| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength |
6.55
MPa @Strain 100 % |
950
psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
|
PolyOne Geon™ HC 2175 Polyvinyl Chloride, Flexible (PVC, Flexible)
Geon HC 2175 is a 75 Shore A non-phthalate flexible vinyl compound made from FDA sanctioned ingredients. HC 2175 can be used for extrusion and injection molding healthcare applications.NOTE: All ing..
|
|||
| Tensile Strength |
6.55
MPa @Strain 100 % |
950
psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
|
PolyOne Geon™ Vinyl Flexible XV3683 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
|
|||
| Tensile Strength |
6.55
MPa @Strain 100 % |
950
psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
|
PolyOne Geon™ Vinyl Flexible XV3785 Polyvinyl Chloride, Flexible (PVC, Flexible)
All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high ..
|
|||
| Tensile Strength | 6.55 MPa | 950 psi | ASTM D412-98 |
|
Saint-Gobain Tygon® Norprene® A-60-N Drinking Water Tubing Formulation.
Formulated for use as drinking water tubing. Complies with FDA and NSF61 criteria.Information provided by Saint Gobain Performance Products.
|
|||
| Tensile Strength | 6.55 MPa | 950 psi | ASTM D412 |
|
Teknor Apex Telcar® OBC 2419B Thermoplastic Elastomer
Notes: Telcar OBC has superior mechanical strength and higher elongation which will provide a tougher more durable finished product. Telcar OBC can be used in less demanding sealing applications. T..
|
|||
| Tensile Strength | 6.55 MPa | 950 psi | Silicone Property; ASTM D412 |
|
Arlon 18596R026 0.026" (0.66 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: 11523 Style FiberglassSide 2: Uncured Silicone RubberInterleave: PolyethyleneThis data represents typical values for the production materi..
|
|||
| Tensile Strength | 6.55 MPa | 950 psi | Side 2; ASTM D412 |
|
Arlon 19586R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: 1523 Style FiberglassSide 2: Uncured Silicone RubberThis data represents typical values for the production mat..
|
|||
| Tensile Strength | 6.55 MPa | 950 psi | Silicone Property; ASTM D412 |
|
Arlon 32580B035 0.035" (0.889 mm) Uncured Silicone Rubber on PET Carrier
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PETThis data represents typical values for the production material. The data should not be used to write, or in p..
|
|||
| Tensile Strength | 6.55 MPa | 950 psi | Silicone Property; ASTM D412 |
|
Arlon 32580R035 0.035" (0.889 mm) Uncured Silicone Rubber on PET Carrier
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PETAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. ..
|
|||
| Tensile Strength | 6.55 MPa | 950 psi | Side 2, Silicone Property; ASTM D412 |
|
Arlon 51586R015 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Appearance: Red silicone gum and rubber on fiberglass clot..
|
|||
| Tensile Strength | 6.55 MPa | 950 psi | Side 2, Silicone Property; ASTM D412 |
|
Arlon 51586R015H 0.016" (0.406 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene This data represents typical values for the production mat..
|
|||
| Tensile Strength | 6.55 MPa | 950 psi | Silicone Property; ASTM D412 |
|
Arlon 51581R028 0.028" (0.711 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave 2: Polyethylene Appearance: Red silicone gu..
|
|||
| Tensile Strength | 6.55 MPa | 950 psi | Side 2, Silicone Property; ASTM D412 |
|
Arlon 51586R052 0.052" (1.32 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Appearance: Red silicone gum and rubber on fiberglass clothInterleave: Polyethylene..
|
|||
| Tensile Strength | 6.55 MPa | 950 psi | Side 1, Silicone Property; ASTM D412 |
|
Arlon 51588R019 0.019" (0.483 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2, Layer 1: Cured Silicone RubberSide 2, Layer 2: Uncured Silicone Rubber Interleave: Polyethylene Appearanc..
|
|||
| Tensile Strength | 6.55 MPa | 950 psi | Side 2, Layer 2, Silicone Property; ASTM D412 |
|
Arlon 51588R019 0.019" (0.483 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2, Layer 1: Cured Silicone RubberSide 2, Layer 2: Uncured Silicone Rubber Interleave: Polyethylene Appearanc..
