Polymer Property : Adhesive Bond Strength = 17.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 17.0 MPa
2470 psi
Resin Technology Group 310 Porous Fill, Slow Set Fusion™ Cyanoacrylate Instant Ethyl Adhesive
Resin Technology Group 310 Porous Fill, Slow Set Fusion™ Cyanoacrylate Instant Ethyl Adhesive
Adhesive Bond Strength 17.0 - 31.0 MPa
2470 - 4500 psi
Aluminum, Shear; ASTM D1002
Permabond ES550 Epoxy Resin
PERMABOND ES550 is a single-part epoxy paste which is slump-resistant (does not flow) during cure. The adhesive is toughened for maximum impact resistance, along with excellent peel and shear streng..
Adhesive Bond Strength 17.0 - 31.0 MPa
2470 - 4500 psi
Aluminum, Shear; ASTM D1002
Permabond ES558 Epoxy Resin
PERMABOND ES558 is a single-part epoxy paste which flows like solder when heated during curing. The adhesive is toughened for maximum impact resistance, along with excellent peel and shear strength...
Adhesive Bond Strength 17.0 - 31.0 MPa
2470 - 4500 psi
Aluminum, Shear; ASTM D1002
Permabond ES578 Epoxy Resin
PERMABOND® ES578 is a single-part heat cured epoxy adhesive with excellent adhesion to metal surfaces, ceramics as well as composite materials. ES578 provides excellent thermal conductivity and bon..
Adhesive Bond Strength 17.0 MPa
2470 psi
steel collar and pin shear; ISO 10123
Permabond HH120 Anaerobic Threadlocker
Permabond® HH120 Threadlocker is an excellent general purpose threadlocker and sealant. It is used for locking bolts, nuts and screws that require permanent assembly. Its high viscosity allows for ..
Adhesive Bond Strength 17.0 MPa
2470 psi
steel collar and pin shear; ISO 10123
Permabond HH131 High Temperature Threadlocker
Permabond® HH131 is a very high temperature resistant, high strength anaerobic threadlocker and sealant. This material cures in the absence of air between tight fitting metal parts. It is used for ..
Adhesive Bond Strength 17.0 MPa
2470 psi
steel collar and pin shear; ISO 10123
Permabond HM118 Anaerobic Threadlocker
Permabond® HM118 Threadlocker is an excellent general-purpose threadlocker and sealant. It is used for locking bolts, nuts and screws that require permanent assembly. Cure is fast and reliable on s..
Adhesive Bond Strength 17.0 MPa
2470 psi
steel collar and pin shear; ISO 10123
Permabond HM128 Anaerobic Threadlocker
Permabond® HM128 Threadlocker is a high strength adhesive for permanent assembly. It is typically used for preventing vibration loosening of bolts, studs and cap screws. Full cure to a cross-linked..
Adhesive Bond Strength 17.0 MPa
2470 psi
steel collar and pin shear; ISO 10123
Permabond HM129 Anaerobic Threadlocker
Permabond® HM129 is a high strength medium viscosity anaerobic threadlocker and sealant. This material cures in the absence of air between tight fitting metal parts. Cure is fast and reliable on st..
Adhesive Bond Strength 17.0 - 31.0 MPa
2470 - 4500 psi
Aluminum, Shear; ASTM D1002
Permabond ES569 Epoxy Resin
PERMABOND® ES569 is a single-part heat cured epoxy adhesive with excellent adhesion to metal surfaces as well as composite materials. The high bond strength of this adhesive allows it to replace me..
Adhesive Bond Strength 17.0 - 20.0 MPa
2470 - 2900 psi
Zinc, Shear
Permabond ET538 Epoxy Resin
PERMABOND ET538 is a structural, room temperature curing epoxy adhesive that has excellent adhesion to a wide variety of surfaces such as wood, metal, ceramics and many plastic and composite materia..
Adhesive Bond Strength 17.0 MPa
2470 psi
steel collar and pin shear; ISO 10123
Permabond A1044 Anaerobic Threadsealant
Permabond® A1044 is a rapid curing sealant designed to lock and seal metal pipe connections, offering very good resistance to even the most aggressive chemicals. Permabond A1044 can be used to seal..