Mechanical Properties Metric English Comments
Modulus of Elasticity 380 GPa
55100 ksi
Plansee DENSIMET® D180 Tungsten-Nickel-Iron Alloy
Characteristics:Easy processingHigh densityPrecision forming and machiningHigh ductilityHigh strength100 % impermeableTypical Applications:Balancing weights in motors and drive componentsVibration d..
Modulus of Elasticity 380 GPa
55100 ksi
H.C. Starck HPM 1850W Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
Modulus of Elasticity 380 GPa
55100 ksi
H.C. Starck HPM 1850 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
Modulus of Elasticity 380 GPa
55100 ksi
Specialty Materials SCS-6 Silicon Carbide Monofilament
High strength at high temperature. These fibers are used in metal, ceramic and polymer matrix composites and are extremely effective for high-temperature applications. Silicon carbide reinforced tit..
Modulus of Elasticity 380 GPa
55100 ksi
Sapco 99.7% Aluminum Oxide
Information provided by Sapco.
Modulus of Elasticity 380 GPa
55100 ksi
ASTM E494
M Cubed Technologies RBBC-751 Reaction Bonded Boron Carbide
Reaction-bonded boron carbide for extreme wear environments. Can be cast into very large components (greater than 4 ft. square)Information provided by M Cubed Technologies, Inc.
Modulus of Elasticity 380 GPa
55100 ksi
ASTM E494
M Cubed Technologies SSC-802 Reaction-Bonded Silicon Carbide
Medium-grained reaction-bonded SiC for high wear applications. Bullnoses, fan liners, hydrocyclone liners, etc. Can be cast into very large shapes (greater than 4 ft. square, 5-6 inches thick)Info..
Modulus of Elasticity 380 GPa
55100 ksi
Zircar Ceramics HC Sapphire (Single Crystal Aluminum Oxide) Hangar Clip
ZIRCAR hanger clips are comprised of sapphire (single crystal aluminum oxide) and are designed for use with hanger rod (HR-1). The single crystal structure of these clips prevents creep and deformat..
Modulus of Elasticity 380 GPa
55100 ksi
In Tension
Cytec Thornel® P-55S 2K Carbon Fiber, Pitch Precursor
Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous filament, high modulus strands made from a pitch precursor. The fiber surface has been treated to increase the interla..