| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Impact Test |
27.0
J <br>@Thickness 3.17 mm,<br> Temperature -40.0 °C
|
19.9
ft-lb <br>@Thickness 0.125 in,<br> Temperature -40.0 °F
|
Rotational Molded, Instrumented |
|
NOVA Chemicals Surpass® RMs539-U Octene sMDPE Rotational Molding Film
Features: Octene copolymerExceptional low temperature impact propertiesOutstanding stiffnessBroad processing windowSuperior whiteness for improved part appearanceEasy mold releaseNSF listed for Stan..
|
|||
| Impact Test |
27.0
J <br>@Thickness 3.17 mm,<br> Temperature -40.0 °C
|
19.9
ft-lb <br>@Thickness 0.125 in,<br> Temperature -40.0 °F
|
Rotational Molded, Instrumented |
|
NOVA Chemicals Surpass® RMs539-UG Octene sMDPE Rotational Molding Film
Features: Octene copolymerExceptional low temperature impact propertiesOutstanding stiffnessBroad processing windowSuperior whiteness for improved part appearanceEasy mold releaseNSF listed for Stan..
|
|||
| Impact Test |
27.0
J <br>@Temperature -30.0 °C
|
19.9
ft-lb <br>@Temperature -22.0 °F
|
Instrumented Impact Energy @ peak; ASTM D 3763 |
|
SABIC Innovative Plastics Noryl GTX GTX917 PPE+PS+PA
This data was supplied by SABIC-IP for the Americas region.
|
|||
| Impact Test |
27.0
J <br>@Temperature -18.0 °C
|
19.9
ft-lb <br>@Temperature -0.400 °F
|
ASTM D3763 |
|
Diamond Polymers Centrex® 825 Sheet Extrusion Grade
Centrex 825 resin is a high-gloss, high-impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, and it ..
|
|||
| Impact Test |
27.0
J <br>@Temperature 23.0 °C
|
19.9
ft-lb <br>@Temperature 73.4 °F
|
Total Energy; ASTM D3763 |
|
Diamond Polymers DIAMALOY GLY 7510 High Heat ASA Weatherable Polymer
Diamaloy GLY 7510 resin is a high gloss, high heat and high impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. This product is rated f1 by UL and be customed..
|
|||