Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Adhesive Bond Strength = 1310 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 7.00 - 9.00 MPa
1020 - 1310 psi
Aluminum, Shear; ISO 4587
Permabond 101 Cyanoacrylate, Wicking Viscosity
PERMABOND® 101 is a low viscosity product useful in wicking or penetrating applications or bonding closely fitting parts. It is fast setting and suitable for use on plastics, rubber and metals. Cya..
Adhesive Bond Strength 7.00 - 9.00 MPa
1020 - 1310 psi
Aluminum, Shear; ISO 4587
Permabond 2010 Cyanoacrylate, gap filling
PERMABOND 200 is a high viscosity product with good flow control useful in wire tacking applications or bonding components. It is fast setting and suitable for use on plastics, rubber and metals. Cy..
Adhesive Bond Strength 8.00 - 9.00 MPa
1160 - 1310 psi
Aluminum, Shear; ISO 4587
Permabond 2011 Cyanoacrylate, gel
PERMABOND® 2011 is a thixotropic, fast-setting cyanoacrylate particularly suitable for use on vertical and porous substrates. This material can be used on metals, plastics, elastomers, ceramics and..
Adhesive Bond Strength 8.00 - 9.00 MPa
1160 - 1310 psi
Aluminum, Shear; ISO 4587
Permabond 940 Cyanoacrylate, low odor
PERMABOND 940 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad..
Adhesive Bond Strength 8.00 - 9.00 MPa
1160 - 1310 psi
Glass/steel, Shear
Permabond UV670 UV-curable Adhesive
PERMABOND UV670 is a single part, fast curing, UV curable adhesive. The cured adhesive is tough, flexible and has excellent impact resistance. Permabond UV670 is well suited for bonding glass to met..
Adhesive Bond Strength 7.00 - 9.00 MPa
1020 - 1310 psi
Aluminum, Shear
Permabond 102 Cyanoacrylate, General purpose
PERMABOND® 102 is a low viscosity general purpose cyanoacrylate adhesive suitable for bonding close-fitting components. It is fast setting and suitable for use on plastics, rubber and metals. Cyano..
Adhesive Bond Strength 8.00 - 9.00 MPa
1160 - 1310 psi
Aluminum, Shear; ISO 4587
Permabond 240 Cyanoacrylate, gap filling
PERMABOND® 240 is a high viscosity product useful in large gap applications. It is ideal for porous substrates. It is fast setting and suitable for use on plastics, rubber and metals. Cyanoacrylate..
Adhesive Bond Strength 8.00 - 9.00 MPa
1160 - 1310 psi
Aluminum, Shear; ISO 4587
Permabond 920 Cyanoacrylate, High temperature
PERMABOND® 920 is the original allyl cyanoacrylate adhesive. It is a single part, low viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. PERMAB..
Adhesive Bond Strength 8.00 - 9.00 MPa
1160 - 1310 psi
Aluminum, Shear; ISO 4587
Permabond 941 Cyanoacrylate, low odor
PERMABOND 941 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad..
Adhesive Bond Strength 8.00 - 9.00 MPa
1160 - 1310 psi
Aluminum, Shear; ISO 4587
Permabond 943 Cyanoacrylate, low odor
PERMABOND 943 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad..
Adhesive Bond Strength 8.00 - 9.00 MPa
1160 - 1310 psi
Aluminum, Shear; ISO 4587
Permabond 947 Cyanoacrylate, low odor
PERMABOND 947 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad..
Copyright © lookpolymers.com All Rights Reserved