| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Compressive Strength | 82.7 MPa | 12000 psi | Ultimate; TM R050-38 |
|
Resinlab® EP1285HD-9 Highly Filled, Medium Viscosity Casting Resin
Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C..
|
|||
| Compressive Strength | 83.0 MPa | 12000 psi | |
|
Pyrotek Pyrocast FSC-2000 Stabilized fused silica cement
Pyrocast FSC-2000 eliminates the need for cement pre-mixing or rolling while providing the same outstanding characteristics of all dense fused silica products.ApplicationsAdhesive Coating Patching c..
|
|||
| Compressive Strength |
82.7
MPa <br>@Strain 10.0 %,<br> Temperature 22.8 °C
|
12000
psi <br>@Strain 10.0 %,<br> Temperature 73.0 °F
|
ASTM D695 |
|
Quadrant EPP Quadrant Nylon 612 |
|||
| Compressive Strength | 82.7 MPa | 12000 psi | Break; TM R050-38 |
|
Resinlab® EP1325 Thixotropic, Heat Curing Epoxy Adhesive
Resinlab™ EP1325 and EP1325LV are one part thixotropic, heat curing epoxy adhesives. They can also be used as a small mass potting compounds, staking or damming adhesives, or polymer systems where ..
|
|||
| Compressive Strength | 82.7 MPa | 12000 psi | ASTM D695 |
|
Quantum Polycarbonate
Information provided by Quantum Advanced Engineering Plastics
|
|||
| Compressive Strength | 83.0 MPa | 12000 psi | 10% pressing; EN ISO 604 |
|
Schwartz Technical Plastics LAMIGAMID® 600 Polyoxymethylene
Application: friction bearings, wear and sliding linersInformation provided by Schwartz Technical Plastics GmbH
|
|||
| Compressive Strength | 82.7 MPa | 12000 psi | ASTM D695 |
|
Plastics Group Polifil® GFABS-10 10% Glass-Reinforced Acrylonitrile-Butadiene Styrene (ABS)
Polifil® GFABS series compounds combine the most desirable properties of both components - allowing for enhanced processability and toughness together with the stiffness of glass.Applications: Fire..
|
|||
| Compressive Strength | 82.7 MPa | 12000 psi | |
|
Wingate Alloys Winco Poly NLT Engineered UHMW
Winco Poly NLT is one of the oldest and most widely used engineered mechanical plastics. Its combination of toughness, dimensional stability, wear resistance, availability and versatility make it a ..
|
|||
| Compressive Strength |
83.0
MPa <br>@Strain 3.50 %
|
12000
psi <br>@Strain 3.50 %
|
DIN EN ISO 604 |
|
Wolf Kunststoff ZEDEX® ZX-750V5KF 055 Polymer Alloy. Fiber Reinforced
Main Characteristics: Stiff; High elongation and yield stress; Low thermal expansion; Impact resistantApplications: Textile Machinery; Compressors; Hinges; Handling; Machine Tools; Automitve Technol..
|
|||
| Compressive Strength | 82.7 MPa | 12000 psi | ASTM D695 |
|
Chesterton ARC 855 Abrasion Control Liquid
Description: An advanced ceramic composite formulated to protect equipment from aggressive chemical attack, corrosion, and erosion. The product is a low viscosity composite that is easily applied by..
|
|||
| Compressive Strength | 82.7 MPa | 12000 psi | |
|
CMT Materials HYTAC® B Solid Polymer Tooling Material
Sometimes, finer plug assist details are required which are not obtainable or maintainable with syntactic foam plugs. For these high detail applications, where high toughness and easy machinability ..
|
|||
| Compressive Strength | 82.7 MPa | 12000 psi | Compared to 3500 for concrete |
|
Abatron AboCrete Cement/Grout Resurfacing and Patching Epoxy
Cement/grout resurfacing and patching epoxy for industrial, marine, institutional, and residential uses. The ultimate restoration and resurfacing material structurally and chemically superior to co..
|
|||
| Compressive Strength | 82.7 - 96.5 MPa | 12000 - 14000 psi | ASTM D695 |
|
Cast Nylons Nycast® GX Solid Lubricant Filled Gray Cast Nylon 6
NYCAST® GX is a specially formulated, self-lubricating grade designed to deliver low coefficient of friction, superior wear resistance, high pressure/velocity performance, and low moisture absorpti..
|
|||
| Compressive Strength | 82.7 - 96.5 MPa | 12000 - 14000 psi | ASTM D695 |
|
Cast Nylons Nycast® RX Solid Lubricant Filled Red Cast Nylon 6
NYCAST® RX is a specially formulated, self-lubricating grade designed to deliver low coefficient of friction, superior wear resistance, high pressure/velocity performance, and low moisture absorpti..
|
|||
| Compressive Strength | 82.7 MPa | 12000 psi | ASTM D695 |
|
3M Scotchkote™ PR 415 Epoxy Concrete Repair
Scotchkote Epoxy Concrete Repair PR 415 has been specifically developed as a three component 100% solids self priming concrete repair system.Product Features:Combines good application characteristic..
|
|||
| Compressive Strength | 82.7 MPa | 12000 psi | |
|
Aremco AREMCOLOX™ 502-1100 (Unfired) Machinable Alumino-Silicate
Good thermal and dielectric properties and can be fired to increase temperature resistance and mechanical strength. Easily machined to close tolerances. Plates, rods and bars available to 12".
|
|||
| Compressive Strength | 82.7 MPa | 12000 psi | in plane |
|
Carlisle 201HL Carbon-Carbon Composite
Carbon-Carbon Composite manufactured as sheets from 4mm to 125mm thick this material is essentially a fracture tough, fiber reinforced graphite often referred to as a “CFC”. Good for use in air t..
|
|||
| Compressive Strength | 82.7 MPa | 12000 psi | for Epoxy Coating |
|
Aremco Corr-Paint™ CP2060 High Temperature Protective Coating Novolac-Epoxy, Silicon Carbide Filled
This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho..
|
|||
| Compressive Strength | 82.7 MPa | 12000 psi | Break; TM R050-38 |
|
Resinlab® EP1285HD-10 Highly Filled, Medium Viscosity Casting Resin
Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C..
|
|||
| Compressive Strength | 82.7 MPa | 12000 psi | 10% Def.; ASTM D695 |
|
Quadrant EPP Quadrant PVC Polyvinyl Chloride, Type I, Grade 1 (ASTM Product Data Sheet) |
|||
| Compressive Strength | 82.7 MPa | 12000 psi | Ultimate; TM R050-38 |
|
Resinlab® EP1190 Flame Retardant Epoxy Casting Resin
Resinlab™ EP1190 is a medium viscosity, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File# E186034, Proje..
|
|||