|
|||
| Tensile Strength | 6.55 MPa | 950 psi | Silicone Property; ASTM D412 |
|
Arlon 55580R028 0.028" (0.711 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: 162 Style FiberglassAppearance: Red silicone gum on fiberglass clothThis data represents typical values for th..
|
|||
| Tensile Strength | 6.55 MPa | 950 psi | Silicone Property; ASTM D412 |
|
Arlon 55581R028 0.028" (0.711 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave 1: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: 162 Style FiberglassSide 2: Uncured Silicone RubberInterleave 2: PolyethyleneAppearance: Red silicone gum on..
|
|||
| Tensile Strength | 6.55 MPa | 950 psi | Side 2, Silicone Property; ASTM D412 |
|
Arlon 55586R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave: PolyethyleneAppearance: Red silicone gum and rubber on fiberglass clothTh..
|
|||
| Tensile Strength | 6.55 MPa | 950 psi | Side 2, Silicone Property; ASTM D412 |
|
Arlon 56586R026 0.027" (0.686 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone Rubber Substrate: 1564 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Appearance: Red silicone gum and rubber on fiberglass clo..
|
|||
| Tensile Strength | >= 6.55 MPa | >= 950 psi | Compound Property |
|
Arlon R34482X062 0.062" (0.356 mm) Uncured/Cured Silicone Rubber
Design/Construction:Side 1: Cured/Post-cured Unsupported Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, materi..
|
|||
| Tensile Strength | 6.55 MPa | 950 psi | Silicone Property; ASTM D412 |
|
Arlon 32580R060 0.060" (1.52 mm) Uncured Silicone Rubber on PET Carrier
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PETAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. ..
|
|||
| Tensile Strength | 6.55 MPa | 950 psi | Side 2, Silicone Property; ASTM D412 |
|
Arlon 49586B010 0.0115" (0.292 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 1681 FiberglassSide 2: Uncured Silicone RubberInterleave: Polyethylene This data represents typical values for the production mater..
|
|||
| Tensile Strength | 6.55 MPa | 950 psi | Silicone Property; ASTM D412 |
|
Arlon 51581B015 0.015" Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave 1: 2.5 mil LDPESide 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave 2: 2.5 mil LDPEThis data represents typical..
|
|||
| Tensile Strength | 6.55 MPa | 950 psi | Silicone Property; ASTM D412 |
|
Arlon 51581R027 0.027" (0.686 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave 2: Polyethylene Appearance: Red silicone gu..
|
|||
| Tensile Strength | 6.55 MPa | 950 psi | Silicone Property; Arlon SQA-TMS-008 |
|
Arlon 51583R018 0.018" Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave 1: 2.5 mil LDPESide 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberInterleave 2: 2.5 mil LDPEThis data represents typical val..
|
|||
| Tensile Strength | 6.55 MPa | 950 psi | Layer 1, Silicone Property; ASTM D412 |
|
Arlon 55589G028 0.0295" (0.749 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: 162 Style FiberglassAppearance: Green silicone gum and rubber on fiberglass Th..
|
|||
| Tensile Strength | >= 6.55 MPa | >= 950 psi | Compound Property |
|
Arlon 59463X068CT 0.068" (1.73 mm) Textured, Cured Rubber with Fiberglass Substrate
Design/Construction:Side 1: Textured, Cured Rubber Side 2: Textured, Cured Rubber This data Represents typical values for the production material. The data should not be used to write, or in place o..
|
|||
| Tensile Strength | 6.55 MPa | 950 psi | Silicone Property; Arlon SQA-TMS-009 |
|
Arlon 915-20Hxx-P0 0.015" Self-Fusing Silicone Rubber
2 inch wide, 15 mil thick, pale yellow, rectangular cross-section, silicone self-fusing tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part num..
|
|||
| Tensile Strength | 6.55 MPa | 950 psi | Silicone Property; ASTM D412 |
|
Arlon 44580R020 0.020" Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 2.5 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1165 Fiberglass (Flexible Heater Substrate)This data represents typical values for the producti..
|
|||
| Tensile Strength | 6.55 MPa | 950 psi | Silicone Property; ASTM D412 |
|
Arlon 47581R007 0.007" (0.178 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave 1: PESide 1: Uncured Silicone RubberSubstrate: 2113 Style FiberglassSide 2: Uncured Silicone RubberInterleave 2: PE This data represents typical values for the produc..
|
|||