| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Compressive Strength | 60.0 MPa | 8700 psi | Cold Crushing Strength |
| Gouda Vuurvast AK 55 S Dense Refractory Brick Description: This andalusite based brick is characterized by a low porosity and a good creep resistance (After 24 hours at 1350°C under a load of 0.2 MPa gives between 14th and 24th hour a creep .. |
|||
| Compressive Strength | 60.0 MPa | 8700 psi | Cold Crushing Strength |
| Gouda Vuurvast AK 70 K Dense Refractory Brick Description: A high quality andalusite/corundum brick with a mullite bond with a very good volume stability. Also good slag- and thermal shock resistance.Remarks: This data represents average values.. |
|||
| Compressive Strength | 60.0 MPa | 8700 psi | Cold Crushing Strength |
| Gouda Vuurvast AK 70 M Dense Refractory Brick Description: This mullite brick is characterized by a very good thermal shock resistance, a high resistance against slag penetration and a high strength.Remarks: This data represents average values,.. |
|||
| Compressive Strength | 60.0 MPa | 8700 psi | Cold Crushing Strength |
| Gouda Vuurvast AK 80 B Dense Refractory Brick Description: A brick made from very pure Guyana bauxite. For applications under severe working conditions such as electric arc furnace roofs.Remarks: This data represents average values, obtained fr.. |
|||
| Compressive Strength | 60.0 MPa | 8700 psi | Cold Crushing Strength |
| Gouda Vuurvast B 1 Sp Dense Refractory Brick Description: High mechanical strength and very low porosity are typical for this type of brick. Application: transition zone in cement kilns, incinerators, steel ladles.Remarks: This data represents.. |
|||
| Compressive Strength | 60.0 MPa | 8700 psi | Cold Crushing Strength |
| Gouda Vuurvast B Sp Dense Refractory Brick Description: A very dense brick, high resistance against slag penetration. Application: in rotary kilns (cement) and incinerators.Remarks: This data represents average values, obtained from samples .. |
|||
| Compressive Strength | 60.0 MPa | 8700 psi | Cold Crushing Strength |
| Gouda Vuurvast AK 65 A Dense Refractory Brick Description: This andalusite based brick with a very pure mullite bond has a low alkali and iron content. In addition, it has a high creep resistance and is therefore used in applications where load.. |
|||
| Compressive Strength | 60.0 MPa | 8700 psi | Cold Crushing Strength |
| Gouda Vuurvast AK 70 A Dense Refractory Brick Description: This brick is made of a high quality bauxite. Application: transition zone of rotary cement kiln.Remarks: This data represents average values, obtained from samples that were cut from s.. |
|||
| Compressive Strength | 60.0 MPa | 8700 psi | Cold Crushing Strength |
| Gouda Vuurvast AK 85 M Dense Refractory Brick Description: A bauxite based brick with a mullite bond. Application: torpedo ladles, electric arc furnace roofs, cement kilns.Remarks: This data represents average values, obtained from samples that.. |
|||
| Compressive Strength | 60.0 MPa | 8700 psi | ASTM D362 |
| Unitika M1030B PA6, Conditioned Nano composite nylonInformation provided by Unitika Ltd. |
|||
| Compressive Strength | 60.0 MPa @Time 360000 sec |
8700 psi @Time 100 hour |
|
| Wolf Kunststoff ZEDEX® ZX-100K A1K Polymer Alloy Main Characteristics: Hard; Stiff; Tough; High fatigue strength; Good weather resistance; Good machinability; FDA compliant LABS; PTFE and silicone-free; KTW approved; Stress resistantApplications: .. |
|||
| Compressive Strength | 60.0 MPa @Time 3.60e+7 sec |
8700 psi @Time 10000 hour |
|
| Wolf Kunststoff ZEDEX® ZX-324VMT A3B PEEK, Fiber Reinforced Main Characteristics: Maximum rigidity; Very good wear resistance; Low stick-slip tendency; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInfor.. |
|||
| Compressive Strength | 60.0 MPa @Time 360000 sec |
8700 psi @Time 100 hour |
|
| Wolf Kunststoff ZEDEX® ZX-530EL3 066 Polymer Alloy, Carbon Fiber Reinforced Main Characteristics: Low thermal expansion; High rigidity; High yield stress; High wear resistance; Low friction; Stress ResistantApplications: Chemical Engineering; Laboratory Technology; Automitv.. |
|||
| Compressive Strength | 60.0 - 150 MPa | 8700 - 21800 psi | Perpendicular to Plane |
| Goodfellow Carbon-Carbon Composite Carbon Fiber - Carbon MatrixInformation provided by Goodfellow. |
|||
| Compressive Strength | >= 60.0 MPa | >= 8700 psi | Axial; IEC 1212-2 4.2 |
| Hippe EP MP 21 Mica Paper Reinforced Epoxy Resin - Round, Rolled Tube Used in mechanical, electrical and electronic applications. Good stability of electrical properties when exposed to high relative humidity. Good heat resistance.Information provided by Hippe. |
|||