Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage, Flow = 0.018 in/in Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.018 cm/cm
<br>@Thickness 2.00 mm
0.018 in/in
<br>@Thickness 0.0787 in
ISO 294-4
DuPont Performance Polymers Delrin® 100TL NC010 Acetal Homopolymer &nbsp;(Unverified Data**)
Delrin® 100TL NC010 is a high viscosity acetal homopolymer with 1.5% Teflon® PTFE Micropowder.Information provided by DuPont Performance Polymers
Linear Mold Shrinkage, Flow 0.018 cm/cm
<br>@Thickness 2.00 mm
0.018 in/in
<br>@Thickness 0.0787 in
ISO 294-4
DuPont Performance Polymers Delrin® 500AL NC010 Acetal Homopolymer &nbsp;(Unverified Data**)
Delrin® 500AL is a medium viscosity acetal homopolymer, with an advanced system of lubrication for applications requiring low wear and/or coefficient of friction against steel, itself or other plas..
Linear Mold Shrinkage, Flow 0.018 cm/cm
<br>@Time 86400 sec
0.018 in/in
<br>@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP IL004 PA 6/12
LNP* LUBRICOMP* IL004 is a compound based on Nylon 6/12 resin containing 20% PTFE. Added features of this material include: Wear Resistant.
Linear Mold Shrinkage, Flow 0.018 cm/cm
<br>@Time 86400 sec
0.018 in/in
<br>@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP IL004 PA 6/12 (Asia Pacific)
LNP* Lubricomp* IL004 is a compound based on Nylon 6/12 resin containing PTFE. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Flow 0.018 - 0.020 cm/cm
<br>@Time 86400 sec
0.018 - 0.020 in/in
<br>@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP RB008 PA 66 (Asia Pacific)
LNP THERMOCOMP* RB008 is a compound based on Nylon 66 resin containing Glass Bead.
Linear Mold Shrinkage, Flow 0.018 - 0.020 cm/cm
<br>@Time 86400 sec
0.018 - 0.020 in/in
<br>@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP RB008 PA 66 (Asia Pacific)
LNP THERMOCOMP* RB008 is a compound based on Nylon 66 resin containing Glass Bead.
Linear Mold Shrinkage, Flow 0.018 cm/cm
<br>@Time 86400 sec
0.018 in/in
<br>@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-LOY K3000SZ Acetal Copoly
LNP* STAT-LOY* K3000SZ is a compound based on Acetal Copolymer resin. Added feature of this material is: AntiSstatic.
Linear Mold Shrinkage, Flow 0.018 cm/cm
<br>@Time 86400 sec
0.018 in/in
<br>@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-LOY K3000SZ Acetal Copoly (Asia Pacific)
LNP* Stat-loy* K3000SZ is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat.
Linear Mold Shrinkage, Flow 0.018 cm/cm
<br>@Time 86400 sec
0.018 in/in
<br>@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-LOY K3000Z Acetal
LNP* STAT-LOY* K3000Z is a compound based on unfilled Acetal resin. Added feature of this material is: Antistat.
Linear Mold Shrinkage, Flow 0.018 - 0.020 cm/cm
<br>@Time 86400 sec
0.018 - 0.020 in/in
<br>@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP RB008 PA 66
LNP THERMOCOMP* RB008 is a compound based on Nylon 66 resin containing 40% Glass Bead.
Linear Mold Shrinkage, Flow 0.018 - 0.020 cm/cm
<br>@Time 86400 sec
0.018 - 0.020 in/in
<br>@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP RB008 PA 66
LNP THERMOCOMP* RB008 is a compound based on Nylon 66 resin containing 40% Glass Bead.
Linear Mold Shrinkage, Flow 0.018 cm/cm
<br>@Thickness 3.20 mm
0.018 in/in
<br>@Thickness 0.126 in
DAM
DuPont Performance Polymers Zytel® ST811HS NC010 Nylon 6 &nbsp;(Unverified Data**)
Zytel® ST811HS is a flexible, heat stabilized Super Tough polyamide 6 resin developed for extrusion and injection molding applications such as cable and rope jacketing, hose inner cores and fastene..
Linear Mold Shrinkage, Flow 0.018 cm/cm
<br>@Thickness 2.00 mm
0.018 in/in
<br>@Thickness 0.0787 in
DAM; ISO 294-4
DuPont Performance Polymers Zytel® ST811HS NC010 Nylon 6 &nbsp;(Unverified Data**)
Zytel® ST811HS is a flexible, heat stabilized Super Tough polyamide 6 resin developed for extrusion and injection molding applications such as cable and rope jacketing, hose inner cores and fastene..
Linear Mold Shrinkage, Flow 0.018 - 0.021 cm/cm
<br>@Thickness 4.00 mm
0.018 - 0.021 in/in
<br>@Thickness 0.157 in
Parallel, 24h; ISO 294-4
DuPont Performance Polymers Delrin® 111P NC010 Acetal Homopolymer
Delrin® 111P is a high viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, fewer voids). It has higher tensile strength and mod..
Linear Mold Shrinkage, Flow 0.018 cm/cm
<br>@Thickness 2.00 mm
0.018 in/in
<br>@Thickness 0.0787 in
ISO 294-4
DuPont Performance Polymers Delrin® FG100TL NC010 Acetal Homopolymer &nbsp;(Unverified Data**)
Delrin® 100TL is a high viscosity acetal homopolymer, containing 1.5% Teflon® PTFE Micropowder. It has been developed for consideration into applications such as parts for the food industry.Inform..
Copyright © lookpolymers.com All Rights Reserved