| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Compressive Strength | 6.21 - 8.27 MPa | 900 - 1200 psi | @ 1.0% Strain; ASTM D695 |
| Technetics Group Texolon™ 9406 PTFE
(Unverified Data**) General purpose 25% glass filled PTFE for applications less demandingPTFE CharacteristicsChemical ResistanceThermal StabilityCryogenic PropertiesLow Coefficient of FrictionLow Surface EnergyLow Diel.. |
|||
| Compressive Strength | 6.21 - 8.62 MPa @Strain 1.00 % |
900 - 1250 psi @Strain 1.00 % |
ASTM D695 |
| Garlock 9405 PTFE Rubber Sheet, 25% Glass Filled Premium Grade 25% Glass-filled Skived PTFE SheetInformation provided by Garlock Rubber Technologies |
|||