| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| 300% Modulus | 0.00400 GPa | 0.580 ksi | ISO/R527 |
|
Polykemi AB POLYelast TPE Z700 Thermoplastic Elastomer, SEBS-based
Information provided by Polykemi AB
|
|||
| 300% Modulus | 0.00400 GPa | 0.580 ksi | ISO/R527 |
|
Polykemi AB POLYelast TPE Z706 Thermoplastic Elastomer, SEBS-based
Information provided by Polykemi AB
|
|||
| 300% Modulus | 0.00400 GPa | 0.580 ksi | ISO/R527 |
|
Polykemi AB POLYelast TPE Z706EX Thermoplastic Elastomer, SEBS-based
Information provided by Polykemi AB
|
|||
| 300% Modulus | 0.00400 GPa | 0.580 ksi | ASTM D412 |
|
Polimeri Europa Europrene® SOL TH 2314 Styrene - Ethylene / Butylene Block Copolymer
Europrene® SOL TH 2314 is a linear block copolymer obtained by selective hydrogenation of styrene-butadiene-styrene block copolymers. The polymer is based on styrene and ethylene/butylene, where b..
|
|||
| 300% Modulus | 0.00400 GPa | 0.580 ksi | ISO/R527 |
|
Polykemi AB POLYelast TPE ZSB60650 Thermoplastic Elastomer, SEBS/SBS-based, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| 300% Modulus | 0.00400 GPa | 0.580 ksi | Injection molded parts; DIN 53504 |
|
Huntsman IROGRAN® CA116-203 TPU-Polyester
Introduction: IROGRAN CA116-203 is a high performance polyester based thermoplastic polyurethane intended for flat die extrusion applications. IROGRAN CA116-203 is part of the HUNTSMAN film and shee..
|
|||
| 300% Modulus | 0.00400 GPa | 0.580 ksi | Injection molded parts; DIN 53504 |
|
Huntsman IROGRAN® CA116-205 TPU-Polyester
Introduction: IROGRAN CA116-205 is a high performance polyester based thermoplastic polyurethane intended for flat die extrusion applications. IROGRAN CA116-205 is part of the HUNTSMAN film and shee..
|
|||
| 300% Modulus | 0.00400 GPa | 0.580 ksi | ISO 37 |
|
Huntsman AVALON® 65 AC Thermoplastic Polyurethane
Introduction: AVALON 65 AC is a polyester based thermoplastic polyurethane for injection molding. AVALON 65 AC is part of the AVALON Crystal Range and offers a specially designed transparent materia..
|
|||
| 300% Modulus | 0.00400 GPa | 0.580 ksi | ISO 37 |
|
Huntsman AVALON® 65 AE Thermoplastic Polyurethane
Introduction: AVALON 65 AE is a polyester based thermoplastic polyurethane for injection molding. AVALON 65 AE is part of the AVALON Soft Range and offers a premium soling material for casual, sport..
|
|||
| 300% Modulus | 0.00400 GPa | 0.580 ksi | ASTM D412 |
|
Lubrizol Advanced Materials PEARLCOAT® DIPP-119 Thermoplastic Polyurethane Elastomer
PEARLCOAT® DIPP-119 is polycaprolactone copolyester based thermoplastic polyurethane, supplied in form of translucent pellets. Featuring low melting point and excellent transparency, this product..
|
|||
| 300% Modulus | 0.00400 GPa | 0.580 ksi | |
|
Taiwan PU Corporation UR60 Polyester Urethane Rubber
UR60 is a polyester urethane rubber which is an easy to process millable gum especially developed for improved compounding and processing benefits. It can be processed and compounded by the use of ..
|
|||
| 300% Modulus | 0.00400 GPa | 0.580 ksi | ASTM D638 |
|
ELASTO UK Dryflex® 400701S SBS Based Material, 70A Hardness, Natural
The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for..
|
|||
| 300% Modulus | 0.00400 GPa | 0.580 ksi | ASTM D638 |
|
ELASTO UK Dryflex® 402701S SBS Based Material, 70A Hardness, Black
The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for..
|
|||
| 300% Modulus | 0.00400 GPa | 0.580 ksi | ASTM D638 |
|
ELASTO UK Dryflex® 500700S SEBS Based Material, Unfilled Qualities, 70A Hardness, Translucent
The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha..
|
|||
| 300% Modulus | 0.00400 GPa | 0.580 ksi | ASTM D638 |
|
ELASTO UK Dryflex® 502700S SEBS Based Material, Unfilled Qualities, 70A Hardness, Black
The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha..
|
|||
| 300% Modulus | 0.00400 GPa | 0.580 ksi | ASTM D638 |
|
ELASTO UK Dryflex® 600650S SEBS Based Material, Filled Qualities, 65A Hardness, Natural
The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material ..
|
|||
| 300% Modulus | 0.00400 GPa | 0.580 ksi | ASTM D638 |
|
ELASTO UK Dryflex® 600700S SEBS Based Material, Filled Qualities, 70A Hardness, Natural
The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material ..
|
|||
| 300% Modulus | 0.00400 GPa | 0.580 ksi | ASTM D638 |
|
ELASTO UK Dryflex® 600750S SEBS Based Material, Filled Qualities, 75A Hardness, Natural
The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material ..
|
|||
| 300% Modulus | 0.00400 GPa | 0.580 ksi | ASTM D638 |
|
ELASTO UK Dryflex® 602650S SEBS Based Material, Filled Qualities, 65A Hardness, Black
The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material ..
|
|||
| 300% Modulus | 0.00400 GPa | 0.580 ksi | ASTM D638 |
|
ELASTO UK Dryflex® 602700S SEBS Based Material, Filled Qualities, 70A Hardness, Black
The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material ..
|
|||
| 300% Modulus | 0.00400 GPa | 0.580 ksi | ASTM D638 |
|
ELASTO UK Dryflex® 602750S SEBS Based Material, Filled Qualities, 75A Hardness, Black
The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material ..
|
|||
| 300% Modulus | 0.00400 GPa | 0.580 ksi | ASTM D638 |
|
ELASTO UK Dryflex® 660650S SEBS Based Material, Semi-Filled Qualities, 65A Hardness, Natural
The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t..
|
|||
| 300% Modulus | 0.00400 GPa | 0.580 ksi | ASTM D638 |
|
ELASTO UK Dryflex® 660700S SEBS Based Material, Semi-Filled Qualities, 70A Hardness, Natural
The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t..
|
|||
| 300% Modulus | 0.00400 GPa | 0.580 ksi | ASTM D638 |
|
ELASTO UK Dryflex® 662650S SEBS Based Material, Semi-Filled Qualities, 65A Hardness, Black
The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t..
|
|||
| 300% Modulus | 0.00400 GPa | 0.580 ksi | ASTM D638 |
|
ELASTO UK Dryflex® 662700S SEBS Based Material, Semi-Filled Qualities, 70A Hardness, Black
The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t..
|
|||
| 300% Modulus | 0.00400 GPa | 0.580 ksi | ASTM D 638 |
|
API Megol AM T A SEBS Adhesion Modified Overmolding for Polar Polymers
Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as ..
|
|||