| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Adhesive Bond Strength | 24.1 MPa | 3500 psi | alum/aluminum |
|
Resinlab® AR 4305 Metal Bonding Methacrylate Adhesive
Resinlab™ AR 4305 is a 1:1 mix methacrylate-based structural adhesive designed for general purpose bonding of a wide variety of materials in industrial applications. AR 4305 forms tough, durable bo..
|
|||
| Adhesive Bond Strength | 24.1 - 31.0 MPa | 3500 - 4500 psi | Steel, Shear; ASTM D1002 |
|
Permabond TA4810 Toughened Acrylic Adhesive
PERMABOND TA4810 is a 2-part, 1:1 toughened methacrylate adhesive designed for bonding thermoplastics, thermosets, metals and composites. TA4810 has excellent adhesion to as received metal surfac..
|
|||
| Adhesive Bond Strength | 24.1 - 31.0 MPa | 3500 - 4500 psi | Steel, Shear; ASTM D1002 |
|
Permabond TA4820 Structural Acrylic Adhesive
PERMABOND TA4820 is a 2-part, 1:1 toughened methacrylate adhesive designed for bonding thermoplastics, thermosets, metals and composites. TA4820 has excellent adhesion to as received metal surfac..
|
|||
| Adhesive Bond Strength | 24.1 MPa | 3500 psi | alum/aluminum |
|
Resinlab® AR 4305 HP Metal Bonding Methacrylate Adhesive
Resinlab™ AR 4305 HP is a 1:1 mix methacrylate-based structural adhesive designed for general purpose bonding of a wide variety of materials in industrial applications. AR 4305 HP forms tough, dur..
|
|||
| Adhesive Bond Strength | 24.1 MPa | 3500 psi | alum/aluminum |
|
Resinlab® AR 4305 White Metal Bonding Methacrylate Adhesive
Resinlab™ AR 4305 White is a 1:1 mix methacrylate-based structural adhesive designed for general purpose bonding of a wide variety of materials in industrial applications. AR 4305 White forms tough..
|
|||
| Adhesive Bond Strength | 24.1 MPa | 3500 psi | alum/aluminum |
|
Resinlab® AR 4315 HP Metal Bonding Methacrylate Adhesive
Resinlab™ AR 4315 HP is a 1:1 mix methacrylate-based structural adhesive formulated to bond almost all engineered thermoplastics, thermosets, composites, and metal structural elements together in a..
|
|||
| Adhesive Bond Strength | 24.1 MPa | 3500 psi | steel/steel |
|
Resinlab® AR 4340 HP Metal Bonding Methacrylate Adhesive
Resinlab™ AR 4340 HP is a 1:1 mix methacrylate-based structural adhesive designed for general purpose bonding of a wide variety of materials in industrial applications. It is an accelerated version..
|
|||
| Adhesive Bond Strength | 24.1 MPa | 3500 psi | steel/steel |
|
Resinlab® AR 4400 HP Metal & Composite Bonding Methacrylate Adhesive
Resinlab™ AR 4400 HP is a 1:1 mix methacrylate-based structural adhesive formulated to bond almost all engineered thermoplastics, thermosets, composites, and metal structural elements together in a..
|
|||
| Adhesive Bond Strength | 24.1 MPa | 3500 psi | lap shear (on grit blasted steel, bond line thickness of 0.010"); ASTM D1002 |
|
ITW Devcon Plastic Welderâ„¢ Methacrylate Adhesive, Straw, White, Black
Information provided by ITW Devcon
|
|||
| Adhesive Bond Strength | 24.1 MPa | 3500 psi | Lap shear, alum to alum |
|
Tra-Con Tra-Bond 2111 Rigid Epoxy Staking Compound
TRA-BOND 2111 is a thixotropic epoxy resin and hardener formulation developed for industrial adhesive, staking, laminating, repair and manufacturing applications where long pot-life, good wetting, n..
|
|||
| Adhesive Bond Strength | 24.1 MPa | 3500 psi | Lap shear, alum to alum, 4 hrs @ 65°C |
|
Tra-Con Tra-Bond 716C01 Medium Viscosity Epoxy Adhesive
TRA-BOND 716C01 is a medium viscosity epoxy resin system specifically developed for bonding and coating applications. This two-part amber adhesive is easily mixed, used and cured at room temperature..
