| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Modulus of Elasticity | 350 - 400 GPa | 50800 - 58000 ksi | Young's modulus |
|
Momentive Performance Materials Niobium Carbide (NbC) Coating
High temperature protective coating for graphite.TaC, NbC, and ZrC coatings resist chemical attack by corrosive liquids and gases at very high temperatures. They are finding increasing acceptance i..
|
|||
| Modulus of Elasticity | 350 - 400 GPa | 50800 - 58000 ksi | Young's modulus |
|
Momentive Performance Materials Zirconium Carbide (ZrC) Coating
High temperature protective coating for graphite.TaC, NbC, and ZrC coatings resist chemical attack by corrosive liquids and gases at very high temperatures. They are finding increasing acceptance i..
|
|||