| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Compressive Strength | 345 MPa @Temperature 204 °C |
50000 psi @Temperature 400 °F |
Dry; ASTM D695 |
| Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 581 Quartz Reinforced Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp.. |
|||
| Compressive Strength | 345 MPa | 50000 psi | |
| Pyrotek TS-111 Thermoset Electrical Insulation Product (Nema Grade: G-11) Glass reinforcement, Epoxy Resin, Natural Color. Good electrical and mechanical properties.ApplicationsSuperstructure support pads Bus bar insulators Pot cradle insulators Exhaust duct insulators M.. |
|||
| Compressive Strength | 345 MPa | 50000 psi | 10% Def.; ASTM D695 |
| Quadrant EPP Duratron® PBI CU60 Polybenzimidazole, unfilled, compression molded (ASTM Product Data Sheet) Duratron® PBI is the highest performance engineering plastic available from Quadrant EPP. It offers the highest mechanical properties of any thermoplastic above 400° F (205° C). Duratron® PBI .. |
|||
| Compressive Strength | 345 MPa @Thickness 3.17 mm |
50000 psi @Thickness 0.125 in |
Flatwise |
| Industrial Laminates/Norplex MC507U Glass Fabric Description: MC507U is a utility grade, glass fabric/silicone resin binder composite product that can be substituted for NEMA G-7, in most heating, appliance insulation and some bearing applications.. |
|||
| Compressive Strength | 345 MPa @Thickness 12.7 mm |
50000 psi @Thickness 0.500 in |
ASTM D695 |
| Industrial Laminates/Norplex NP424 Laminate Description: Composite material composed of woven glass fabric surfaces and paper core combined with epoxy resin. Primarily used in the printed circuit board industry. Easy punching and excellent el.. |
|||
| Compressive Strength | 345 MPa @Thickness 8.00 mm |
50000 psi @Thickness 0.315 in |
Flatwise |
| Industrial Laminates/Norplex SP525M (WaveMax 5000) Glass Fabric Description: Non-woven substrate combined with high temperature, static dissipative epoxy resin. Superior machining properties. Capable of producing thin walls with high strength for finely machined.. |
|||
| Compressive Strength | 345 MPa | 50000 psi | Axial; ASTM D695 |
| Glastic Laminates/Shapes SG-200 Fiberglass-Reinforced Polyester Rod Data provided by Glastic Corporation.A continuous-filament fiberglass-roving provides superior strength. Excellent thermal endurance - used to replace silicone rod. |
|||
| Compressive Strength | 345 MPa | 50000 psi | Axial; ASTM D-695 |
| Glastic SG-200 Corner Angles Corner angles used for coil winding.Information provided by Glastic Corporation |
|||
| Compressive Strength | 345 MPa | 50000 psi | ASTM D695 |
| Sumitomo Bakelite Durez® 32633 Glass Filled Phenolic, Compression Grade Durez 32633 Black Phenolic is a two-stage, glass filled, special purpose molding compound. It is designed for applications requiring high physical strengths, dimensional stability, and heat resista.. |
|||
| Compressive Strength | 345 MPa | 50000 psi | |
| TriStar CJ Composite Bearing This family of materials offers the combination of high compressive strength, low coefficient of friction, and excellent abrasion and corrosion resistance while running without lubrication. They are.. |
|||
| Compressive Strength | 345 MPa | 50000 psi | |
| TriStar FCJ Composite Bearing This family of materials offers the combination of high compressive strength, low coefficient of friction, and excellent abrasion and corrosion resistance while running without lubrication. They are.. |
|||
| Compressive Strength | 345 MPa | 50000 psi | |
| Corning Macor® Machinable Glass Ceramic The CTE of Macor® matches most metals and sealing glasses. It is nonwetting, exhibits zero porosity, and, unlike ductile materials, will not deform. It is an excellent insulator at high voltages,.. |
|||
| Compressive Strength | 345 MPa | 50000 psi | ASTM D695 |
| CIP Composites 100 Series Laminated Polymer Bearing Material The 100 series consists of polyester fabric and one of several solid lubricants (optional) in a resin matrix. Non-metallic, high load, high impact and self lubricating laminated material. Laminated.. |
|||
| Compressive Strength | 345 MPa | 50000 psi | |
| Accuratus MACOR Machinable Glass Ceramic Macor is cast as a two phase glass. After casting, it is heat treated causing crystallization of one phase giving rise to its glass-like and ceramic-like characteristics.Key Properties of MACOR: Mac.. |
|||
| Compressive Strength | 345 MPa | 50000 psi | |
| Astro Met Macor® Machinable Glass Ceramic General Description:Macor is a machinable glass-ceramic material with a unique combination of useful properties. A product of Corning Incorporated, it is stocked, distributed and fabricated by Astro.. |
|||
| Compressive Strength | 345 MPa | 50000 psi | |
| Aremco AREMCOLOX™ 502-800 Macor Glass Ceramic
(Unverified Data**) Recommended for temperatures to 1472°F (800°C) and peaks up to 1832°F (1000°C). Demonstrates low thermal conductivity, high strength, high electrical insulation, zero porosity, non-wetting, and .. |
|||
| Compressive Strength | 345 MPa | 50000 psi | |
| Aremco AREMCOLOX™ 502-800 Macor® Machinable Glass Ceramic, MGC Recommended for temperatures to 1472°F (800°C) and peaks up to 1832°F (1000°C). Demonstrates low thermal conductivity, high strength, high electrical insulation, zero porosity, non-wetting, and .. |
|||
| Compressive Strength | 345 MPa | 50000 psi | |
| Saint-Gobain Rulon® FCJ Grade Bearing/Seal PTFE
(discontinued **) Saint Gobain Rulon® CJ is now produced as a part of the TriStar Plastics Corp. product line under the CJ Bearings trade name.Description: Rulon® is the Saint-Gobain trade name for their family of .. |
|||