| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Adhesive Bond Strength | 10.3 MPa | 1500 psi | Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37 |
|
Resinlab® EP1287 Filled, Flame Retardant Epoxy Syntactic Foam
Resinlab™ EP1287 is a two part filled, flame retardant epoxy syntactic foam. It utilizes glass microspheres to reduce cured density and improve machinability. This product will be self-extinguishin..
|
|||
| Adhesive Bond Strength | 10.3 MPa | 1500 psi | Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37 |
|
Resinlab® EP1325 Thixotropic, Heat Curing Epoxy Adhesive
Resinlab™ EP1325 and EP1325LV are one part thixotropic, heat curing epoxy adhesives. They can also be used as a small mass potting compounds, staking or damming adhesives, or polymer systems where ..
|
|||
| Adhesive Bond Strength | 10.3 MPa | 1500 psi | Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37 |
|
Resinlab® EP1330 Heat Cure Epoxy Polymer System
Resinlab™ EP1330 and EP1330LV are one part heat cure epoxy polymer systems. They can also be used as a small mass potting or staking compounds, or a dam adhesive in and “dam and fill” application..
|
|||
| Adhesive Bond Strength | 10.3 MPa | 1500 psi | Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37 |
|
Resinlab® EP965 Clear Unfilled Electronic Grade Epoxy Encapsulant
Resinlab™ EP965 Clear is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting ..
|
|||
| Adhesive Bond Strength | 10.3 MPa | 1500 psi | lap shear (on grit blasted steel, bond line thickness of 0.010"); ASTM D1002 |
|
ITW Devcon Flex Welderâ„¢ Methacrylate Adhesive, Off-White
Information provided by ITW Devcon
|
|||
| Adhesive Bond Strength | 10.3 MPa | 1500 psi | Lap shear, alum to alum, 1 hr @ 65°C |
|
Tra-Con Tra-Bond 216C03 Flexible Plastic Bonder
TRA-BOND 216C03 is a flexible thixotropic bonding adhesive designed for bonding all types of plastics including nylon, PVC, polyethylene, acrylic, lexan, polypropylene, kapton or almost any thermopl..
|
|||
| Adhesive Bond Strength | 10.3 MPa | 1500 psi | Lap shear, alum to alum |
|
Tra-Con Tra-Bond 9349J Room Temperature Cure Flexible Epoxy Adhesive
TRA-BOND 9349J epoxy adhesive is a flexible, two part, room temperature curing system with high peel and sheer strengths. TRA-BOND 9349J is excellent for bonding many metals and woods, most plastics..
|
|||
| Adhesive Bond Strength | 10.3 MPa | 1500 psi | Lap shear, alum to alum, 2 hrs @ 65°C |
|
Tra-Con Tra-Duct 2907 Silver-Filled Epoxy Adhesive
TRA-DUCT 2907 is an electrically conducting silver-filled medium viscosity epoxy compound recommended for electronic bonding and sealing applications that require a combination of good mechanical an..
|
|||
| Adhesive Bond Strength | 10.3 MPa | 1500 psi | Lap shear, alum to alum |
|
Tra-Con Tra-Duct 921M01 Low Viscosity Long Pot Life Silver-Filled Epoxy
TRA-DUCT 921M01 is a two component, silver-filled electrically conductive epoxy adhesive designed for applications which require electrical conductivity and a long pot life at a relatively low heat ..
|
|||
| Adhesive Bond Strength | 10.3 MPa | 1500 psi | Lap shear, alum to alum |
|
Tra-Con Tra-Duct 925M01 Low Ion Snap Cure Silver-Filled Epoxy
TRA-DUCT 925M01 is a low ion snap cure silver-filled epoxy. TRA-DUCT 925M01 develops strong, durable, void free electrically and thermally conducting bonds. The product can be screen printed, stenci..
|
|||
| Adhesive Bond Strength | >= 10.3 MPa | >= 1500 psi | Shear, Al/Al, after 30 days at 400°F |
|
Master Bond Supreme 33CLV Two Component, Room Temperature Curing Toughened Epoxy
Master Bond Polymer System Supreme 33CLV is a special, room temperature curing, toughened epoxy adhesive/sealant, featuring exceptionally high temperature resistance. This innovative system has outs..
|
|||
| Adhesive Bond Strength | 10.3 MPa | 1500 psi | Lap shear, alum to alum, 1 hr @ 65°C |
|
Tra-Con Tra-Bond 2204
Information provided by Tra-Con Inc.
|
|||
| Adhesive Bond Strength | 10.3 MPa | 1500 psi | |
|
Trelleborg Emerson & Cuming Eccobond® G757 One-Component High Strength-Impact Resistant Epoxy Adhesive
Emerson & Cuming G757 Eccobond® One-Component High Strength-Impact Resistant Epoxy AdhesiveVery flexible, thixotropic, epoxy adhesive. Excellent low temperature resistance. Excellent adhesion to gl..
|
|||
| Adhesive Bond Strength |
10.3
MPa @Temperature 25.0 °C |
1500
psi @Temperature 77.0 °F |
Aluminum-Aluminum tensile shear |
|
Armstrong A-271 Epoxy Adhesive
A clear amber adhesive system. A-271 is a medium viscosity liquid with excellent wetting ability. It is ideal for bonding glass or similar smooth surfaces. It features very low shrinkage coupled ..
|
|||
| Adhesive Bond Strength |
10.3
MPa @Temperature 82.2 °C |
1500
psi @Temperature 180 °F |
Aluminum-Aluminum tensile shear |
|
Armstrong X-81-A/F Epoxy Adhesive
Information provided by Ellsworth Adhesives.
