| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Compressive Strength | 31.0 - 41.4 MPa | 4500 - 6000 psi | ASTM D695 |
|
Arkema Group Kynar Flex® 2900 PVDF Copolymer
(discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
|
|||
| Compressive Strength | 31.0 - 41.4 MPa | 4500 - 6000 psi | ASTM D695 |
|
Arkema Group Kynar Flex® 3120 PVDF Copolymer
(discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
|
|||
| Compressive Strength | 31.0 MPa | 4500 psi | 1% deflection; ASTM D695 |
|
Westlake Plastics Pomalux® Acetal Copolymer For Medical Applications
Medical grade Pomalux is made from acetal copolymer resin which allows machined products the ability to retain dimensional integrity, maintain stability in water and most chemicals at elevated tempe..
|
|||
| Compressive Strength | 31.0 MPa | 4500 psi | |
|
Cotronics Resbond™ 919 High Temperature Ceramic Adhesive, High Resistance |
|||
| Compressive Strength | 31.0 MPa | 4500 psi | |
|
Cotronics Resbond™ 954 High Temperature Ceramic Adhesive, Stainless Steel Composition |
|||
| Compressive Strength | 31.0 MPa | 4500 psi | ASTM D695 |
|
Ensinger Tecaform™ AH ID Metal Detectable Acetal Copolymer (POM)
TECAFORM™ AH ID is the fist commercially available acetal that is fully detectable by standard metal detection equipment. Exhibiting excellent machinability and a good combination of physical prop..
|
|||
| Compressive Strength | 31.0 MPa | 4500 psi | ASTM D695 |
|
Ensinger Tecaform™ Acetal Copolymer - Extruded Products (POM)
Tecaform™ is a semi-crystalline thermoplastic offering high strength, stiffness and toughness. It is resistant to hot water, hydrocarbons and solvents, and it posses good bearing and wear properti..
|
|||
| Compressive Strength | 31.0 MPa | 4500 psi | ASTM D695 |
|
Ensinger Tecaform™ FG Blue Food Grade Acetal (POM)
Tecaform™ is resistant to hot water and typical cleaning chemicals. It possesses good bearing and wear properties. The blue color makes it more visible than standard grades. It is commonly used ..
|
|||
| Compressive Strength | 31.0 MPa | 4500 psi | |
|
Aremco Ceramacast™ 584 High Temperature Potting & Casting Material Magnesia
Two-part, quick-set ceramic for small parts.
|
|||
| Compressive Strength | 31.0 - 41.0 MPa | 4500 - 5950 psi | ASTM D695 |
|
Arkema Group KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..
|
|||
| Compressive Strength | 31.0 - 41.0 MPa | 4500 - 5950 psi | ASTM D695 |
|
Arkema Group KYNAR FLEX® 2800-01 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical s..
|
|||
| Compressive Strength | 31.0 - 41.0 MPa | 4500 - 5950 psi | ASTM D695 |
|
Arkema Group KYNAR FLEX® 2900-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness..
|
|||
| Compressive Strength | 31.0 - 41.0 MPa | 4500 - 5950 psi | ASTM D695 |
|
Arkema Group KYNAR FLEX® 3120-15 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness..
|
|||
| Compressive Strength | 31.0 - 41.0 MPa | 4500 - 5950 psi | ASTM D695 |
|
Arkema Group KYNAR FLEX® 3120-50 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, 150°C temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..
|
|||
| Compressive Strength | 31.0 MPa | 4500 psi | |
|
3M D32/4500 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
|
|||
| Compressive Strength | 31.0 - 41.0 MPa | 4500 - 5950 psi | ASTM D695 |
|
Arkema Group KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..
|
|||