Mechanical Properties Metric English Comments
Compressive Strength 207 MPa
<br>@Temperature 23.9 °C
30000 psi
<br>@Temperature 75.0 °F
Dry; 325°F Autoclave; ASTM D695
Park Electrochemical Nelcote® F-557 Phenolic Prepreg, Aerospace Silica Fabric Reinforced
Nelcote® F-557 is a high purity silica filler phonic resin coated on Commercial or Aerospace grade silica fabric. F-557 is used in the manufacture of intermediate temperature ablative rocket nozzle..
Compressive Strength 207 MPa
30000 psi
10% Def.; ASTM D695
Quadrant EPP Semitron® ESd 520HR (ASTM Product Data Sheet)
Compressive Strength 207 MPa
30000 psi
ASTM D695
Resinoid 1365 Phenolic Molding, Glass Reinforced
Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance
Compressive Strength 207 MPa
30000 psi
Poco Graphite ZEE-2 Ion Implant Grade Graphite
ZEE is a hard, wear-resistant material. This next generation ion implant material offers improved performance through the entire range of low to high-energy implants. POCO ZEE is high-purity, isotro..
Compressive Strength 207 MPa
30000 psi
XX Phenolic Laminate
Paper based phenolic provides low cost electrical and mechanical properties. It is widely used for switchboards, panel boards, insulating washers, and intricate punched parts.Information provided b..
Compressive Strength 207 MPa
30000 psi
ASTM D695
IDI Composites C-108 Thermoset Polyester, Molding
Vinylester compounds in a range of strengths with superior corrosion resistance.Data provided by the manufacturer.
Compressive Strength 207 MPa
30000 psi
ASTM D695
IDI Composites C-206 Thermoset Polyester, Sheet
CORROSION - (Patent pending). Versatile family of compounds designed for pressurized and thermo-mechanically stressed applications. Excellent corrosion resistance and high strength.Data provided by ..
Compressive Strength 207 MPa
30000 psi
ASTM D695
IDI Composites E-205 Thermoset Polyester, Sheet
ELECTRICAL - U.L. recognized (E53587). Versatile family of compounds designed to meet the most demanding electrical and electronic applications. Excellent dielectric properties and arc/track resista..
Compressive Strength 207 MPa
<br>@Thickness 12.7 mm
30000 psi
<br>@Thickness 0.500 in
ASTM D695
Industrial Laminates/Norplex NP320U Cotton Fabric
Description: Utility version of NP320E. Meets most, but not all, NEMA properties for L and LE, and is not certifiable as a NEMA Grade.Thickness Tested: 0.062", 0.125", and 0.500"
Compressive Strength 207 MPa
<br>@Thickness 12.7 mm
30000 psi
<br>@Thickness 0.500 in
ASTM D695
Industrial Laminates/Norplex NP630 Paper Base Laminate
Description: Machining grade with good electrical properties and moisture resistance. Low cold flow with good dimensional stability. Thickness Tested: 0.062", 0.125", and 0.500"
Compressive Strength 207 MPa
30000 psi
Flatwise; ASTM D695
Haysite H1000 Polyester Laminate
Haysite Grade 1000 laminate sheet is an outstanding material that is used in applications requiring exceptional weather and corrosion resistance. Grade H1000's unique polyester resin system provide..
Compressive Strength 207 MPa
30000 psi
Haysite HCR-100 Corrosion Resistant Polyester/Glass Sheet
A general purpose isophthalic polyester sheet with flame retardants and ultraviolet inhibitors. Standard color is gray.
Compressive Strength 207 MPa
30000 psi
Haysite HCR-125 Corrosion Resistant Vinyl Ester/Glass Sheet
A fiber glass reinforced thermoset sheet using DEREKANE® 470 vinylester in the resin matrix with flame retardant and ultraviolet inhibitors. Standard color is beige. Derakane® 470 is a registe..
Compressive Strength 207 MPa
30000 psi
Haysite HCR-196 Corrosion Resistant Vinyl Ester/Glass Sheet
A fiber glass reinforced thermoset sheet using DEREKANE® 470 vinylester in the resin matrix. Standard color is grey. Additional data covering resistance to specific chemicals is available upon re..
Compressive Strength 207 MPa
<br>@Thickness 12.7 mm
30000 psi
<br>@Thickness 0.500 in
ASTM D695
Industrial Laminates/Norplex NP664 Paper Base Laminate
Description: Low cost room temperature punching grade with mechanical and electrical properties similar to NP612. This version is made with pigment cover plies on the surface.Thickness Tested: 0.062..
