Polymer Property : Linear Mold Shrinkage, Flow = 0.019 in/in Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.017 - 0.019 cm/cm
<br>@Time 86400 sec
0.017 - 0.019 in/in
<br>@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP IL004 PA 6/12
LNP* LUBRICOMP* IL004 is a compound based on Nylon 6/12 resin containing 20% PTFE. Added features of this material include: Wear Resistant.
Linear Mold Shrinkage, Flow 0.017 - 0.019 cm/cm
<br>@Time 86400 sec
0.017 - 0.019 in/in
<br>@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP IL004 PA 6/12 (Asia Pacific)
LNP* Lubricomp* IL004 is a compound based on Nylon 6/12 resin containing PTFE. Added features of this material include: Internally Lubricated.