Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 100% Modulus = 2.35 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
100% Modulus 0.0162 GPa
2.35 ksi
Colorite Polymers Self Frosting™ 9511SF Vinyl Compound
Description: Colorite has developed a family of vinyl compounds to satisfy the needs of those who need a smooth, low gloss, low friction surface for the products that they produce. Historically, thi..
100% Modulus 0.0162 GPa
2.35 ksi
Colorite Polymers 9511 Clear Extrusion Vinyl Compound
Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for the extrusion of various components for the production of devices. The vinyl components used in pre..
100% Modulus 0.0162 GPa
2.35 ksi
Colorite Polymers 9512 Clear Injection Molding Vinyl Compound
Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for injection molding of various components such as drip chambers, connectors, valves, etc. The vinyl c..
100% Modulus 0.0162 GPa
2.35 ksi
ASTM D-638
Axiall 8940 Moldings & Extrusions Flexible PVC
General purpose semi-rigid extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.0162 GPa
2.35 ksi
ASTM D-638
Axiall 19470 Wire & Cable Flexible PVC
Semi-rigid, 105°C insulation compound recommended for a minimum wall thickness of 10 mils. Designed to meet the performance criteria of military spec. MIL-W-16878D.Information provided by Georgia ..
100% Modulus 0.0162 GPa
2.35 ksi
ASTM D-638
Axiall 01540 Plenum Flexible PVC
CAT 5 rated plenum jacket. UL QMTM2 Plenum Cable Compound Component.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.0162 GPa
2.35 ksi
ASTM D-638
Axiall 8490 Moldings & Extrusions Flexible PVC
A general purpose extrusion compound especially formulated for extruded T-moldings, tubings and other shapes where uniform flow through the die is required. Standard colors and black and natural.In..
100% Modulus 0.0162 GPa
2.35 ksi
ASTM D412
Lubrizol Estane® 2102-55D Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Load-bearing capacityAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product line from Dow in..
Copyright © lookpolymers.com All Rights Reserved