|
|||
| Adhesive Bond Strength | >= 10.3 MPa | >= 1500 psi | Steel (epoxy primer), Primer Failure; ASTM D4541 Elcometer |
|
ACC EP AEP EPI Engineered Polymers
EP AEP is a new generation of Internetwork Polymers of polyurea and Epoxy, “Powered by Reactamine® Technology”. EP AEP was developed for a colorfast floor for both residential and industrial appl..
|
|||
| Adhesive Bond Strength | >= 10.3 MPa | >= 1500 psi | Steel (no primer), Substrate Failure; ASTM D4541 Elcometer |
|
ACC EP LCP EPI Engineered Polymers Aromatic Polyurea
EP LCP Aromatic Polyurea, “Powered by Reactamine® Technology” is a two component 100% solid Polyurea (silicone optional) with superior performance in industrial applications. EP LCP displays extr..
|
|||
| Adhesive Bond Strength | >= 10.3 MPa | >= 1500 psi | Steel (epoxy primer), Primer Failure; ASTM D4541 Elcometer |
|
ACC EP RAP 45 EPI Engineered Polymers Aliphatic Polyurea
EP RAP 45 Aliphatic Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solids, no VOC is, aliphatic polyurea (silicone optional) coating, that was developed for UV stable (col..
|
|||
| Adhesive Bond Strength | >= 10.3 MPa | >= 1500 psi | Steel (epoxy primer), Primer Failure; ASTM D4541 Elcometer |
|
ACC EP RAP-1567 EPI Engineered Polymers Aliphatic Polyurea
RAP-1567 HX is a two component 100% solids, no VOC’s, aliphatic polyureas “Powered by ReactAmine® Technology” that was developed for UV stable (colorfast) polyurea applications. This new generat..
|
|||
| Adhesive Bond Strength | >= 10.3 MPa | >= 1500 psi | Steel (epoxy primer), Primer Failure; ASTM D4541 Elcometer |
|
ACC EP RAP-1567 SP-HX EPI Engineered Polymers Silicone Aliphatic Polyurea
RAP-1567 SP-HX is a two component 100% solids, no VOC’s, silicone aliphatic polyureas “Powered by ReactAmine® Technology” that was developed for UV stable (colorfast) polyurea applications. This..
|
|||
| Adhesive Bond Strength | >= 10.3 MPa | >= 1500 psi | Steel (no primer), Substrate Failure; ASTM D4541 Elcometer |
|
ACC EP RASP EPI Engineered Polymers Aliphatic Silicone Polymer
EP RASP Aliphatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Polyurea that has excellent UV stability (colorfast) with superior performance in industria..
|
|||
| Adhesive Bond Strength | >= 10.3 MPa | >= 1500 psi | Steel (no primer), Substrate Failure; ASTM D4541 Elcometer |
|
ACC EP RPSP EPI Engineered Polymers Aliphatic Silicone Polymer
EP RPSP Aromatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Polyurea with superior performance in industrial applications. EP RPSP displays extremely fa..
|
|||
| Adhesive Bond Strength | >= 10.3 MPa | >= 1500 psi | Steel (no primer), Substrate Failure; ASTM D4541 Elcometer |
|
ACC EP WQS EPI Engineered Polymers Water Base Quick Set Epoxy
EP WQS Water Base Quick Set, “Powered by Reactamine® Technology”, is a two component 60% solids, no VOC, self-leveling modified epoxy. This versatile new generation epoxy displays low blush, fast..
|
|||
| Adhesive Bond Strength | >= 10.3 MPa | >= 1500 psi | Steel (no primer), Substrate Failure; ASTM D4541 Elcometer |
|
ACC SMP™ EP EF SP EPI Engineered Polymers Extra Flex with Silicone
EP EF SP, “Powered by Reactamine® Technology”, is a two component 100% solid Silicone Polyurea with superior performance in industrial applications. EP EF SP displays extremely fast cure times wi..
|
|||
| Adhesive Bond Strength | 10.3 MPa | 1500 psi | |
|
Atom Adhesives AA-DUCT AD1 Epoxy Adhesive
AA-DUCT AD1 is a single component epoxy, formulated with pure silver power combined with organic binders and solvents to produce electrically conductive paths, films or patterns over non-conductive ..
|
|||
| Adhesive Bond Strength | 10.3 MPa | 1500 psi | cured |
|
Atom Adhesives AA-DUCT CG2 Epoxy Adhesive
AA-DUCT CG2 is a single component epoxy, formulated with silver coated ceramic that results in lower material costs without adversely sacrificing the properties obtained with a pure silver formulati..
|
|||
| Adhesive Bond Strength | >= 10.3 MPa | >= 1500 psi | Steel (no primer), Substrate Failure; ASTM D4541 Elcometer |
|
ACC EP QS EPI Engineered Polymers Quick Set Epoxy
EP QS Quick Set Epoxy, “Powered by Reactamine® Technology”, is a two component 100% solids, no VOC, self-leveling modified epoxy. This versatile new generation epoxy displays low blush, fast cure..
|
|||
| Adhesive Bond Strength | >= 10.3 MPa | >= 1500 psi | Steel (no primer), Substrate Failure; ASTM D4541 Elcometer |
|
ACC ReactAmine® EP 350 EPI Engineered Polymers Polyurea
ReactAmine® EP-350 is a two component 100% solid Polyurea with superior performance in industrial applications. EP-350 displays extremely fast cure times with excellent adhesions to different subst..
|
|||
| Adhesive Bond Strength | 10.3 MPa | 1500 psi | Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37 |
|
Resinlab® EP1199 Black Unfilled Epoxy Adhesive
Resinlab™ EP1199 Black is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. This product gives good resistance to water, salt spray, inorganic acids and..
|
|||