| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Compressive Strength | 110 MPa | 16000 psi | |
|
Poco Graphite PLS Semiconductor Grade Graphite
Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their ..
|
|||
| Compressive Strength | 110 MPa | 16000 psi | 10% Def.; ASTM D695 |
|
Quadrant EPP Acetron® POM-H Homopolymer Acetal, Unfilled, Extruded (ASTM Product Data Sheet) |
|||
| Compressive Strength | 110 MPa | 16000 psi | 10% Def.; ASTM D695 |
|
Quadrant EPP Nylatron® 4.6 (ASTM Product Data Sheet) |
|||
| Compressive Strength | 110 MPa | 16000 psi | Break; TM R050-38 |
|
Resinlab® EP1320LV Heat Cure Epoxy Conformal Coating
Resinlab™ EP1320 and EP1320LV are one part heat cure epoxy conformal coatings. They can also be used as a small mass potting compounds, structural adhesives, or insulating polymer systems where the..
|
|||
| Compressive Strength | 110 MPa | 16000 psi | Ultimate; TM R050-38 |
|
Resinlab® EP1330LV Heat Cure Epoxy Polymer System
Resinlab™ EP1330 and EP1330LV are one part heat cure epoxy polymer systems. They can also be used as a small mass potting or staking compounds, or a dam adhesive in and “dam and fill” application..
|
|||
| Compressive Strength | 110 MPa | 16000 psi | ASTM D695 |
|
Solvay Specialty Polymers KetaSpire® KT-820 SL30 Polyetheretherketone (PEEK)
(Unverified Data**)
Ketaspire KT-820 SL30 is a polyetheretherketone (PEEK) compound designed to provide a balance of excellent mechanical properties, wear resistance and low coefficient of friction in both dry and exte..
|
|||
| Compressive Strength | 110 MPa | 16000 psi | Sample Type B, 5 mm/min; ISO 604:2002 |
|
Global EPP POM C Acetal Copolymer
Polyacetals are highly crystalline thermoplastics, characterised by their high mechanical strength, rigidity and impact resistance. Acetal absorbs very little moisture, enabling the product to maint..
|
|||
| Compressive Strength | 110 MPa | 16000 psi | ASTM D695 |
|
Solvay Specialty Polymers AvaSpire® AV-630 Polyaryletherketone (PAEK)
AvaSpire® AV-630 is an unreinforced polyaryletherketone (PAEK) developed as an alternative to low melt flow PEEK for the extrusion of ultra-thin films. Films with thicknesses as low as 0.2 mils (..
|
|||
| Compressive Strength | 110 MPa | 16000 psi | ASTM D256 |
|
Techmer ES Luriblend® PA6/6 GF30 ML5 HS 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and Molybdenum Disulfide Lubricant(5%)Features: Lubricated and Heat Stabiliz..
|
|||
| Compressive Strength | 110 MPa | 16000 psi | ASTM D695 |
|
Techmer ES Plaslube® J-50/20/SI/2 Polycarbonate, 20% GFR, 2% Silicone |
|||
| Compressive Strength | 110 MPa | 16000 psi | |
|
Engineered Syntactic Systems HZ-40 Deep Water Syntactic Foam
Syntactic foams are a unique combination of hollow spheres, a resin matrix, and other additives. When combined and processed properly, the constituents form a lightweight homogeneous material having..
|
|||
| Compressive Strength | 110 MPa | 16000 psi | ASTM D695; at 10% Deflection |
|
Westlake Plastics Pomalux® Acetal Copolymer
Pomalux is a high performance acetal copolymer that has excellent mechanical, electrical, and wear properties. It is engineered to provide outstanding dimensional stability, even when machining par..
|
|||
| Compressive Strength | 110 MPa | 16000 psi | ASTM D695 |
|
Westlake Plastics Zelux® 20% GF Polycarbonate 20% Glass Filled
Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and ..
|
|||
| Compressive Strength | 110 MPa | 16000 psi | Absolute Drying; ASTM-D695 |
|
Toyobo GLAMIDE® T-400G15 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
|
|||
| Compressive Strength |
110
MPa @Treatment Temp. 250 °C, Time 3600 sec |
16000
psi @Treatment Temp. 482 °F, Time 1.00 hour |
ISO 604; IEC/EN 60893-2 5.3 |
|
Elektro-Isola G-Etronax SI Silicone, Glass Fabric Reinforcement, White, Sheets
Description: Electrical and electrotechnical applications. Suitable as high-frequency insulation on account of its dielectric loss. Used as, among other things, an insulation material in large induc..
|
|||
| Compressive Strength | 110 MPa | 16000 psi | ASTM D695 |
|
Ensinger Tecapeek® XP-117 Compression Molded PEEK Compound, 25% PTFE Filled
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..
|
|||
| Compressive Strength | 110 MPa | 16000 psi | |
|
3M iM16K Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
|
|||
| Compressive Strength | 110 MPa | 16000 psi | ASTM D695 |
|
Applied Composites 185 Polyester SMC
Industry Application: TransportationProduct Application: Lawn and GardenDistinct Features: Limited PigmentabilityInformation provided by Applied Composites Corporation.
|
|||
| Compressive Strength | 110 - 138 MPa | 16000 - 20000 psi | |
|
Bulk Molding Compounds BMC 324 Automotive Grade Molding Compound
BMC 324 is a low profile, automotive grade molding compound that is suitable for Injection, Compression or Transfer molding operations. BMC 324 can be metallized directly, without an initial base-co..
|
|||
| Compressive Strength | 110 - 138 MPa | 16000 - 20000 psi | |
|
Bulk Molding Compounds BMC T12(18) General Purpose Molding Compound
BMC T12(18) is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. Ty..
|
|||
| Compressive Strength | 110 - 138 MPa | 16000 - 20000 psi | |
|
Bulk Molding Compounds BMC T12-15541 General Purpose Molding Compound
BMC T12 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. Typica..
|
|||
| Compressive Strength | 110 MPa | 16000 psi | ASTM D695 |
|
PolyOne Edgetek® NI-20GF/000 Nylon 6/10, Glass Filled
(discontinued **)
Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
|
|||
| Compressive Strength | 110 MPa | 16000 psi | ASTM D695 |
|
Quantum Polycarbonate 20% Glass Fiber Filled
Information provided by Quantum Advanced Engineering Plastics
|
|||
| Compressive Strength | 110 - 130 MPa | 16000 - 18900 psi | GB/T 1040 |
|
Beijing Evergrow Resources Glass Filled Nylon
Information provided by Beijing Evergrow Resources.
|
|||
| Compressive Strength | 110 MPa | 16000 psi | ASTM D695 |
|
Quantum Acetal-Homopolymer
Information provided by Quantum Advanced Engineering Plastics
|
|||
| Compressive Strength | 110 MPa | 16000 psi | Break; TM R050-38 |
|
Resinlab® EP1305LV Black Epoxy Casting Resin
Resinlab™ EP1305LV Black is a black two-part epoxy casting resin designed to give good adhesion to metals and especially PVC. It has good wetting to most surfaces and is free flowing to penetrate c..
|
|||
| Compressive Strength | 110 - 138 MPa | 16000 - 20000 psi | |
|
Bulk Molding Compounds BMC T15(GPS) General Purpose Molding Compound
BMC T15(GPS) is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15(GPS) is well suited for injection, transfer or compression..
|
|||
| Compressive Strength | 110 - 138 MPa | 16000 - 20000 psi | |
|
Bulk Molding Compounds BMC T15(GPT) General Purpose Molding Compound
BMC T15(GPT) is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15(GPT) is well suited for injection, transfer or compression..
|
|||