Tensile Strength 6.55 MPa
<br>@Strain 100 %
950 psi
<br>@Strain 100 %
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ HC 2175 Polyvinyl Chloride, Flexible (PVC, Flexible)
Geon HC 2175 is a 75 Shore A non-phthalate flexible vinyl compound made from FDA sanctioned ingredients. HC 2175 can be used for extrusion and injection molding healthcare applications.NOTE: All ing..
Tensile Strength 6.55 MPa
<br>@Strain 100 %
950 psi
<br>@Strain 100 %
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ HC 2175G Polyvinyl Chloride, Flexible (PVC, Flexible)
Geon HC 2175G is a 75 Shore A non-phthalate, gamma-stable flexible vinyl compound made from FDA sanctioned ingredients. HC 2175G can be used for extrusion and injection molding healthcare applicatio..
Tensile Strength 6.55 MPa
950 psi
ASTM D412-98
Saint-Gobain Tygon® Norprene® A-60-N Drinking Water Tubing Formulation.
Formulated for use as drinking water tubing. Complies with FDA and NSF61 criteria.Information provided by Saint Gobain Performance Products.
Tensile Strength 6.55 MPa
950 psi
Teknor Apex Tekbond® TB 1339B Thermoplastic Elastomer
Notes: Tekbond® TPEs are a functional series of elastomer compounds designed to not only bond to the most difficult neat and reinforced engineering substrates with no primer or surface treatment, b..
Tensile Strength 6.55 MPa
950 psi
ASTM D412
Teknor Apex Telcar® OBC 2419B Thermoplastic Elastomer
Notes: Telcar OBC has superior mechanical strength and higher elongation which will provide a tougher more durable finished product. Telcar OBC can be used in less demanding sealing applications. T..
Tensile Strength 6.55 MPa
950 psi
Silicone Property; ASTM D412
Arlon 18596R026 0.026" (0.66 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: 11523 Style FiberglassSide 2: Uncured Silicone RubberInterleave: PolyethyleneThis data represents typical values for the production materi..
Tensile Strength 6.55 MPa
950 psi
Side 2; ASTM D412
Arlon 19586R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: 1523 Style FiberglassSide 2: Uncured Silicone RubberThis data represents typical values for the production mat..
Tensile Strength 6.55 MPa
950 psi
Silicone Property; ASTM D412
Arlon 32580R020 0.020" (0.508 mm) Uncured Silicone Rubber on Polyester Film Carrier
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: Polyester FilmAppearance: Red silicone gum on polymer linerThis data represents typical values for the production..
Tensile Strength 6.55 MPa
950 psi
Silicone Property; ASTM D412
Arlon 32580R035 0.035" (0.889 mm) Uncured Silicone Rubber on PET Carrier
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PETAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. ..
Tensile Strength 6.55 MPa
950 psi
Side 2, Silicone Property; ASTM D412
Arlon 51586R015H 0.016" (0.406 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene This data represents typical values for the production mat..
Tensile Strength 6.55 MPa
950 psi
Side 1 Uncured Silicone Property; ASTM D412
Arlon 51588R015 0.015" Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: LDPESide 1 Layer 2: Uncured Silicone RubberSide 1 Layer 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: LDPETh..
Tensile Strength 6.55 MPa
950 psi
Side 2 Silicone Property; ASTM D412
Arlon 51588R015 0.015" Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: LDPESide 1 Layer 2: Uncured Silicone RubberSide 1 Layer 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: LDPETh..
Tensile Strength 6.55 MPa
950 psi
Side 1, Silicone Property; ASTM D412
Arlon 51588R019 0.019" (0.483 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2, Layer 1: Cured Silicone RubberSide 2, Layer 2: Uncured Silicone Rubber Interleave: Polyethylene Appearanc..
Tensile Strength 6.55 MPa
950 psi
Side 2, Layer 2, Silicone Property; ASTM D412
Arlon 51588R019 0.019" (0.483 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2, Layer 1: Cured Silicone RubberSide 2, Layer 2: Uncured Silicone Rubber Interleave: Polyethylene Appearanc..