|
|||
| Adhesive Bond Strength | 24.1 MPa | 3500 psi | Lap shear, alum to alum, 1 hr @ 65°C |
|
Tra-Con Tra-Bond 716K01 Radio Opaque Epoxy Adhesive
TRA-BOND 716K01 is a low viscosity epoxy resin system specifically developed for adhesive coating applications where radio opacity is required. This two part dark grey adhesive is commonly used for ..
|
|||
| Adhesive Bond Strength | 24.1 MPa | 3500 psi | Lap shear, alum to alum, @ 25°C |
|
Tra-Con Tra-Bond 931-1 Low Viscosity Encapsulant
TRA-BOND 931-1 low viscosity epoxy encapsulant is designed for high reliability applications, where capillary action is desired. This encapsulant provides environmental and mechanical protection.Inf..
|
|||
| Adhesive Bond Strength | 24.1 MPa | 3500 psi | Lap shear, alum to alum |
|
Tra-Con Tra-Bond FDA12 Food and Drug Application Epoxy Adhesive
TRA-BOND FDA12 is a medium viscosity epoxy resin system specifically developed for bonding and coating applications in accordance with Title 21, U.S. Code of Federal Regulations, Food and Drug Admin..
|
|||
| Adhesive Bond Strength | 24.1 MPa | 3500 psi | |
|
Trelleborg Emerson & Cuming Eccobond® 91 Two-Component High Strength-Peel Epoxy Adhesive
Emerson & Cuming 91 Eccobond® Two-Component High Strength-Peel Epoxy AdhesiveFiberglass filled, medium viscosity, epoxy adhesive with excellent thermal cycling properties. Used with a variety of ca..
|
|||
| Adhesive Bond Strength | 24.1 MPa | 3500 psi | Varies with substrates |
|
Loctite® 332 Severe Environment Structural Adhesive
Acrylic Bonding AdhesivesLoctite® Acrylic Adhesives were developed for bonding applications that require tensile, shear and peel strength combined with maximum impact, stress and shock resistance. ..
|
|||
| Adhesive Bond Strength | 24.1 MPa | 3500 psi | Lap shear, alum to alum |
|
Tra-Con Tra-Bond FDA12WH01 Food and Drug Application Epoxy Adhesive
TRA-BOND FDA12 WH01 is a medium viscosity epoxy resin system specifically developed for bonding and coating applications in accordance with Title 21, U.S. Code of Federal Regulations, Food and Drug ..
|
|||
| Adhesive Bond Strength | 24.1 MPa | 3500 psi | Grit blasted steel |
|
Loctite® Quick Set™ 404 Industrial Adhesive
Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-..
|
|||
| Adhesive Bond Strength | 24.1 MPa | 3500 psi | Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37 |
|
Resinlab® EP1026HP Epoxy Adhesive
Resinlab™ EP1026HP is a high performance fast setting epoxy adhesive designed for bonding metals, ceramics, glass and most plastics. This product gives good resistance to water salt spray, inorgan..
|
|||
| Adhesive Bond Strength | 24.1 MPa | 3500 psi | Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37 |
|
Resinlab® EP1056LV Black Urethane Modified Epoxy Casting Resin
Resinlab™ EP1056LV Black is a two part urethane modified epoxy casting resin designed to give good adhesion to metals and PVC. It has good wetting to most surfaces and is free-flowing to penetrate ..
|
|||
| Adhesive Bond Strength | 24.1 MPa | 3500 psi | Steel/Steel; Varies with substrates |
|
Loctite® 661 Retaining Compound
RetainersLoctite Corporation, the pioneer of anaerobic adhesives, has applied this technology to create retaining compounds that increase the shear strength of cylindrical, non-threaded assemblies. ..
|
|||
| Adhesive Bond Strength | 24.1 MPa | 3500 psi | Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37 |
|
Resinlab® EP1056LC Urethane Modified Epoxy Adhesive
Resinlab™ EP1056LC is a two part urethane modified epoxy adhesive designed to give good adhesion to metals and hard to bond surfaces such as PVC. It is thixotropic to provide good gap filling abili..
|
|||