| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Compressive Strength | 45.0 MPa | 6530 psi | Cold Crushing Strength |
|
Gouda Vuurvast A 1 S Dense Refractory Brick
Description: A brick with a high creep resistance, successfully applied in anode baking furnaces and in the transition zone of rotary cement kilns.Remarks: This data represents average values, obtai..
|
|||
| Compressive Strength | 45.0 MPa | 6530 psi | Cold Crushing Strength |
|
Gouda Vuurvast AK 44 Dense Refractory Brick
Description: A very dense, high duty fireclay brick with low iron and alkali content. Widely used in anode-baking furnaces (aluminum industry) and as the lining of the top of blast furnaces.Remarks:..
|
|||
| Compressive Strength | 45.0 MPa | 6530 psi | 10% pressing; EN ISO 604 |
|
Schwartz Technical Plastics LAMIGAMID® 300 Cast Polyamide 6, Conditioned
Application: slippers and center blocks for heavy rolling mills, outrigger floatsInformation provided by Schwartz Technical Plastics GmbH
|
|||
| Compressive Strength | 45.0 MPa | 6530 psi | 10% pressing; EN ISO 604 |
|
Schwartz Technical Plastics LAMIGAMID® 300 Cast Polyamide 6, Dry
Application: slippers and center blocks for heavy rolling mills, outrigger floatsInformation provided by Schwartz Technical Plastics GmbH
|
|||
| Compressive Strength |
45.0
MPa @Time 3.60e+7 sec |
6530
psi @Time 10000 hour |
|
|
Wolf Kunststoff ZEDEX® ZX-100MT A1T Polymer Alloy, Mineral Reinforced
Stiff; Hard; Very high strength; No fiber reinforcementApplications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automotive Technology, Machine ToolsInformation provided by Zed..
|
|||
| Compressive Strength | 45.0 MPa | 6530 psi | Practical Use (Water Absorption 1.8%); ASTM-D695 |
|
Toyobo GLAMIDE® T-422VOR Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
|
|||
| Compressive Strength |
45.0
MPa @Temperature 23.0 °C |
6530
psi @Temperature 73.4 °F |
ASTM D695 |
|
DuPont Performance Polymers VESPEL TP-8549 Polyimide
Thermoplastic parts from filled PI (polyimide) for high mechanical properties and low wear and friction performance in high temperature hostile environmentsInformation provided by DuPont Performance..
|
|||
| Compressive Strength | 45.0 MPa | 6530 psi | Cold Crushing Strength |
|
Chosun Refractories ASC-1 Alumina Silicon Carbide Carbon Bricks for Torpedo Car
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
|
|||
| Compressive Strength | 45.0 MPa | 6530 psi | Cold Crushing Strength |
|
Gouda Vuurvast AK 45 Dense Refractory Brick
Description: High quality refractory brick with a good volume stability up to 1450°C. Used where high load bearing capacities are required e.g. blast furnace stoves.Remarks: This data represents av..
|
|||