Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Adhesive Bond Strength = 27.6 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 27.6 MPa
4000 psi
steel/steel
Resinlab® AR 4305 Metal Bonding Methacrylate Adhesive
Resinlab™ AR 4305 is a 1:1 mix methacrylate-based structural adhesive designed for general purpose bonding of a wide variety of materials in industrial applications. AR 4305 forms tough, durable bo..
Adhesive Bond Strength 27.6 MPa
4000 psi
Steel lap shear
Resinlab® CYNERGY CA6101 Adhesive
Description: The CYNERGY 6100 SERIES products are used to bond metal to itself or other substrates. It is available in five standard viscosities.Application: The CYNERGY SERIES of the cyanoacrylates..
Adhesive Bond Strength 27.6 MPa
4000 psi
Steel lap shear
Resinlab® CYNERGY CA6103 Adhesive
Description: The CYNERGY 6100 SERIES products are used to bond metal to itself or other substrates. It is available in five standard viscosities.Application: The CYNERGY SERIES of the cyanoacrylates..
Adhesive Bond Strength 27.6 MPa
4000 psi
Steel lap shear
Resinlab® CYNERGY CA6104 Adhesive
Description: The CYNERGY 6100 SERIES products are used to bond metal to itself or other substrates. It is available in five standard viscosities.Application: The CYNERGY SERIES of the cyanoacrylates..
Adhesive Bond Strength 27.6 MPa
4000 psi
Steel lap shear
Resinlab® CYNERGY CA6105 Adhesive
Description: The CYNERGY 6100 SERIES products are used to bond metal to itself or other substrates. It is available in five standard viscosities.Application: The CYNERGY SERIES of the cyanoacrylates..
Adhesive Bond Strength 27.6 MPa
4000 psi
steel/steel
Resinlab® AR 4305 HP Metal Bonding Methacrylate Adhesive
Resinlab™ AR 4305 HP is a 1:1 mix methacrylate-based structural adhesive designed for general purpose bonding of a wide variety of materials in industrial applications. AR 4305 HP forms tough, dur..
Adhesive Bond Strength 27.6 MPa
4000 psi
steel/steel
Resinlab® AR 4305 White Metal Bonding Methacrylate Adhesive
Resinlab™ AR 4305 White is a 1:1 mix methacrylate-based structural adhesive designed for general purpose bonding of a wide variety of materials in industrial applications. AR 4305 White forms tough..
Adhesive Bond Strength 27.6 MPa
4000 psi
steel/steel
Resinlab® AR 4315 HP Metal Bonding Methacrylate Adhesive
Resinlab™ AR 4315 HP is a 1:1 mix methacrylate-based structural adhesive formulated to bond almost all engineered thermoplastics, thermosets, composites, and metal structural elements together in a..
Adhesive Bond Strength 27.6 MPa
4000 psi
Steel lap shear
Resinlab® CYNERGY CA6102 Adhesive
Description: The CYNERGY 6100 SERIES products are used to bond metal to itself or other substrates. It is available in five standard viscosities.Application: The CYNERGY SERIES of the cyanoacrylates..
Adhesive Bond Strength >= 27.6 MPa
>= 4000 psi
tensile lap shear, Al to Al
Master Bond FLM36 B-staged film for high performance bonding and sealing
Master Bond FLM36 is a film adhesive with exceptional strength properties, high temperature resistance and first class thermal conductivity and electrical insulation properties. Based on the Master ..
Adhesive Bond Strength 27.6 MPa
4000 psi
Lap shear, alum to alum
Tra-Con Tra-Bond 221U01 Electrically Insulating Epoxy Encapsulant
TRA-BOND 221U01 is an electrically insulating, non-sagging epoxy encapsulant formulated to provide a smooth crown over the device of wire bonds. This encapsulant provides protection from thermal and..
Adhesive Bond Strength 27.6 MPa
4000 psi
Lap shear, gold to gold
Tra-Con Tra-Bond 293-1 General Purpose Instrument Epoxy Adhesive
TRA-BOND 293-1 general purpose epoxy adhesive is designed to provide strong, resilient bonds to a variety of difficult-to-bond substrates, such as gold, nickel, silver, copper, and brass. The 293-se..
Adhesive Bond Strength 27.6 MPa
4000 psi
Lap shear, brass to brass
Tra-Con Tra-Bond 293-1 General Purpose Instrument Epoxy Adhesive
TRA-BOND 293-1 general purpose epoxy adhesive is designed to provide strong, resilient bonds to a variety of difficult-to-bond substrates, such as gold, nickel, silver, copper, and brass. The 293-se..
Adhesive Bond Strength 27.6 MPa
4000 psi
Lap shear, gold to gold
Tra-Con Tra-Bond 293-1.5T General Purpose Instrument Epoxy Adhesive-Flexible
TRA-BOND 293-1.5T general purpose epoxy adhesive is designed to provide strong, semi-rigid bonds to a variety of difficult-to-bond substrates, such as gold, nickel, silver, copper, and brass. This v..
Adhesive Bond Strength 27.6 MPa
4000 psi
Lap shear, brass to brass
Tra-Con Tra-Bond 293-1.5T General Purpose Instrument Epoxy Adhesive-Flexible
TRA-BOND 293-1.5T general purpose epoxy adhesive is designed to provide strong, semi-rigid bonds to a variety of difficult-to-bond substrates, such as gold, nickel, silver, copper, and brass. This v..
Adhesive Bond Strength 27.6 MPa
4000 psi
Lap shear, gold to gold
Tra-Con Tra-Bond 293-1M General Purpose Instrument Epoxy Adhesive
TRA-BOND 293-1M general purpose epoxy adhesive is designed to provide strong, resilient bonds to a variety of difficult-to-bond substrates, such as gold, nickel, silver, copper and brass. The 293-se..
Adhesive Bond Strength 27.6 MPa
4000 psi
Lap shear, alum to alum, 2 hrs @ 65°C
Tra-Con Tra-Bond F113 High Impact Optically Clear Epoxy Adhesive
TRA-BOND F113 is an optically clear, low viscosity, high impact epoxy adhesive developed for bonding and small volume potting of plastic or glass optical fibers, lenses, and prisms, LED displays, an..
Adhesive Bond Strength 27.6 MPa
4000 psi
Lap shear, gold to gold
Tra-Con Tra-Bond 293-1T General Purpose Instrument Epoxy Adhesive-Thixotropic
TRA-BOND 293-1T general purpose epoxy adhesive is designed to provide strong, semi-rigid bonds to a variety of difficult-to-bond substrates, such as gold, nickel, silver, copper, and brass. This ver..
Adhesive Bond Strength 27.6 MPa
4000 psi
Lap shear, brass to brass
Tra-Con Tra-Bond 293-1T General Purpose Instrument Epoxy Adhesive-Thixotropic
TRA-BOND 293-1T general purpose epoxy adhesive is designed to provide strong, semi-rigid bonds to a variety of difficult-to-bond substrates, such as gold, nickel, silver, copper, and brass. This ver..
Adhesive Bond Strength 27.6 MPa
4000 psi
Lap shear, alum to alum
Tra-Con Tra-Bond Ablebond 868-7 Thixotropic Epoxy Adhesive
Ablebond 868-7 flexible epoxy adhesive is a thixotropic version of the 868-series. This nonsag adhesive provides strong bonds to a variety of surfaces.Information provided by Tra-Con Inc.
Adhesive Bond Strength 27.6 MPa
4000 psi
Lap shear, alum to alum
Tra-Con Tra-Bond F109 Fiber Optic Epoxy Adhesive
TRA-BOND F109 is specially designed to be used in fiber optic connectors where connections must be made in high humidity environments. This two part, low viscosity epoxy remains at a constant viscos..
Adhesive Bond Strength 27.6 MPa
4000 psi
Steel/Steel; Varies with substrates
Loctite® 635 High Strength/Slow Cure Retaining Compound
RetainersLoctite Corporation, the pioneer of anaerobic adhesives, has applied this technology to create retaining compounds that increase the shear strength of cylindrical, non-threaded assemblies. ..
Adhesive Bond Strength 27.6 MPa
4000 psi
Steel/Steel; Varies with substrates
Loctite® 680 High Strength/High Viscosity Retaining Compound
RetainersLoctite Corporation, the pioneer of anaerobic adhesives, has applied this technology to create retaining compounds that increase the shear strength of cylindrical, non-threaded assemblies. ..
Adhesive Bond Strength 27.6 MPa

