| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Modulus of Elasticity | 2.00 - 3.00 GPa | 290 - 435 ksi | ASTM D638-04 |
|
Proto3000 Objet Digital Materials™ DM_8210 Rigid Opaque Prototyping Polymer
Primary material: VeroBlueSecondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide the ..
|
|||
| Modulus of Elasticity | 2.00 - 3.00 GPa | 290 - 435 ksi | ASTM D638-04 |
|
Proto3000 Objet Digital Materials™ DM_8310 Rigid Opaque Prototyping Polymer
Primary material: VeroWhitePlusSecondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide..
|
|||
| Modulus of Elasticity | 2.00 - 3.00 GPa | 290 - 435 ksi | ASTM D638-04 |
|
Proto3000 Objet Digital Materials™ DM_8320 Rigid Opaque Prototyping Polymer
Primary material: VeroWhitePlusSecondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide..
|
|||
| Modulus of Elasticity | 2.00 - 3.00 GPa | 290 - 435 ksi | ASTM D638-04 |
|
Proto3000 Objet Digital Materials™ DM_8330 Rigid Opaque Prototyping Polymer
Primary material: VeroWhitePlusSecondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide..
|
|||
| Modulus of Elasticity | 2.00 - 3.00 GPa | 290 - 435 ksi | ASTM D638-04 |
|
Proto3000 Objet Digital Materials™ DM_Dots_7513 Transparent Prototyping Polymer
Primary material: FullCure720Secondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide t..
|
|||
| Modulus of Elasticity | 2.00 - 3.00 GPa | 290 - 435 ksi | ASTM D638-04 |
|
Proto3000 Objet Digital Materials™ DM_Grid_7523 Transparent Prototyping Polymer
Primary material: FullCure720Secondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide t..
|
|||
| Modulus of Elasticity | 2.60 - 3.00 GPa | 377 - 435 ksi | ASTM D638-04 |
|
Proto3000 Objet Digital Materials™ RGD5160-DM ABS-like Prototyping Polymer
Objet ABS-like Digital Material made of Object RGD515 & Objet RGD535Digital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to..
|
|||
| Modulus of Elasticity | 2.00 - 3.00 GPa | 290 - 435 ksi | ASTM D638-04 |
|
Proto3000 Objet FullCure720 Transparent Prototyping Polymer
Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid ..
|
|||
| Modulus of Elasticity | 2.00 - 3.00 GPa | 290 - 435 ksi | ASTM D638-04 |
|
Proto3000 Objet VeroBlack FullCure870 Rigid Opaque Prototyping Polymer
Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid ..
|
|||
| Modulus of Elasticity | 2.00 - 3.00 GPa | 290 - 435 ksi | ASTM D638-04 |
|
Proto3000 Objet VeroBlue FullCure840 Rigid Opaque Prototyping Polymer
Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid ..
|
|||
| Modulus of Elasticity | 2.00 - 3.00 GPa | 290 - 435 ksi | ASTM D638-04 |
|
Proto3000 Objet VeroClear FullCure810
Information provided by Proto3000 for their protoyping engineering services.
|
|||
| Modulus of Elasticity | 2.00 - 3.00 GPa | 290 - 435 ksi | ASTM D638-04 |
|
Proto3000 Objet VeroGray FullCure850 Rigid Opaque Prototyping Polymer
Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid ..
|
|||
| Modulus of Elasticity | 2.50 - 3.00 GPa | 363 - 435 ksi | Average value: 2.75 GPa Grade Count:4 |
|
Overview of materials for PVC, Uncompounded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Uncompounded". Each property range of values reported is minimum and maximum values of appropriate ..
|
|||
| Modulus of Elasticity | 1.80 - 3.00 GPa | 261 - 435 ksi | Average value: 2.34 GPa Grade Count:243 |
|
Overview of materials for Polycarbonate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri..
|
|||
| Modulus of Elasticity | 2.00 - 3.00 GPa | 290 - 435 ksi | ASTM D638-04 |
|
Proto3000 Objet VeroWhitePlus FullCure835 Rigid Opaque Prototyping Polymer
Information provided by Proto3000 for their protoyping engineering services.
|
|||