Mechanical Properties Metric English Comments
Impact Test 230 J
<br>@Thickness 6.35 mm,<br> Temperature -40.0 °C
170 ft-lb
<br>@Thickness 0.250 in,<br> Temperature -40.0 °F
ARM Low Temperature Impact on Rotomolded samples; ARM Method
NOVA Chemicals Surpass® RMs341-U Octene sHDPE Rotational Molding Resin
RMs341-U complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. RMs341-..
Impact Test 230 J
<br>@Thickness 3.17 mm,<br> Temperature -40.0 °C
170 ft-lb
<br>@Thickness 0.125 in,<br> Temperature -40.0 °F
Rotational Molded; ARM Method
NOVA Chemicals Surpass® RMs539-U Octene sMDPE Rotational Molding Film
Features: Octene copolymerExceptional low temperature impact propertiesOutstanding stiffnessBroad processing windowSuperior whiteness for improved part appearanceEasy mold releaseNSF listed for Stan..
Impact Test 230 J
<br>@Thickness 3.17 mm,<br> Temperature -40.0 °C
170 ft-lb
<br>@Thickness 0.125 in,<br> Temperature -40.0 °F
Rotational Molded; ARM Method
NOVA Chemicals Surpass® RMs539-UG Octene sMDPE Rotational Molding Film
Features: Octene copolymerExceptional low temperature impact propertiesOutstanding stiffnessBroad processing windowSuperior whiteness for improved part appearanceEasy mold releaseNSF listed for Stan..
Impact Test 230 J
<br>@Thickness 6.35 mm,<br> Temperature -40.0 °C
170 ft-lb
<br>@Thickness 0.250 in,<br> Temperature -40.0 °F
ARM Low Temperature Impact on Rotomolded samples; ARM Method
NOVA Chemicals Surpass® RMs341-UG Octene sHDPE Rotational Molding Resin