| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Adhesive Bond Strength | 8.27 MPa | 1200 psi | Lap shear; 2024 T3 Al Abraded / MEK Wipe |
| Resinlab® EP1112 Clear Electronic Grade Epoxy Encapsulant Resinlab™ EP 1112 Clear is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexib.. |
|||
| Adhesive Bond Strength | 8.30 MPa | 1200 psi | Per ASTM D1002-94; shear strength of single lap-joint metal coupons in tension loading. |
| Aremco Aremco-Bond™ 597 Conductive Epoxy Adhesive
(discontinued **) Electrically and thermally conductive, silver-filled, one-part paste. Inorganic system for adhesive (597A) & coating (597C) applications to 1200 ºF (650 °C). |
|||
| Adhesive Bond Strength | 8.30 MPa | 1200 psi | Aluminum, Shear |
| Permabond 200 Cyanoacrylate, wire tacking PERMABOND 200 is a high viscosity product with good flow control useful in wire tacking applications or bonding components. It is fast setting and suitable for use on plastics, rubber and metals. Cy.. |
|||
| Adhesive Bond Strength | 8.30 MPa | 1200 psi | Aluminum, Shear |
| Permabond 260 Cyanoacrylate PERMABOND 260 is a low viscosity cyanoacrylate ideal for wicking type application. PERMABOND 260 provides faster set times and improved gap-filling capability compared to conventional cyanoacrylates.. |
|||
| Adhesive Bond Strength | 8.30 MPa | 1200 psi | Aluminum, Shear |
| Permabond 265 Cyanoacrylate PERMABOND 265 is a medium viscosity cyanoacrylate ideal for intermediate gap fill application. PERMABOND 265 provides faster set times and improved gap-filling capability compared to conventional cy.. |
|||
| Adhesive Bond Strength | 8.27 MPa | 1200 psi | lap shear (on grit blasted steel, bond line thickness of 0.010"); ASTM D1002 |
| ITW Devcon Safety Clear Coatâ„¢ Epoxy, Water Clear Information provided by ITW Devcon |
|||
| Adhesive Bond Strength | 8.27 MPa | 1200 psi | ABS-ABS; Substrate Failure; Tensile Lap Shear |
| Master Bond MB306 Low Viscosity Methyl Cyanoacrylate Features superior bonding properties. Master Bond MB306 is a single component, low viscosity, rapid setting, methyl cyanoacrylate adhesive. Similar to other types of “super glue”, MB306 cures ver.. |
|||
| Adhesive Bond Strength | 8.27 MPa | 1200 psi | Lap shear, alum to alum, 24 hrs @ 25°C |
| Tra-Con Tra-Duct 2907 Silver-Filled Epoxy Adhesive TRA-DUCT 2907 is an electrically conducting silver-filled medium viscosity epoxy compound recommended for electronic bonding and sealing applications that require a combination of good mechanical an.. |
|||
| Adhesive Bond Strength | >= 8.27 MPa | >= 1200 psi | shear, Al/Al |
| Master Bond EP21FRNS-2 Two Component, Flame Resistant Epoxy System Master Bond Polymer System EP21FRNS-2 is a two component, room temperature curing, flame retardant compound for potting, encapsulating and casting. Particularly noteworthy are its low smoke generati.. |
|||
| Adhesive Bond Strength | 8.27 MPa | 1200 psi | |
| Trelleborg Emerson & Cuming Eccobond® 930-09 Low Temperature Performance Lighting Epoxy Adhesive Emerson & Cuming 930-09 Eccobond® Low Temperature Performance Lighting Epoxy AdhesiveFlexible, non-blushing, epoxy adhesive for glass headlamp bonding. Maintains flexibility at temperatures as low .. |
|||
| Adhesive Bond Strength | >= 8.27 MPa | >= 1200 psi | Lap Shear Strength |
| Epoxyset Epoxiohm EO-98HT Electrically Conductive Epoxy Adhesive EO-98HT is a one component, electrically and thermally conductive, snap cure, die attach epoxy. It was designed for IC plastic packaging of semiconductors, hybrid micro-electronics, and photonic dev.. |
|||
| Adhesive Bond Strength | 8.27 MPa @Temperature 82.2 °C |
1200 psi @Temperature 180 °F |
Aluminum-Aluminum tensile shear |
| Armstrong A-2/W Epoxy Adhesive This off-white paste epoxy is a versatile adhesive systems. The choice of one of four recommended Activators (A, E, W or H-20) makes A-2 Adhesive an ideal choice for many applications. A-2 with Ac.. |
|||
| Adhesive Bond Strength | 8.27 MPa | 1200 psi | Al-to-Al Lap Shear; Cured property; ASTM D1002 |
| Aptek 2209-A/B Clear, non-yellowing urethane adhesive APTEK 2209-A/B is a water clear, thixotropic, two component, electrically insulating, urethane adhesive designed for bonding various substrates. APTEK 2209-A/B is effective for bonding plastics and.. |
|||
| Adhesive Bond Strength | 8.27 MPa | 1200 psi | Lap shear; 2024 T3 Al Abraded / MEK Wipe |
| Resinlab® EP1112 Black Electronic Grade Epoxy Encapsulant Resinlab™ EP 1112 Black is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexib.. |
|||
| Adhesive Bond Strength | 8.30 MPa | 1200 psi | Aluminum, Shear |
| Permabond 262 Cyanoacrylate PERMABOND 262 is a low viscosity cyanoacrylate ideal for wicking type application. PERMABOND 262 provides faster set times and improved gap-filling capability compared to conventional cyanoacrylates.. |
|||