Polymer Property : Adhesive Bond Strength = 20.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 16.0 - 20.0 MPa
2320 - 2900 psi
Steel, Shear; ISO 4587
Permabond 2050 Cyanoacrylate, flexible
PERMABOND® 2050 is a flexible cyanoacrylate adhesive, exhibiting improved peel strengths when compared to other grades. It has excellent impact and vibration resistance, and is suitable for bonding..
Adhesive Bond Strength 16.0 - 20.0 MPa
2320 - 2900 psi
Steel, Shear; ISO 4587
Permabond 940 Cyanoacrylate, low odor
PERMABOND 940 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad..
Adhesive Bond Strength 10.0 - 20.0 MPa
1450 - 2900 psi
steel collar and pin shear; ISO 10123
Permabond HL126 Anaerobic Threadlocker
PERMABOND® HL126 Threadlocker is a water thin product for locking pre-assembled parts through wicking action. PERMABOND® HL126 Threadlocker prevents vibration loosening. Because of the low viscosi..
Adhesive Bond Strength 14.0 - 20.0 MPa
2030 - 2900 psi
Mild steel, Shear
Permabond TA437 Toughened Acrylic Adhesive
PERMABOND TA437 is a single component structural acrylic adhesive designed primarily for bonding metals, ferrites and ceramics. The typical fixture time of TA437 when used with Initiator 41 is 30 –..
Adhesive Bond Strength 15.0 - 20.0 MPa
2180 - 2900 psi
Zinc, Shear
Permabond TA4592 Toughened Acrylic Adhesive
PERMABOND® TA4592 is a two component structural acrylic adhesive ideal for bonding magnets and ferrites for electric motors on fast-moving production lines. Permabond® TA4592 provides high strengt..
Adhesive Bond Strength 17.0 - 20.0 MPa
2470 - 2900 psi
Zinc, Shear
Permabond ET538 Epoxy Resin
PERMABOND ET538 is a structural, room temperature curing epoxy adhesive that has excellent adhesion to a wide variety of surfaces such as wood, metal, ceramics and many plastic and composite materia..
Adhesive Bond Strength 18.0 - 20.0 MPa
2610 - 2900 psi
Mild steel, Shear
Permabond ET538 Epoxy Resin
PERMABOND ET538 is a structural, room temperature curing epoxy adhesive that has excellent adhesion to a wide variety of surfaces such as wood, metal, ceramics and many plastic and composite materia..
Adhesive Bond Strength 16.0 - 20.0 MPa
2320 - 2900 psi
Steel, Shear; ISO 4587
Permabond 941 Cyanoacrylate, low odor
PERMABOND 941 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad..
Adhesive Bond Strength 16.0 - 20.0 MPa
2320 - 2900 psi
Steel, Shear; ISO 4587
Permabond 943 Cyanoacrylate, low odor
PERMABOND 943 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad..
Adhesive Bond Strength 18.0 - 20.0 MPa
2610 - 2900 psi
Mild steel, Shear
Permabond ET514 Epoxy Resin
PERMABOND ET514 is a 1:1 mixable epoxy adhesive. It has excellent resistance to impact and vibration and is ideal for structural bonding of metal, wood, composites and certain plastics. Its rapid cu..
Adhesive Bond Strength 16.0 - 20.0 MPa
2320 - 2900 psi
Steel, Shear; ISO 4587
Permabond 947 Cyanoacrylate, low odor
PERMABOND 947 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad..
Adhesive Bond Strength 10.0 - 20.0 MPa
1450 - 2900 psi
steel collar and pin shear; ISO 10123
Permabond A126 Anaerobic Retainer
Permabond® A126 is a high-strength anaerobic adhesive for permanent assembly of coaxial assemblies or threaded metal components. The exceptionally low viscosity of this product makes it ideal for u..