| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Compressive Strength | 131 MPa @Temperature 23.9 °C |
19000 psi @Temperature 75.0 °F |
Dry; ASTM D695 |
| Park Electrochemical Nelcote® F-562 Phenolic Prepreg, C2 Carbonized Rayon Reinforced Nelcote® F-562 is an elastomer modified phenolic resin used in the manufacture of intermediate temperature ablative rocket nozzles, heat shields and combustion chambers in highly oxidative environm.. |
|||
| Compressive Strength | 131 MPa | 19000 psi | 10% Def.; ASTM D695 |
| Quadrant EPP Ketron® CM GF30 Compression Molded, 30% Glass Reinforces Polyethererther Ketone(ASTM Product Data Sheet) |
|||
| Compressive Strength | 131 MPa | 19000 psi | ASTM D695 |
| PolyOne Edgetek® PS-30GF/000 FR V0 Polybutylene Terephthalate (PBT), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedFlame RetardantPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
| Compressive Strength | 131 MPa | 19000 psi | ASTM D695 |
| IDI Composites 44-10 MW Thermoset Polyester, Molding Moderate strength material specifically formulated for microwave oven performance.Data provided by the manufacturer. |
|||
| Compressive Strength | 131 MPa | 19000 psi | ASTM D695 |
| IDI Composites W-102 Thermoset Polyester, Molding Premium appearance grade materials in a range of strengths for cookware and appliance applications.Data provided by the manufacturer. |
|||
| Compressive Strength | 131 MPa | 19000 psi | ASTM D695 |
| Greene Tweed Arlon® 1000 Polyketone Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie.. |
|||
| Compressive Strength | 131 MPa | 19000 psi | |
| Haysite 270FRII Polyester BMC, Glass Reinforced Haysite Grade 270FRII is a second generation glass reinforced thermoset polyester bulk molding compound. This material can be compression, transfer, or injection molded. Qualified under MIL-M-14, Ty.. |
|||
| Compressive Strength | 131 MPa @Temperature 149 °C |
19000 psi @Temperature 300 °F |
|
| Haysite Heatmeiser® H340 Platen Insulation Haysite’s family of mold and platen insulation products are specially engineered fiberglass reinforced thermoset polyester composites which offer superior energy efficiency, temperature control.. |
|||
| Compressive Strength | 131 MPa | 19000 psi | ASTM D695 |
| Techmer ES Plaslube® J-4/35/TF/15 NAT PA6/12 |
|||
| Compressive Strength | >= 131 MPa | >= 19000 psi | |
| Master Bond EP45HTQ Quartz Filled Heat Resistant Epoxy Description: Master Bond Polymer Compound EP45HTQ is a two component quartz filled, epoxy compound for high performance structural bonding and casting. It is suitable for applications where long ter.. |
|||
| Compressive Strength | 131 MPa | 19000 psi | ASTM D695 |
| Plenco 1581 Polyester, Pellet, Injection Molded PLENCO 01581 is a glass and mineral reinforced pelletized polyester molding compound, exhibiting excellent dimensional stability, mechanical strength and also arc resistance, track resistance, and f.. |
|||
| Compressive Strength | 131 MPa @Time 36.0 sec |
19000 psi @Time 0.0100 hour |
|
| Wolf Kunststoff ZEDEX® ZX-324VMT A3B PEEK, Fiber Reinforced Main Characteristics: Maximum rigidity; Very good wear resistance; Low stick-slip tendency; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInfor.. |
|||
| Compressive Strength | 131 MPa @Temperature 23.0 °C |
19000 psi @Temperature 73.4 °F |
EN ISO 604 |
| Ensinger TECASINT™ 2031 Polyimide, 40% Graphite Filled (PI) TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications... |
|||
| Compressive Strength | 131 - 138 MPa | 19000 - 20000 psi | |
| Bulk Molding Compounds BMC 1605 Low Shrink, Medium Strength BMC 1605 is an excellent low-cost HB material with low shrink and medium strength. Has excellent surface finish and gloss. Can be injection, compression or transfer molded. UL® recognized. This mat.. |
