Mechanical Properties Metric English Comments
Compressive Strength 69.0 MPa
10000 psi
Practical Use (Water Absorption 2.3%); ASTM-D695
Toyobo GLAMIDE® T-422-02 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Compressive Strength 69.0 MPa
10000 psi
Trelleborg Emerson & Cuming Eccolite® Composite Materials Ultra Syntactic Foam
Eccolite Ultra syntactic foam plug assist materials a new engineered thermoplastic compound incorporating Eccospheres, glass microspheres. It is one of the toughest materials designed for the therm..
Compressive Strength 69.0 - 103 MPa
10000 - 14900 psi
ASTM D695
Arkema Group KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Compressive Strength 69.0 - 103 MPa
10000 - 14900 psi
ASTM D695
Arkema Group KYNAR® 710, 710 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Compressive Strength 69.0 - 103 MPa
10000 - 14900 psi
ASTM D695
Arkema Group KYNAR® 740 Black/Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistance; high purityAppli..
Compressive Strength 69.0 - 103 MPa
10000 - 14900 psi
ASTM D695
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Compressive Strength 69.0 - 103 MPa
10000 - 14900 psi
ASTM D695
Arkema Group KYNAR® 740-02 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mecha..
Compressive Strength 69.0 - 103 MPa
10000 - 14900 psi
ASTM D695
Arkema Group KYNAR® 760 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Compressive Strength 69.0 - 103 MPa
10000 - 14900 psi
ASTM D695
Arkema Group KYNAR® 720, 720 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Compressive Strength 69.0 - 82.8 MPa
10000 - 12000 psi
ASTM C133
Ceradyne Thermo-Sil® Isomolded™ Fused Silica
Fused Silica is an excellent thermal insulator with an extremely low coefficient of thermal expansion. It is excellent for thermal shock applications. The key characteristics of this material are:Hi..