Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tangent Modulus = 1586 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Tangent Modulus 1586 MPa
230000 psi
ASTM D790
Flint Hills AP5106-HA Polypropylene Impact Copolymer
Features: Excellent impact stiffness balance, good mold release.Applications: Compression and injection molding: caps and closuresInformation Provided by Flint Hills Resources
Tangent Modulus 1586 MPa
230000 psi
ASTM D790
Flint Hills AP5206-HN Polypropylene Impact Copolymer
Features: Nucleated for fast cycle and good mold release. Product does not contain animal derived components.Applications: Compression and injection molding: caps and closuresInformation Provided b..
Copyright © lookpolymers.com All Rights Reserved