| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength | >= 9.00 MPa | >= 1310 psi | Type IV, 500mm/min; ISO 37 |
|
S&E Specialty Polymers XP44-10MG PVC
Description: PVC weatherable, integral colored, filledApplication: Body side end cap molding compound which meets the GMP.PVC.002 & GMP.PVC.014.Information provided by S&E Specialty Polymers
|
|||
| Tensile Strength | 9.00 MPa | 1310 psi | ISO 37 |
|
Termopol Termoton® V6GA3075A TPV Compound
Termoton®V, TPV compounds with a dynamically cured EPDM phase closely dispersed in a polyolefin phase (PP). Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable;..
|
|||
| Tensile Strength | 9.00 MPa | 1310 psi | |
|
Momentive Performance Materials Addisilâ„¢ 482 E Healthcare Extrusion Grade Heat Cured Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
|
|||
| Tensile Strength | 9.00 MPa | 1310 psi | |
|
Momentive Performance Materials Siloprenâ„¢ Electro 242-3 Electrically Insulating Liquid Silicone Rubber
This LSR elastomer is an electrically insulating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate..
|
|||
| Tensile Strength | 9.00 MPa | 1310 psi | |
|
Momentive Performance Materials Siloprenâ„¢ LIM 6040 Liquid Silicone Rubber - Fast Cure / High Tear
This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera..
|
|||
| Tensile Strength | 9.00 MPa | 1310 psi | |
|
Momentive Performance Materials Siloprenâ„¢ LIM 6045 Liquid Silicone Rubber - Fast Cure / High Tear
This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera..
|
|||
| Tensile Strength | 9.00 MPa | 1310 psi | |
|
Momentive Performance Materials Siloprenâ„¢ LSR 2070 Liquid Silicone Rubber - General Purpose
This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera..
|
|||
| Tensile Strength | 9.00 MPa | 1310 psi | |
|
Momentive Performance Materials Siloprenâ„¢ LSR 2641 Liquid Silicone Rubber - Non Post Cure / Low Compression Set
This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera..
|
|||
| Tensile Strength | 9.00 MPa | 1310 psi | |
|
Momentive Performance Materials Siloprenâ„¢ LSR 2660 Liquid Silicone Rubber - Fast Cure / High Tear
This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera..
|
|||
| Tensile Strength | 9.00 MPa | 1310 psi | |
|
Momentive Performance Materials Siloprenâ„¢ LSR 2671 Liquid Silicone Rubber - Non Post Cure / Low Compression Set
This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera..
|
|||
| Tensile Strength | 9.00 MPa | 1310 psi | |
|
Momentive Performance Materials Siloprenâ„¢ LSR 3186/50 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set
This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time..
|
|||
| Tensile Strength | 9.00 MPa | 1310 psi | |
|
Momentive Performance Materials Siloprenâ„¢ LSR 4040 Liquid Silicone Rubber - Healthcare
LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding ..
|
|||
| Tensile Strength | 9.00 MPa | 1310 psi | |
|
Momentive Performance Materials Siloprenâ„¢ LSR 4070 Liquid Silicone Rubber - Healthcare
LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding ..
|
|||
| Tensile Strength | 9.00 MPa | 1310 psi | |
|
Momentive Performance Materials Siloprenâ„¢ LSR 4660 Liquid Silicone Rubber - Healthcare
LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding ..
|
|||
| Tensile Strength | 9.00 MPa | 1310 psi | |
|
Momentive Performance Materials Silplusâ„¢ 30 HS High Strength Heat Cured Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
|
|||
| Tensile Strength | 9.00 MPa | 1310 psi | |
|
Momentive Performance Materials Silplusâ„¢ 40 MP Heat Cured Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
|
|||
| Tensile Strength | 9.00 MPa | 1310 psi | |
|
Momentive Performance Materials Siloprenâ„¢ LSR 3485/35 Liquid Silicone Rubber - Self-Lubricating / Standard
This LSR elastomer is a self-lubricating, standard, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at eleva..
|
|||
| Tensile Strength | 9.00 MPa | 1310 psi | |
|
Momentive Performance Materials Siloprenâ„¢ LSR 3486/35 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set
This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time..
|
|||
| Tensile Strength | 9.00 MPa | 1310 psi | |
|
Shin-Etsu Silicones LIMSâ„¢ KE2090-40AB Elastomer
KE-2090-40 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is lo..
|
|||
| Tensile Strength | 9.03 MPa | 1310 psi | ASTM D412 |
|
Teknor Apex Telcar® OBC 4975A Thermoplastic Elastomer
Notes: Telcar OBC has superior mechanical strength and higher elongation which will provide a tougher more durable finished product. Telcar OBC can be used in less demanding sealing applications. T..
|
|||
| Tensile Strength |
9.00
MPa @Strain 20.0 % |
1310
psi @Strain 20.0 % |
ISO 37 |
|
BASF Elastollan 1198 A TPUR
Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi..
|
|||
| Tensile Strength | >= 9.00 MPa | >= 1310 psi | Type IV, 500mm/min; ISO 37 |
|
S&E Specialty Polymers XP11-289A1MG PVC
Description: PVC weatherable, integral colored, filledApplications: Body side end cap molding compound which meets GMW16084 Type 4, Grade I, Class B, GMP.PVC.002.Information provided by S&E Specialt..
|
|||