdu Polyster 20 LPI Lenticular Lens Sheet, PS
The image printed by this sheet material is being separated into layers clearly. It has the 3D effect, and has high UV resistance. It has been designed for posters, outdoor billboards, signboards, ..
|
|||
| Storage Temperature | 23.0 - 30.0 °C | 73.4 - 86.0 °F | |
|
Chengdu Polyster 70 LPI Lenticular Lens Sheet, APET
Specially designed for advertisement. It is used for posters, billboards, etc. The suitable graphic effects: flip, 3D, animation, morph, zoom, etc.Information provided by Chengdu Polyster Co., Ltd.
|
|||
| Storage Temperature | 23.0 - 30.0 °C | 73.4 - 86.0 °F | |
|
Chengdu Polyster 70 LPI Lenticular Lens Sheet, PP
Specially designed for advertisement. It is used for posters, billboards, etc. The suitable graphic effects: flip, 3D, animation, morph, zoom, etc.Information provided by Chengdu Polyster Co., Ltd.
|
|||
| Storage Temperature | 23.0 - 30.0 °C | 73.4 - 86.0 °F | |
|
Chengdu Polyster 75 LPI Lenticular Lens Sheet, APET
The thickness is moderate. It is good for ink adhesion, and specially designed for advertisement and packing. It is one of the lenticular lens sheets used widely, such as packaging bags, gift boxes,..
|
|||
| Storage Temperature | 23.0 - 30.0 °C | 73.4 - 86.0 °F | |
|
Chengdu Polyster 75 LPI Lenticular Lens Sheet, PP
The thickness is moderate. It is good for ink adhesion, and specially designed for advertisement and packing. It is one of the lenticular lens sheets used widely, such as packaging bags, gift boxes,..
|
|||
| Storage Temperature | 23.0 - 30.0 °C | 73.4 - 86.0 °F | |
|
Chengdu Polyster PET Film PET Films/Sheets
High transparency, is specially manufactured for thermoforming products and printing products. It is suitable for the packaging of foods, cosmetics, medicines and other products, and it is also used..
|
|||
| Storage Temperature | 23.0 - 30.0 °C | 73.4 - 86.0 °F | |
|
Chengdu Polyster PP Film PP Films/Sheets
High transparency, is specially manufactured for thermoforming products and printing products. It is suitable for the packaging of foods, cosmetics, medicines and other products, and it is also used..
|
|||
| Storage Temperature | -25.0 - 30.0 °C | -13.0 - 86.0 °F | |
|
Akzo Nobel Trigonox® M-55 Polymerization Initiator
Initiator for the (co)polymerization of styrene, butadiene, acrylonitrile, acrylates and methacrylates. Chemical Description: Isopropylcumyl hydroperoxide, 55% solution in diisopropylbenzeneCAS Numb..
|
|||
| Storage Temperature | 5.00 - 30.0 °C | 41.0 - 86.0 °F | No freezing |
|
3M Dyneon™ PFA 6910GZ Fluoroplastic Dispersion
3M™ Dyneon™ PFA 6910GZ is a 50% solids fluorothermoplastic aqueous dispersion. It is a copolymer of tetrafluoroethylene and perfluorinated comonomers, with a melt viscosity several orders of magni..
|
|||
| Storage Temperature | 5.00 - 30.0 °C | 41.0 - 86.0 °F | Frost-free |
|
3M Dyneon™ TF 5050Z PTFE
Because of its special particle size distribution, 3M™ Dyneon™ PTFE TF 5050Z is particularly good for producing aqueous non-stick coating systems, which can be used to coat suitably prepared metal..
|
|||
| Storage Temperature | 12.8 - 30.0 °C | 55.0 - 86.0 °F | |
|
Aremco Cerama-Dip™ 538-N-BLK High Temperature Specialty Ceramic-Inorganic Coating
Low viscosity, light gray coating for powder resistors and rheostats to 2600°F (1427°C). black and green pigments also available.
|
|||
| Storage Temperature | 12.8 - 30.0 °C | 55.0 - 86.0 °F | |
|
Aremco Cerama-Dip™ 538-N-GRN High Temperature Specialty Ceramic-Inorganic Coating
Low viscosity, light gray coating for powder resistors and rheostats to 2600°F (1427°C). black and green pigments also available.
|
|||