Compressive Strength 207 MPa
30000 psi
ASTM D695
Sumitomo Bakelite Durez® 118 Phenolic, Compression Grade
Durez 118 Black Phenolic is a two-stage, asbestos free, general purpose molding material. It exhibits improved impact strength and resistance to flexural fatigue for demanding automotive, electrica..
Compressive Strength 207 MPa
30000 psi
ASTM D695
Sumitomo Bakelite Durez® 118 Phenolic, Injection Grade
Durez 118 Black Phenolic is a two-stage, asbestos free, general purpose molding material. It exhibits improved impact strength and resistance to flexural fatigue for demanding automotive, electrica..
Compressive Strength 207 MPa
30000 psi
ASTM D695
Sumitomo Bakelite Durez® 152 Phenolic, Compression Grade
Durez 152 Phenolic is a two-stage, heat resistant/electrical molding material. It exhibits superior dimensional stability, good strength retention at elevated temperature and good molded appearance..
Compressive Strength 207 MPa
30000 psi
ASTM D695
Sumitomo Bakelite Durez® 152 Phenolic, Injection Grade
Durez 152 Phenolic is a two-stage, heat resistant/electrical molding material. It exhibits superior dimensional stability, good strength retention at elevated temperature and good molded appearance..
Compressive Strength 207 MPa
30000 psi
ASTM D695
Sumitomo Bakelite Durez® 31735 Phenolic, Compression Grade
Durez 31735 is a special purpose phenolic molding compound developed for automotive and industrial pulleys. This material is designed to optimize pulley performance relating to belt life, dimension..
Compressive Strength 207 MPa
30000 psi
ASTM D695
Saint-Gobain Meldin® 5001 Thermoplastic Bearing Material
General Notes on Meldin 3000/5000 Series Bearing Products:Injection Moldable, High-Performance Bearings. Can withstand environments of high temperature, corrosive, and water.Specific Notes on Meldin..
Compressive Strength 207 MPa
30000 psi
ASTM D695
Sumitomo Bakelite Durez® 29502 Phenolic, Compression Grade
Durez 29502 Brown Phenolic is a two stage, asbestos free, glass filled, special purpose molding material. It is formulated for close tolerance applications such as transmission valve bodies, and di..
Compressive Strength 207 MPa
30000 psi
ASTM D695
Sumitomo Bakelite Durez® 32962 Phenolic Molding Compound, Injection Grade
Durez 32962 Black Phenolic is a medium impact, molding compound. It is designed for applications where additional mechanical strength is required. Typical applications include appliance housings whe..
Compressive Strength 207 MPa
30000 psi
ASTM D695
Plenco 2408 Phenolic, Granular, Compression Molded
PLENCO 02408 is a general purpose, organic filled phenolic molding compound, offering excellent cosmetic characteristics and improved electrical strength properties. UL recognized under component fi..
Compressive Strength 207 MPa
30000 psi
1% offset; ASTM D695
Ensinger TECATOR™ TI 5013 Polyamide-imide (PAI)
TECATOR™ is a high performance melt processable polyamideimide that maintains its excellent mechanical and wear properties in temperature environments exceeding 500°F. Stock shapes from Ensinger ..
Compressive Strength 207 MPa
30000 psi
Lengthwise; ASTM D635
Bedford Plastics Glass Reinforced FR Polyester Structural Fiberglass Profiles
Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod..
Compressive Strength 207 MPa
30000 psi
Lengthwise; ASTM D635
Bedford Plastics Glass Reinforced Vinylester Structural Fiberglass Profiles
Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod..
Compressive Strength 207 MPa
30000 psi
45° stress angle
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Crossply
CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li..
Compressive Strength 207 MPa
30000 psi
XXXPC Phenolic Laminate
Paper based phenolic provides low cost electrical and mechanical properties. It is widely used for switchboards, panel boards, insulating washers, and intricate punched parts.Information provided b..
Compressive Strength 207 MPa
30000 psi
ASTM D695
Sumitomo Bakelite North America FM 4009 Fiberglass Reinforced Phenolic Novolac
FM 4009 is a fiberglass reinforced phenolic novolac molding compound formulated for excellent wear resistance.Information supplied by Sumitomo Bak North America.