| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| 100% Modulus | 0.00431 GPa | 0.625 ksi | |
|
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR N774 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
|
|||
| 100% Modulus | 0.00431 GPa | 0.625 ksi | |
|
Colorite Polymers Flexchem 5551-02 Vinyl Compound
Description: The Flexchem "51" series is a group of translucent, flexible, non-toxic vinyl compounds which were specifically developed to replace silicone in various applications. These compounds ut..
|
|||
| 100% Modulus | 0.00431 GPa | 0.625 ksi | ASTM D638 |
|
Colorite Polymers MULTICHEM™ 7014 Vinyl-Urethane Blend
Description: MULTICHEM™ is characterized by:Greater ResiliencyImproved ElasticityLow Temperature PropertiesLower ExtractabilityMolding and ExtrusionInformation provided by Colorite Polymers.
|
|||
| 100% Modulus | 0.00431 GPa | 0.625 ksi | ASTM D-638 |
|
Axiall 11701 Wire & Cable Flexible PVC
Non-lead stabilized, matte finish extrusion compound recommended for speaker wire and other general purpose extrusion applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corp..
|
|||
| 100% Modulus | 0.00431 GPa | 0.625 ksi | ASTM D-638 |
|
Axiall 6640 Moldings & Extrusions Flexible PVC
Injection molding compound specifically developed for footwear applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
|
|||
| 100% Modulus | 0.00431 GPa | 0.625 ksi | ASTM D638 |
|
Colorite Polymers 7014 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
|
|||
| 100% Modulus | 0.00431 GPa | 0.625 ksi | |
|
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR N774 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
|
|||