Polymer Property : Adhesive Bond Strength = 10.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 8.00 - 10.0 MPa
1160 - 1450 psi
Zinc, Shear; ISO 4587
Permabond 101 Cyanoacrylate, Wicking Viscosity
PERMABOND® 101 is a low viscosity product useful in wicking or penetrating applications or bonding closely fitting parts. It is fast setting and suitable for use on plastics, rubber and metals. Cya..
Adhesive Bond Strength 9.00 - 10.0 MPa
1310 - 1450 psi
Glass/steel, Shear
Permabond UV620 UV-curable Adhesive
PERMABOND UV620 is a single part, fast curing, UV curable adhesive. Its excellent optical clarity and resistance to yellowing make it ideal for bonding glass and crystal for a high quality finish. I..
Adhesive Bond Strength 8.00 - 10.0 MPa
1160 - 1450 psi
Zinc, Shear
Permabond 102 Cyanoacrylate, General purpose
PERMABOND® 102 is a low viscosity general purpose cyanoacrylate adhesive suitable for bonding close-fitting components. It is fast setting and suitable for use on plastics, rubber and metals. Cyano..