Tensile Strength 6.55 MPa
950 psi
Silicone Property; ASTM D412
Arlon 55580R028 0.028" (0.711 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: 162 Style FiberglassAppearance: Red silicone gum on fiberglass clothThis data represents typical values for th..
Tensile Strength 6.55 MPa
950 psi
Silicone Property; ASTM D412
Arlon 55581R028 0.028" (0.711 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave 1: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: 162 Style FiberglassSide 2: Uncured Silicone RubberInterleave 2: PolyethyleneAppearance: Red silicone gum on..
Tensile Strength 6.55 MPa
950 psi
Side 2, Silicone Property; ASTM D412
Arlon 55586R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave: PolyethyleneAppearance: Red silicone gum and rubber on fiberglass clothTh..
Tensile Strength 6.55 MPa
950 psi
Side 2, Silicone Property; ASTM D412
Arlon 56586R026 0.027" (0.686 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone Rubber Substrate: 1564 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Appearance: Red silicone gum and rubber on fiberglass clo..
Tensile Strength 6.55 MPa
950 psi
Silicone Property; ASTM D412
Arlon 56596R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone Rubber Substrate: 1564 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Product Use: Flexible heater insulationAppearance: Red si..
Tensile Strength 6.55 MPa
950 psi
Silicone Property; ASTM D412
Arlon 99580R010 0.010" (0.254 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Design/Construction: Interleave: FEP FilmSide 1: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassFlexible heater substrateAppearance: Red, High viscosity gum on release linersThis data repres..
Tensile Strength >= 6.55 MPa
>= 950 psi
Compound Property
Arlon R34482X062 0.062" (0.356 mm) Uncured/Cured Silicone Rubber
Design/Construction:Side 1: Cured/Post-cured Unsupported Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, materi..
Tensile Strength 6.55 MPa
950 psi
Side 2, Silicone Property; ASTM D412
Arlon 49586B010 0.0115" (0.292 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 1681 FiberglassSide 2: Uncured Silicone RubberInterleave: Polyethylene This data represents typical values for the production mater..
Tensile Strength 6.55 MPa
950 psi
Silicone Property; ASTM D412
Arlon 51581B015 0.015" Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave 1: 2.5 mil LDPESide 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave 2: 2.5 mil LDPEThis data represents typical..
Tensile Strength 6.55 MPa
950 psi
Silicone Property; ASTM D412
Arlon 51581R027 0.027" (0.686 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave 2: Polyethylene Appearance: Red silicone gu..
Tensile Strength 6.55 MPa
950 psi
Silicone Property; Arlon SQA-TMS-008
Arlon 51583R018 0.018" Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave 1: 2.5 mil LDPESide 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberInterleave 2: 2.5 mil LDPEThis data represents typical val..
Tensile Strength 6.55 MPa
950 psi
Side 2, Silicone Property; ASTM D412
Arlon 55586R040 0.040" (1.02 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave: LDPEAppearance: Red silicone gum and rubber on fiberglass clothThis data ..
Tensile Strength 6.55 MPa
950 psi
Layer 1, Silicone Property; ASTM D412
Arlon 55589G028 0.0295" (0.749 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: 162 Style FiberglassAppearance: Green silicone gum and rubber on fiberglass Th..
Tensile Strength 6.55 MPa
950 psi
Silicone Property; Arlon SQA-TMS-009
Arlon 915-20Hxx-P0 0.015" Self-Fusing Silicone Rubber
2 inch wide, 15 mil thick, pale yellow, rectangular cross-section, silicone self-fusing tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part num..
Tensile Strength 6.55 MPa
950 psi
Silicone Property; ASTM D412
Arlon 44580R020 0.020" Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 2.5 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1165 Fiberglass (Flexible Heater Substrate)This data represents typical values for the producti..
Tensile Strength 6.55 MPa
950 psi
Silicone Property; ASTM D412
Arlon 47581R007 0.007" (0.178 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave 1: PESide 1: Uncured Silicone RubberSubstrate: 2113 Style FiberglassSide 2: Uncured Silicone RubberInterleave 2: PE This data represents typical values for the produc..
Copyright © lookpolymers.com All Rights Reserved