| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
|
SABIC Innovative Plastics LNP FARADEX WX94736 PBT
LNP* Faradex* WX94736 is a compound based on Polybutylene Terephalate resin containing Stainless Steel.
|
|||
| Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
|
SABIC Innovative Plastics LNP LUBRICOMP KCL34A Acetal Homopolymer
LNP* LUBRICOMP* KCL34A is a compound based on Acetal Homopolymer resin containing 15% PTFE, 20% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive.
|
|||
| Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
|
SABIC Innovative Plastics LNP LUBRICOMP KP004L Acetal Copoly (Asia Pacific)
LNP* Lubricomp* KP004L is a compound based on Acetal Copolymer resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated, Low Extractible.
|
|||
| Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
|
SABIC Innovative Plastics LNP Lubricomp KX99792 Acetal Copolymer
LNP* Lubricomp* KX99792 is a compound based on Acetal Copolymer resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the ..
|
|||
| Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
|
SABIC Innovative Plastics LNP LUBRICOMP ML003S PP
LNP* LUBRICOMP* ML003S is a compound based on Polypropylene resin containing 15% PTFE. Added features include: Heat Stabilized, Wear Resistant.
|
|||
| Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
|
SABIC Innovative Plastics LNP LUBRICOMP RFI12 PA 66
LNP* LUBRICOMP* RFI12 is a compound based on Nylon 66 resin containing 10% Glass Fiber, 2% Silicone. Added feature of this material is: Wear Resistant.
|
|||
| Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
|
SABIC Innovative Plastics LNP LUBRICOMP RFL32 PA 66
LNP* Lubricomp* RFL32 is a compound based on Nylon 66 containing 10% Glass Fiber, 15% PTFE. Added feature of this material includes: Wear Resistant.
|
|||
| Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
|
SABIC Innovative Plastics LNP LUBRICOMP RFN14 PA 66
LNP* LUBRICOMP* RFN14 is a compound based on Nylon 66 containing 20% Glass Fiber, 5% MOS2. Added features of this grade include: Wear Resistant.
|
|||
| Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
|
SABIC Innovative Plastics LNP LUBRICOMP RL004 PA 66
LNP* LUBRICOMP* RL004 is a copmpound based on Nylon 66 resin containing 20% PTFE. Added feature of this grade includes: Wear Resistant.
|
|||
| Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
|
SABIC Innovative Plastics LNP LUBRICOMP RP004 PA 66
LNP LUBRICOMP* RP004 is a compound based on Nylon 66 resin containing 20% PTFE/Silicone. Added features of this material include: Wear Resistant.
|
|||
| Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
|
SABIC Innovative Plastics LNP LUBRICOMP WFL33 PBT
LNP* LUBRICOMP* WFL33 is a compound based on PBT containing 15% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant.
|
|||
| Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
|
SABIC Innovative Plastics LNP LUBRILOY R2000A PA 66
LNP LUBRILOY* R2000A is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant.
|
|||
| Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
|
SABIC Innovative Plastics LNP STAT-KON KX96321 POM
LNP* STAT-KON* KX96321 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
|
|||
| Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
|
SABIC Innovative Plastics LNP STAT-KON RFD04 PA 66
LNP STAT-KON* RFD04 is a compound based on Nylon 66 resin containing 20% Glass Fiber. Added features of this material include: Electrically Conductive.
|
|||
| Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
|
SABIC Innovative Plastics LNP STAT-LOY 9X03508 PPO+PA66
LNP* STAT-LOY* 9X03508 is a compound based on PPO+PA66 resin containing Proprietary Filler(s). Added features of this material include: Antistatic, Flame Retardant, High Impact.
|
|||
| Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
|
SABIC Innovative Plastics LNP STAT-LOY AF3009 ABS (Asia Pacific)
LNP* Stat-loy* AF3009 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, Flame Retardant. Added features of this material include: Antistat, Flame Retardant.
|
|||
| Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
|
SABIC Innovative Plastics LNP THERMOCOMP KF002 Acetal Copolymer
LNP THERMOCOMP* KF002 is a compound based on Acetal Copolymer resin containing 10% Glass Fiber.
|
|||
| Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
|
SABIC Innovative Plastics LNP THERMOCOMP KZ002 Acetal
LNP* THERMOCOMP* KZ002 is a compound based on Acetal containing 10% Milled Glass.
|
|||
| Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
|
SABIC Innovative Plastics LNP THERMOCOMP MH0500C PP (Asia Pacific)
LNP* Thermocomp* MH0500C is a compound based on Polypropylene resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
|
|||
| Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
|
SABIC Innovative Plastics LNP Thermocomp OF004AER PPS
LNP* Thermocomp* OF004AER is a compound based on Polyphenylene Sulfide resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.This data was supplied by SA..
|
|||
| Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
|
SABIC Innovative Plastics LNP THERMOCOMP RF0029S PA 66 (Asia Pacific)
LNP* Thermocomp* RF0029S is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant, Heat Stabilized.
|
|||
| Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
|
SABIC Innovative Plastics LNP THERMOCOMP RF002ES PA 66
LNP THERMOCOMP* RF002ES is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized.
|
|||
| Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
|
SABIC Innovative Plastics LNP THERMOCOMP WFB62 PBT
LNP* THERMOCOMP* WFB62 is a compound based on PBT resin containing 10% Glass Fiber, 10% Glass Bead. Added feature of this grade is: Low Warpage.
|
|||
| Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
|
SABIC Innovative Plastics LNP THERMOCOMP ZFM62P PPE+PS
LNP* THERMOCOMP* ZFM62P is a compound based on PPE+PS resin containing 10% Glass Fiber, 30% Mical. Added features of this material include: Exceptional Processing.
|
|||
| Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
|
SABIC Innovative Plastics LNP LUBRICOMP KAL22M Acetal Copolymer
LNP LUBRICOMP* KAL22M is a compound based on Acetal Copolymer resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant.
|
|||
| Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
|
SABIC Innovative Plastics LNP LUBRICOMP LL004 PEEK
LNP LUBRICOMP* LL004 is a compound based on Polyetheretherketone resin containing 20% PTFE. Added feature of this material is: Wear Resistant.
|
|||
| Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
|
SABIC Innovative Plastics LNP LUBRICOMP LL004 PEEK (Asia Pacific)
LNP LUBRICOMP* LL004 is a compound based on Polyetheretherketone resin containing PTFE. Added features of this material include: Internally Lubricated.
|
|||
| Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
|
SABIC Innovative Plastics LNP LUBRICOMP QFL32 PA 6/10
LNP* LUBRICOMP* QFL32 is a compound based on Nylon 6/10 containing 10% Glass Fiber, 15% PTFE. Added features of this grade include: Wear Resistant.
|
|||
| Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
|
SABIC Innovative Plastics LNP THERMOCOMP MF004AS PP
LNP THERMOCOMP* MF004AS is a compound based on Polypropylene resin containing 20% Glass Fiber. Added features of this material include: Heat Stabilized.
|
|||
| Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
|
SABIC Innovative Plastics LNP THERMOCOMP KFB11 Acetal Copoly (Asia Pacific)
LNP* Thermocomp* KFB11 is a compound based on Acetal Copolymer resin containing Glass Fiber, Milled Glass. Added features of this material include: Low Warpage, Chemically Coupled.
|
|||