| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Adhesive Bond Strength | 1.38 MPa | 200 psi | Polystyrene, Substrate Failure, Shear; ASTM D1002 |
|
Permabond 930 Cyanoacrylate
PERMABOND 930 is a low odor, nonfogging, nonfrosting cyanoacrylate. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate adhesives on hot and humid days, is eliminated. The ..
|
|||
| Adhesive Bond Strength | 1.38 MPa | 200 psi | Polystyrene, Substrate Failure, Shear; ASTM D1002 |
|
Permabond 931 Cyanoacrylate
PERMABOND 931 is a low odor, nonfogging, nonfrosting cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate adhesiv..
|
|||
| Adhesive Bond Strength | 1.38 MPa | 200 psi | Polystyrene, Substrate Failure, Shear; ASTM D1002 |
|
Permabond 932 Cyanoacrylate
PERMABOND 932 is a low odor, nonfogging, nonfrosting cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate adhesiv..
|
|||
| Adhesive Bond Strength | 1.38 MPa | 200 psi | Polystyrene, Substrate Failure, Shear; ASTM D1002 |
|
Permabond 935 Cyanoacrylate
The PERMABOND 930 series is a family of low odor, non-fogging, non-frosting cyanoacrylates. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyano..
|
|||
| Adhesive Bond Strength | 1.38 MPa | 200 psi | Typical lap shear |
|
Momentive Performance Materials RTV106 Red Adhesive Sealant, High Strength, High Temperature Paste
One-part alkoxy cure. Typical uses: High-heat applications; encapsulate and seal heating elements.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of Momentive Performance..
|
|||
| Adhesive Bond Strength | 1.38 MPa | 200 psi | Typical lap shear |
|
Momentive Performance Materials RTV133 Black Adhesive Sealant, Flame Retardant Paste
One-part alkoxy cure. Typical uses: As a sealant on firewalls or as a flame retardant coating. Use in switching devices, motors, and high voltage transformers.Data provided by the manufacturer, GE..
|
|||
| Adhesive Bond Strength | 1.38 MPa | 200 psi | Typical lap shear |
|
Momentive Performance Materials RTV1473 Black Adhesive Sealant, FIPG
One-part acetoxy cure. Typical uses: Heavy bodied adhesive sealant for formed-in-place gasketing. Good oil resistance.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of ..
|
|||
| Adhesive Bond Strength | 1.38 MPa | 200 psi | Typical lap shear |
|
Momentive Performance Materials RTV167 Gray Adhesive Sealant, Non-Corrosive High Strength
One-part totally non-corrosive alkoxy cure. Alkoxy cure silicones are neutral cure materials that offer exceptional adhesion and are non-corrosive to most metals. Typical uses: Highest strength ad..
|
|||
| Adhesive Bond Strength | 1.38 MPa | 200 psi | Typical lap shear |
|
Momentive Performance Materials FRV1106 Red Fluorosilicone Adhesive Sealant, Fuel Resistant Paste
One-part acetoxy cure. Alkoxy cure silicones are neutral cure materials that offer exceptional adhesion and are non-corrosive to most metals. Typical uses: For use in contact with fuel, solvents, ..
|
|||
| Adhesive Bond Strength | 1.38 MPa | 200 psi | Typical lap shear |
|
Momentive Performance Materials FRV1107 Gray Adhesive Sealant, Fuel Resistant Paste
One-part acetoxy cure. Typical uses: For use in contact with fuel, solvents, and chemicals.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of Momentive Performance Materi..
|
|||
| Adhesive Bond Strength | 1.38 MPa | 200 psi | Typical lap shear |
|
Momentive Performance Materials IS806 Red Adhesive Sealant, General Purpose Paste
One-part alkoxy cure. Typical uses: High-heat applications; encapsulate and seal heating elements.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of Momentive Performance..
|
|||
| Adhesive Bond Strength | 1.38 MPa | 200 psi | Lap shear, alum to alum |
|
Tra-Con Tra-Bond 2106T Fast Cure Thixotropic Epoxy Adhesive
TRA-BOND 2106T is an exceptional epoxy formulation recommended for lower temperature or wet industrial bonding applications where FAST CURING is required. This versatile two-part epoxy system contai..
|
|||
| Adhesive Bond Strength | 1.38 MPa | 200 psi | Al-to-Al Lap Shear; Cured property, scuff sanded, IPA wiped T3-202Al; cohesive failure; ASTM D1002 |
|
Aptek 2312-PMF Electrically conductive, low modulus adhesive
Premixed-frozen, electrically conductive, low modulus adhesiveAPTEK 2312-PMF is a one component, premixed-frozen, silver filled, electrically conductive soft paste adhesive. It is designed to bond m..
|
|||
| Adhesive Bond Strength | 1.38 MPa | 200 psi | |
|
Atom Adhesives AA-BOND 201 Epoxy Adhesive
AA-BOND 201 is an exceptional epoxy formulation recommended for lower temperature or wet industrial bonding applications where FAST CURING is required. AA-BOND 201 is versatile two-part epoxy system..
|
|||