| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Adhesive Bond Strength | >= 9.00 MPa | >= 1310 psi | ABS, Substrate Failure, Shear; ISO 4587 |
|
Permabond 170 Cyanoacrylate, gap filling
PERMABOND® 170 is a methyl cyanoacrylate adhesive. It is a single part, high viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. Permabond 170 w..
|
|||
| Adhesive Bond Strength | >= 9.00 MPa | >= 1310 psi | ABS, Substrate Failure, Shear; ISO 4587 |
|
Permabond 2011 Cyanoacrylate, gel
PERMABOND® 2011 is a thixotropic, fast-setting cyanoacrylate particularly suitable for use on vertical and porous substrates. This material can be used on metals, plastics, elastomers, ceramics and..
|
|||
| Adhesive Bond Strength | 9.00 MPa | 1310 psi | Steel/steel after 3 mins, Shear |
|
Permabond TA459 Toughened Acrylic Adhesive
Permabond TA459 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This product was specifically designed to be non-corrosive to sens..
|
|||
| Adhesive Bond Strength | 9.00 MPa | 1310 psi | Steel/steel after 3 mins, Shear |
|
Permabond TA4590 Toughened Acrylic Adhesive
Permabond TA4590 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This product was specifically designed to be non-corrosive to sen..
|
|||
| Adhesive Bond Strength | 9.00 - 10.0 MPa | 1310 - 1450 psi | Glass/steel, Shear |
|
Permabond UV620 UV-curable Adhesive
PERMABOND UV620 is a single part, fast curing, UV curable adhesive. Its excellent optical clarity and resistance to yellowing make it ideal for bonding glass and crystal for a high quality finish. I..
|
|||
| Adhesive Bond Strength | >= 9.00 MPa | >= 1310 psi | Polycarbonate, Shear |
|
Permabond UV645 UV-curable Adhesive
PERMABOND UV645 is a single part, fast curing, high viscosity UV curable adhesive designed specifically for bonding plastics. This material has excellent adhesion to a variety of plastics including ..
|
|||
| Adhesive Bond Strength | >= 9.00 MPa | >= 1310 psi | Polycarbonate, Shear |
|
Permabond UV649 UV-curable Adhesive
PERMABOND UV649 is a single part, fast setting, and UV curable adhesive designed specifically for bonding plastics. This material has excellent adhesion to a variety of plastics including polycarbon..
|
|||
| Adhesive Bond Strength | 9.00 - 11.0 MPa | 1310 - 1600 psi | FRP Glass/Epoxy, Shear; ASTM D1002 |
|
Permabond ES569 Epoxy Resin
PERMABOND® ES569 is a single-part heat cured epoxy adhesive with excellent adhesion to metal surfaces as well as composite materials. The high bond strength of this adhesive allows it to replace me..
|
|||
| Adhesive Bond Strength | >= 9.00 MPa | >= 1310 psi | Polycarbonate, Shear |
|
Permabond UV630 UV-curable Adhesive
PERMABOND UV630 is a single part, fast setting, and UV curable adhesive designed specifically for bonding plastics. This material has excellent adhesion to a variety of plastics including polycarbon..
|
|||
| Adhesive Bond Strength | >= 9.00 MPa | >= 1310 psi | Phenolic, Substrate Failure, Shear; ISO 4587 |
|
Permabond 910FS Cyanoacrylate, Methyl grade
PERMABOND® 910FS is the original 100%-methyl cyanoacrylate adhesive. It is a single part, low viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts..
|
|||
| Adhesive Bond Strength | >= 9.00 MPa | >= 1310 psi | ABS, Substrate Failure, Shear; ISO 4587 |
|
Permabond 910FS Cyanoacrylate, Methyl grade
PERMABOND® 910FS is the original 100%-methyl cyanoacrylate adhesive. It is a single part, low viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts..
|
|||