| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength | 207 MPa | 30000 psi | ASTM D638 |
|
PlastiComp Complet® LBF40-PA66 40% Long Basalt Fiber
This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc.
|
|||
| Tensile Strength | 207 MPa | 30000 psi | ASTM D-638 |
|
PlastiComp Complet® LCF30-PEI Polyetherimide, 30% Long Carbon Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyetherimide with 30% long carbon fiber reinforcementInformation provided by PlastiC..
|
|||
| Tensile Strength | 207 MPa | 30000 psi | ASTM D-638 |
|
PlastiComp Complet® LGF40 - PA66 MT Nylon 66, 40% Long Glass Fiber Reinforced, Impact Modified
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 40% long glass fiber reinforcementImpact modifiedInformation provided by..
|
|||
| Tensile Strength | 207 MPa | 30000 psi | ASTM D638 |
|
PlastiComp Complet® LGF40-PA66 MT 40% Long Glass Fiber
This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc.
|
|||
| Tensile Strength | 207 MPa | 30000 psi | MD, supporting material; ASTM D882 |
|
Rogers Corporation Poron® 4701-30-20 Supported Urethane Foam, Very Soft, Supported with Clear Polyester Film
Very soft, easily compressed for use where flexibility is a key requirement. Contains PET film reinforcement.Features and Benefits of PORON Products: Excellent compression set resistance which ena..
|
|||
| Tensile Strength | 207 MPa | 30000 psi | MD, supporting material; ASTM D882 |
|
Rogers Corporation Poron® 4701-30-20064 P Urethane Foam, Very Soft, Supported with Clear Polyester Film
Very soft, easily compressed for use where flexibility is a key requirement. Contains PET film reinforcement. Standard available thickness 0.064"Features and Benefits of PORON Products: Excelle..
|
|||
| Tensile Strength | 207 MPa | 30000 psi | MD, supporting material; ASTM D882 |
|
Rogers Corporation Poron® 4701-30-25037 P Urethane Foam, Very Soft, Supported with Clear Polyester Film
Very soft, easily compressed for use where flexibility is a key requirement. Standard available thickness range from 0.021"Features and Benefits of PORON Products: Excellent compression set resi..
|
|||
| Tensile Strength | 207 MPa | 30000 psi | MD, supporting material; ASTM D882 |
|
Rogers Corporation Poron® 4701-30-25047 P Urethane Foam, Very Soft, Supported with Clear Polyester Film
Very soft, easily compressed for use where flexibility is a key requirement. Standard available thickness range from 0.021"Features and Benefits of PORON Products: Excellent compression set resi..
|
|||
| Tensile Strength | 207 MPa | 30000 psi | MD, supporting material; ASTM D882 |
|
Rogers Corporation Poron® 4701-50 Supported Urethane Foam, Firm, PET Supported
Firm material used for managing high energy impact with gasketing needs. Standard available thickness range from 0.012" to 0.500" (0.30 mm to 12.7 mm).Features and Benefits of PORON Products: Exce..
|
|||
| Tensile Strength | 207 MPa | 30000 psi | MD, supporting material; ASTM D882 |
|
Rogers Corporation Poron® 4790-92-09 Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced
Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression ..
|
|||
| Tensile Strength | 207 MPa | 30000 psi | MD, Supporting material; ASTM D882 |
|
Rogers Corporation Poron® 4790-92-12 P Series Urethane Foam, Extra Soft, Slow Rebound, PET Film Reinforced
Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression ..
|
|||
| Tensile Strength | 207 MPa | 30000 psi | MD, supporting material; ASTM D882 |
|
Rogers Corporation Poron® 4790-92-15 Supported Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced
Extra soft, slow rebound with a very low closure force.Features and Benefits of PORON Products: Excellent compression set resistance which enables durable, long-term performance for gasketing, seali..
|
|||
| Tensile Strength | 207 MPa | 30000 psi | MD, supporting material; ASTM D882 |
|
Rogers Corporation Poron® 4790-92-20 Supported Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced
Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression ..
|
|||
| Tensile Strength | 207 MPa | 30000 psi | MD, supporting material; ASTM D882 |
|
Rogers Corporation Poron® 4790-92-30012 P Urethane Foam, Extra Soft, Slow Rebound, PET Film Reinforced
Extra soft, slow rebound with a very low closure force. Available with thickness of 0.012" (0.30 mm).Features and Benefits of PORON Products: Excellent compression set resistance which enables dura..
|
|||
| Tensile Strength | 207 MPa | 30000 psi | ASTM D-638 |
|
PlastiComp Complet® LGF40 - TPU Rigid Thermoplastic Polyurethane, 40% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 40% long glass fiber reinforcementInformation provided by Plas..
|
|||
| Tensile Strength | 207 MPa | 30000 psi | MD, supporting material; ASTM D882 |
|
Rogers Corporation Poron® 4701-30-25 Supported Urethane Foam, Very Soft, Supported with Clear Polyester Film
Very soft, easily compressed for use where flexibility is a key requirement. Contains PET film reinforcement.Features and Benefits of PORON Products: Excellent compression set resistance which enab..
|
|||
| Tensile Strength | 207 MPa | 30000 psi | MD, supporting material; ASTM D882 |
|
Rogers Corporation Poron® 4790-92-25 Supported Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced
Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression ..
|
|||