Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Adhesive Bond Strength = 200 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 1.38 MPa
200 psi
Polystyrene, Substrate Failure, Shear; ASTM D1002
Permabond 930 Cyanoacrylate
PERMABOND 930 is a low odor, non­fogging, non­frosting cyanoacrylate. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate adhesives on hot and humid days, is eliminated. The ..
Adhesive Bond Strength 1.38 MPa
200 psi
Polystyrene, Substrate Failure, Shear; ASTM D1002
Permabond 931 Cyanoacrylate
PERMABOND 931 is a low odor, non­fogging, non­frosting cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate adhesiv..
Adhesive Bond Strength 1.38 MPa
200 psi
Polystyrene, Substrate Failure, Shear; ASTM D1002
Permabond 932 Cyanoacrylate
PERMABOND 932 is a low odor, non­fogging, non­frosting cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate adhesiv..
Adhesive Bond Strength 1.38 MPa
200 psi
Polystyrene, Substrate Failure, Shear; ASTM D1002
Permabond 935 Cyanoacrylate
The PERMABOND 930 series is a family of low odor, non-fogging, non-frosting cyanoacrylates. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyano..
Adhesive Bond Strength 1.38 MPa
200 psi
Typical lap shear
Momentive Performance Materials RTV106 Red Adhesive Sealant, High Strength, High Temperature Paste
One-part alkoxy cure. Typical uses: High-heat applications; encapsulate and seal heating elements.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of Momentive Performance..
Adhesive Bond Strength 1.38 MPa
200 psi
Typical lap shear
Momentive Performance Materials RTV133 Black Adhesive Sealant, Flame Retardant Paste
One-part alkoxy cure. Typical uses: As a sealant on firewalls or as a flame retardant coating. Use in switching devices, motors, and high voltage transformers.Data provided by the manufacturer, GE..
Adhesive Bond Strength 1.38 MPa
200 psi
Typical lap shear
Momentive Performance Materials RTV1473 Black Adhesive Sealant, FIPG
One-part acetoxy cure. Typical uses: Heavy bodied adhesive sealant for formed-in-place gasketing. Good oil resistance.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of ..
Adhesive Bond Strength 1.38 MPa
200 psi
Typical lap shear
Momentive Performance Materials RTV167 Gray Adhesive Sealant, Non-Corrosive High Strength
One-part totally non-corrosive alkoxy cure. Alkoxy cure silicones are neutral cure materials that offer exceptional adhesion and are non-corrosive to most metals. Typical uses: Highest strength ad..
Adhesive Bond Strength 1.38 MPa
200 psi
Typical lap shear
Momentive Performance Materials FRV1106 Red Fluorosilicone Adhesive Sealant, Fuel Resistant Paste
One-part acetoxy cure. Alkoxy cure silicones are neutral cure materials that offer exceptional adhesion and are non-corrosive to most metals. Typical uses: For use in contact with fuel, solvents, ..
Adhesive Bond Strength 1.38 MPa
200 psi
Typical lap shear
Momentive Performance Materials FRV1107 Gray Adhesive Sealant, Fuel Resistant Paste
One-part acetoxy cure. Typical uses: For use in contact with fuel, solvents, and chemicals.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of Momentive Performance Materi..
Adhesive Bond Strength 1.38 MPa
200 psi
Typical lap shear
Momentive Performance Materials IS806 Red Adhesive Sealant, General Purpose Paste
One-part alkoxy cure. Typical uses: High-heat applications; encapsulate and seal heating elements.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of Momentive Performance..
Adhesive Bond Strength 1.38 MPa
200 psi
Lap shear, alum to alum
Tra-Con Tra-Bond 2106T Fast Cure Thixotropic Epoxy Adhesive
TRA-BOND 2106T is an exceptional epoxy formulation recommended for lower temperature or wet industrial bonding applications where FAST CURING is required. This versatile two-part epoxy system contai..
Adhesive Bond Strength 1.38 MPa
200 psi
Al-to-Al Lap Shear; Cured property, scuff sanded, IPA wiped T3-202Al; cohesive failure; ASTM D1002
Aptek 2312-PMF Electrically conductive, low modulus adhesive
Premixed-frozen, electrically conductive, low modulus adhesiveAPTEK 2312-PMF is a one component, premixed-frozen, silver filled, electrically conductive soft paste adhesive. It is designed to bond m..
Adhesive Bond Strength 1.38 MPa
200 psi
Atom Adhesives AA-BOND 201 Epoxy Adhesive
AA-BOND 201 is an exceptional epoxy formulation recommended for lower temperature or wet industrial bonding applications where FAST CURING is required. AA-BOND 201 is versatile two-part epoxy system..
Copyright © lookpolymers.com All Rights Reserved