@Temperature 25.0 °C
4000 psi

@Temperature 77.0 °F
Aluminum-Aluminum tensile shear
Armstrong A-40 Epoxy Adhesive
Is a high viscosity, dark gray, liquid adhesive system that is qualified under Mil. Spec. MMM-A-134, Type II. NOTE: Adhesives qualified under this Specification (A-40, A-706) feature exceptional re..
Adhesive Bond Strength 27.6 MPa

@Temperature 65.0 °C,
Time 7200 sec
4000 psi

@Temperature 149 °F,
Time 2.00 hour
Lap shear, alum to alum
Atom Adhesives AA-BOND F113 Epoxy Adhesive
AA-BOND F113 is an Optically Clear, low viscosity , High impact epoxy adhesives developed for bonding and small volume potting of plastic or glass optical fibers, lenses and prisms, LED displays, an..
Adhesive Bond Strength 27.6 MPa
4000 psi
Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37
Resinlab® EP1238 Acrylic / Epoxy Hybrid Adhesive
Resinlab™ EP1238 is a two part acrylic / epoxy hybrid adhesive designed for bonding metals and plastics. It cures quickly at room temperature to a tough, semi-rigid material. It has good wetting to..
Adhesive Bond Strength 27.6 MPa
4000 psi
Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37
Resinlab® EP1238 Black Acrylic / Epoxy Hybrid Adhesive
Resinlab™ EP1238 Black is a two part acrylic / epoxy hybrid adhesive designed for bonding metals and plastics. It cures quickly at room temperature to a tough, semi-rigid material. It has good wett..
Adhesive Bond Strength 27.6 MPa
4000 psi
Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37
Resinlab® EP1306 Acrylic / Epoxy Hybrid Adhesive
EP1306 is a two part acrylic / epoxy hybrid adhesive utilizing a 50% weight loading of aluminum powder into both components. It cures quickly at room temperature to a tough, rigid polymer. It has go..