Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Elasticity = 3.00 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Modulus of Elasticity 2.00 - 3.00 GPa
290 - 435 ksi
ASTM D638-04
Proto3000 Objet Digital Materials™ DM_8210 Rigid Opaque Prototyping Polymer
Primary material: VeroBlueSecondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide the ..
Modulus of Elasticity 2.00 - 3.00 GPa
290 - 435 ksi
ASTM D638-04
Proto3000 Objet Digital Materials™ DM_8310 Rigid Opaque Prototyping Polymer
Primary material: VeroWhitePlusSecondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide..
Modulus of Elasticity 2.00 - 3.00 GPa
290 - 435 ksi
ASTM D638-04
Proto3000 Objet Digital Materials™ DM_8320 Rigid Opaque Prototyping Polymer
Primary material: VeroWhitePlusSecondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide..
Modulus of Elasticity 2.00 - 3.00 GPa
290 - 435 ksi
ASTM D638-04
Proto3000 Objet Digital Materials™ DM_8330 Rigid Opaque Prototyping Polymer
Primary material: VeroWhitePlusSecondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide..
Modulus of Elasticity 2.00 - 3.00 GPa
290 - 435 ksi
ASTM D638-04
Proto3000 Objet Digital Materials™ DM_Dots_7513 Transparent Prototyping Polymer
Primary material: FullCure720Secondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide t..
Modulus of Elasticity 2.00 - 3.00 GPa
290 - 435 ksi
ASTM D638-04
Proto3000 Objet Digital Materials™ DM_Grid_7523 Transparent Prototyping Polymer
Primary material: FullCure720Secondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide t..
Modulus of Elasticity 2.60 - 3.00 GPa
377 - 435 ksi
ASTM D638-04
Proto3000 Objet Digital Materials™ RGD5160-DM ABS-like Prototyping Polymer
Objet ABS-like Digital Material made of Object RGD515 & Objet RGD535Digital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to..
Modulus of Elasticity 2.00 - 3.00 GPa
290 - 435 ksi
ASTM D638-04
Proto3000 Objet FullCure720 Transparent Prototyping Polymer
Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid ..
Modulus of Elasticity 2.00 - 3.00 GPa
290 - 435 ksi
ASTM D638-04
Proto3000 Objet VeroBlack FullCure870 Rigid Opaque Prototyping Polymer
Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid ..
Modulus of Elasticity 2.00 - 3.00 GPa
290 - 435 ksi
ASTM D638-04
Proto3000 Objet VeroBlue FullCure840 Rigid Opaque Prototyping Polymer
Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid ..
Modulus of Elasticity 2.00 - 3.00 GPa
290 - 435 ksi
ASTM D638-04
Proto3000 Objet VeroClear FullCure810
Information provided by Proto3000 for their protoyping engineering services.
Modulus of Elasticity 2.00 - 3.00 GPa
290 - 435 ksi
ASTM D638-04
Proto3000 Objet VeroGray FullCure850 Rigid Opaque Prototyping Polymer
Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid ..
Modulus of Elasticity 2.50 - 3.00 GPa
363 - 435 ksi
Average value: 2.75 GPa Grade Count:4
Overview of materials for PVC, Uncompounded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Uncompounded". Each property range of values reported is minimum and maximum values of appropriate ..
Modulus of Elasticity 1.80 - 3.00 GPa
261 - 435 ksi
Average value: 2.34 GPa Grade Count:243
Overview of materials for Polycarbonate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri..
Modulus of Elasticity 2.00 - 3.00 GPa
290 - 435 ksi
ASTM D638-04
Proto3000 Objet VeroWhitePlus FullCure835 Rigid Opaque Prototyping Polymer
Information provided by Proto3000 for their protoyping engineering services.
Copyright © lookpolymers.com All Rights Reserved