Mechanical Properties Metric English Comments
Tensile Strength 8.96 MPa

@Strain 100 %
1300 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Wire & Cable JAL110A Natural Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength 8.96 MPa
1300 psi
ASTM D638
Quadrant EPP Fluorosint® 135 PTFE and PPS Blend, with Proprietary Lubrication Fillers (ASTM Product Data Sheet)
Chemical resistance parallels PTFE Continuous use temperatures to 500°F (260°C) Compared to PTFE higher load carrying capability 1/9 of the deformation under load lower coefficient of thermal exp..
Tensile Strength 8.96 MPa

@Strain 100 %
1300 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible A8001 Polyvinyl Chloride, Flexible (PVC, Flexible)
Recommended for interior applications.Information provided by PolyOne
Tensile Strength 8.96 MPa

@Strain 100 %
1300 psi

@Strain 100 %
510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible B8503 Polyvinyl Chloride, Flexible (PVC, Flexible)
A flexible PVC Compound with good resistance to migration to specific applications.Information provided by PolyOne
Tensile Strength 8.96 MPa

@Strain 100 %
1300 psi

@Strain 100 %
510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible C9000 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength 8.96 MPa

@Strain 100 %
1300 psi

@Strain 100 %
510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible C90A0 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength 8.96 MPa

@Strain 100 %
1300 psi

@Strain 100 %
510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible C90B1 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength 8.96 MPa

@Strain 100 %
1300 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible C90UB Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength 8.96 MPa
1300 psi
Typical
Garlock 2102 C.I. SBR/NBR Sheet Rubber, Polyester Insert
Garlock cloth-inserted materials are designed to add stability where mechanical fastening is necessary, and to reduce gasket creep where heavy flange loading is required.Style #2102 C.I. is a smooth..
Tensile Strength 8.96 MPa
1300 psi
Typical
Garlock 2103 C.I. SBR/NBR Sheet Rubber, Polyester Insert
Garlock cloth-inserted materials are designed to add stability where mechanical fastening is necessary, and to reduce gasket creep where heavy flange loading is required.Style #2103 C.I. is a smooth..
Tensile Strength 8.96 MPa
1300 psi
Typical
Garlock Viton® 501 Fluoroelastomer Sheet Rubber
Style #501 sheet rubber, made with VITON® fluoroelastomer, is a high-performance product resistant to heat, oils, fuels, numerous acids and other chemicals.Information provided by Garlock Rubber ..
Tensile Strength 8.96 MPa
1300 psi
ASTM D638
Ineos A60-70-162 HDPE
Ineos A60-70-162 is a high density polyethylene homopolymer, developed specifically for blow molding food containers on reciprocating screw-type equipment. It exhibits excellent processing character..
Tensile Strength 8.96 MPa
1300 psi
Typical values on polymer compression molded at 350ºF; ASTM D412
Kraton® D4158 K (O/E SBS) Radial Copolymer
Description: Kraton D4158 K is an oiled, radial copolymer based on styrene and butadiene with a polystyrene content of 31%. It is supplied from North America in the physical form: Kraton D4158 KT - ..
Tensile Strength 8.96 MPa
1300 psi
Teknor Apex Elexar® EL 1934D Thermoplastic Elastomer
Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical prop..
Tensile Strength 8.96 MPa
1300 psi
Teknor Apex Elexar® EL 1934C Thermoplastic Elastomer
Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical prop..
Tensile Strength 8.96 MPa
1300 psi
Teknor Apex Elexar® EL 1934F Thermoplastic Elastomer
Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical prop..
Tensile Strength 8.96 MPa
1300 psi
Teknor Apex Elexar® EL 1934G Thermoplastic Elastomer
Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical prop..
Tensile Strength 8.96 MPa
1300 psi
Teknor Apex Tekbond® TB 2005 Thermoplastic Elastomer
Notes: Tekbond® TPEs are a functional series of elastomer compounds designed to not only bond to the most difficult neat and reinforced engineering substrates with no primer or surface treatment, b..
Tensile Strength 8.96 MPa
1300 psi
Silicone; ASTM D412
Arlon 25662T010 0.010" (0.254 mm) Cured Silicone Rubber with Laminated ETFE Film Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Laminated ETFE FilmChemical Compatibility: (ETFE offers good chemical resistance to the following classes of chemicals) Alkalis, Organic a..
Tensile Strength 8.96 MPa
1300 psi
Silicone Property; ASTM D412
Arlon 30400N060 0.060" (1.52 mm) Uncured Silicone Rubber
Design/Construction: Interleave 1: KodacelProduct: Uncured Silicone Rubber Interleave 2: Polyethylene Appearance: Translucent silicone rubber on polymer linerThis data represents typical values for ..
Tensile Strength 8.96 MPa
1300 psi
Silicone Property; ASTM D412
Arlon 99790N010 0.010" (0.254 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Design/Construction: Liner: FEP Side 1: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassThis data represents typical values for the production material. The data should not be used to write,..
Tensile Strength 8.96 MPa
1300 psi
Compound Property
Arlon R34020W062 0.062" (1.57 mm) Uncured, Unsupported Silicone Rubber on a Kodacel Carrier
Design/Construction:Side 1: Uncured, Unsupported Silicone Rubber on a Kodacel Carrier This data Represents typical values for the production material. The data should not be used to write, or in pla..
Tensile Strength 8.96 MPa
1300 psi
Silicone Property; ASTM D412
Arlon 32400N030 0.030" (0.762 mm) Uncured Silicone Rubber on PET Carrier
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PET Appearance: Translucent silicone rubber on polymer linerThis data represents typical values for the productio..
Tensile Strength 8.96 MPa
1300 psi
Silicone Property; ASTM D412
Arlon 32400N060 0.060" (1.52 mm) Uncured Silicone Rubber
Design/Construction: Interleave 1: PET carrierSide 1: Uncured Silicone RubberInterleave 2 : PE carrierAppearance: Translucent silicone rubber on polymer linerThis data represents typical values for ..
Tensile Strength 8.96 MPa
1300 psi
Silicone Property; ASTM D412
Arlon R36613N022 0.022" (0.559 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 7628 Heat Cleaned FiberglassSide 2: Cured Silicone RubberSide 2 Interleave: PolyethyleneFiberglas Weave: PlainThis data represents..
Tensile Strength 8.96 MPa
1300 psi
Silicone Property; ASTM D412
Arlon R36812T010 0.010" Cured Silicone Rubber with Laminated ETFE Film Substrate
Design/Construction:Liner: N/ASide 1: Cured Silicone RubberSubstrate: Laminated ETFE FilmChemical Compatibility: Alkalis, Organic and Inorganic acids, Amines, Epoxies, Aromatic compounds, Chlorin..
Tensile Strength 8.96 MPa
1300 psi
Silicone Property; ASTM D412
Arlon R37223N008 0.008" (0.203 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 1653 Heat Cleaned Fiberglass ScrimSide 2: Cured Silicone RubberFiberglass Scrim Weave: LenoThis data represents typical values for..