|||
| Compressive Strength | 131 - 165 MPa | 19000 - 24000 psi | |
| Bulk Molding Compounds BMC 680 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 680 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression and stuffer injection molding It is characterized by good moldability, very high impa.. |
|||
| Compressive Strength | 131 - 145 MPa | 19000 - 21000 psi | |
| Bulk Molding Compounds BMC 850 Corrosion Resistant, Flame Retardant Molding Compound BMC 850 is a high strength, corrosion resistant and flame retardant molding compound. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk form.Typical applications a.. |
|||
| Compressive Strength | 131 - 159 MPa | 19000 - 23000 psi | |
| Bulk Molding Compounds BMC T40(25)-XHS Die Casting Replacement Grade Molding Compound BMC T40(25)-XHS is a high strength molding compound with excellent dimensional stability. It is UL recognized and is available in a wide range of colors. Because of its superior physical propertie.. |
|||
| Compressive Strength | 131 MPa | 19000 psi | |
| Bulk Molding Compounds BMC T40(25)-XHS-15869 Die Casting Replacement Grade Molding Compound BMC T40(25)-XHS-15869 is a high strength molding compound with excellent dimensional stability. It is UL recognized and is available in a wide range of colors. Because of its superior physical pro.. |
|||
| Compressive Strength | 131 - 159 MPa | 19000 - 23000 psi | |
| Bulk Molding Compounds BMC T9 General Purpose Molding Compound BMC T9 is a low cost, general purpose bulk molding compound designed for the electrical industry. It is UL listed and is used extensively in the manufacture of residential circuit breakers. BMC T9.. |
|||
| Compressive Strength | 131 - 152 MPa | 19000 - 22000 psi | |
| Bulk Molding Compounds BMC 810 General Purpose Molding Compound BMC 810 is a general purpose, very high strength compound suitable for compression, transfer and stuffer injection molding. It is characterized by excellent flow and controlled reactivity and is wel.. |
|||
| Compressive Strength | 131 - 145 MPa | 19000 - 21000 psi | |
| Bulk Molding Compounds BMC 851 Corrosion Resistant, Flame Retardant Molding Compound BMC 851is a high strength, corrosion resistant and flame retardant molding compound. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk form.Typical applications ar.. |
|||
| Compressive Strength | 131 MPa | 19000 psi | ASTM D695 |
| Plenco 1506 Polyester, Briquette, Injection Molded PLENCO 01506 is a mineral and cellulose filled granular polyester molding compound, with glass fiber reinforcement for improved mechanical strength properties. 01506 offers excellent electrical prop.. |
|||
| Compressive Strength | 131 MPa | 19000 psi | ASTM D695 |
| Sumitomo Bakelite North America FS-5 Short-Glass Reinforced Diallyl Phthalate Short glass fiber reinforced, non-flame retardant, diallyl meta-phthalate molding compound which meets the requirements of ASTM D5948 TYPE SIG.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
| Compressive Strength | 131 MPa | 19000 psi | Break; TM R050-38 |
| Resinlab® EP1305 Black Highly Toughened Urethane Modified Epoxy Resinlab™ EP1305 Black is a highly toughened urethane modified epoxy designed for bonding PVC, metals, ceramics and other difficult to bond substrates. The system has a thixotropic non-sag viscosi.. |
|||
| Compressive Strength | 131 - 159 MPa | 19000 - 23000 psi | |
| Bulk Molding Compounds BMC T40(18) Die Casting Replacement Grade Molding Compound BMC T40(18) was formulated as a direct replacement for aluminum die casting applications. T40(18) is UL recognized. Excellent mechanical properties and dimensional control allow molded parts to ma.. |
|||