| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched |
2.67
J/cm @Temperature 23.0 °C |
5.00
ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
|
SABIC Innovative Plastics Cycolac® X15 ABS
Automotive. Very high heat resistance with high impact. UL94 HB rated. High gloss.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Izod Impact, Notched |
2.67
J/cm @Temperature 22.8 °C |
5.00
ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
|
Polymer Resources PPX-FR1 Modified-PPO, V-0 Flame Retardant
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-..
|
|||
| Izod Impact, Notched |
2.67
J/cm @Temperature 22.8 °C |
5.00
ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
|
Polymer Resources PPX-FR2-[color]-EN Modified-PPO, V-1 Flame Retardant, Extrusion Grade
Modified-Polyphenylene Oxide, V-1 Flame Retardant, 210F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte..
|
|||
| Izod Impact, Notched |
2.67
J/cm @Temperature 22.8 °C |
5.00
ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
|
Polymer Resources PPX-FR4 Modified-PPO, V-1 Flame Retardant
Modified-Polyphenylene Oxide, V-1 Flame Retardant, 185F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-..
|
|||
| Izod Impact, Notched |
2.67
J/cm @Temperature 22.8 °C |
5.00
ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
|
Polymer Resources PPX-FR5 Modified-PPO, V-0 Flame Retardant
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 225F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-..
|
|||
| Izod Impact, Notched |
2.67
J/cm @Temperature -17.8 °C |
5.00
ft-lb/in @Temperature 0.000 °F |
ASTM D256 |
|
Polymer Resources PPX-GP4-IM Modified-PPO, Impact Modified
Modified-Polyphenylene Oxide, Impact Modified, 210F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
|
|||
| Izod Impact, Notched |
2.67
J/cm @Thickness 6.35 mm |
5.00
ft-lb/in @Thickness 0.250 in |
ASTM D256 |
|
PTS Trilac® ABS-HH2000 High Impact ABS Resin
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Izod Impact, Notched |
2.67
J/cm @Thickness 6.35 mm |
5.00
ft-lb/in @Thickness 0.250 in |
ASTM D256 |
|
PTS Trilac® ABS-HS5500 High Impact ABS Resin
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Izod Impact, Notched |
2.67
J/cm @Thickness 3.18 mm, Temperature -20.0 °C |
5.00
ft-lb/in @Thickness 0.125 in, Temperature -4.00 °F |
Injection Molded; ASTM D256A |
|
PolyOne Edgetek® XT XT-100-BW01 Natural PC+PBT
(discontinued **)
EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen..
|
|||
| Izod Impact, Notched |
2.67
J/cm @Thickness 6.35 mm |
5.00
ft-lb/in @Thickness 0.250 in |
ASTM D256 |
|
PTS Trilac® ABS-HF5500 High Flow ABS Resin
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Izod Impact, Notched |
2.67
J/cm @Thickness 3.17 mm, Temperature -29.0 °C |
5.00
ft-lb/in @Thickness 0.125 in, Temperature -20.2 °F |
notch |
|
Kraton® G1657 + PA-6 blend (8/12/80)
Blending KRATON D and G polymers with PA significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A..
|
|||
| Izod Impact, Notched |
2.67
J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
5.00
ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
|
Techmer ES Plastiblend® ABS 7000
Availability: North AmericaForms: PelletsFeatures: Low GlossInformation provided by TP Composites, Inc.
|
|||
| Izod Impact, Notched |
2.67
J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
5.00
ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
|
Techmer ES Plastiblend® ABS GN005
Availability: North AmericaForms: PelletsFeatures: General PurposeAppearance: GreenInformation provided by TP Composites, Inc.
|
|||
| Izod Impact, Notched |
2.67
J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
5.00
ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
|
Techmer ES Elastoblend® PA6/6 IM 3757 HS L Nylon 66
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Fast Molding Cycle, High Flow, Heat Stabilized, Lubricant and Impact ModifiedProcessing Met..
|
|||
| Izod Impact, Notched |
2.67
J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
5.00
ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
|
Techmer ES Elastoblend® PA6/6 IM 3757 HS L Nylon 66
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Fast Molding Cycle, High Flow, Heat Stabilized, Lubricant and Impact ModifiedProcessing Met..
|
|||
| Izod Impact, Notched |
2.67
J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
5.00
ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
|
Techmer ES Luriblend® ABS TL2
Availability: North AmericaForms: PelletsAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc.
|
|||
| Izod Impact, Notched |
2.67
J/cm @Temperature 23.0 °C |
5.00
ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
|
SABIC Innovative Plastics Noryl PX1701 PPE+PS
This data was supplied by SABIC-IP for the Americas region.
|
|||
| Izod Impact, Notched |
2.67
J/cm @Temperature -30.0 °C |
5.00
ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
|
DuPont Surlyn® SG201U NC010 Supergloss Molding Alloy
Surlyn® SG201U is a modified ionomer resin for applications that require a high gloss, molded in color surface color surface finish directly from the mold. The material is weatherable, durable, an..
|
|||
| Izod Impact, Notched |
2.67
J/cm @Temperature 23.0 °C |
5.00
ft-lb/in @Temperature 73.4 °F |
ASTM D256A |
|
Formosa Plastics Formolene® 2306N Impact Copolymer Polypropylene
Impact Copolymer for Compression and Injection Molded Caps and Closures Formolene® 2306N is a polypropylene copolymer formulated for compression and injection molded cap applications. It was create..
|
|||
| Izod Impact, Notched |
2.67
J/cm @Thickness 6.35 mm |
5.00
ft-lb/in @Thickness 0.250 in |
|
|
TPI Porene® ABS-GA800 High Impact ABS Resin
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
|
|||
| Izod Impact, Notched |
2.67
J/cm @Thickness 3.17 mm |
5.00
ft-lb/in @Thickness 0.125 in |
|
|
TPI Porene® ABS-GA803 High Gloss, UV Resistant ABS Resin
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
|
|||
| Izod Impact, Notched |
2.67
J/cm @Thickness 6.35 mm |
5.00
ft-lb/in @Thickness 0.250 in |
|
|
TPI Porene® ABS-GA850 High Impact ABS Resin
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
|
|||
| Izod Impact, Notched |
2.67
J/cm @Temperature 0.000 °C |
5.00
ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
|
Dow AFFINITY™ SM 1300G Polyolefin Plastomer (POP)
AFFINITY™ SM 1300G is an ethylene alpha-olefin resin for Injection Molding is produced via INSITE™ Technology from Dow Plastics. The resin offers excellent performance in durable injection molded..
|
|||
| Izod Impact, Notched |
2.67
J/cm @Temperature 22.8 °C |
5.00
ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
|
Clariant ABS4500 ABS, High Impact
Data provided by Clariant Masterbatches
|
|||
| Izod Impact, Notched |
2.67
J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
5.00
ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
ASTM D-256 |
|
Axiall 7456 Rigid PVC, Extrusion
Georgia Gulf 7456 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: ToughnessWeatherabilityWeldabilityChemical ResistanceEase of Proces..
|
|||
| Izod Impact, Notched |
2.67
J/cm @Temperature -20.0 °C |
5.00
ft-lb/in @Temperature -4.00 °F |
ASTM D-256 |
|
Axiall SP-7008 Rigid PVC, Molding
Georgia Gulf SP-7008 is a rigid vinyl compound formulated for electrical fittings and molded parts requiring high impact strength and toughness.Information provided by Georgia GulfGeorgia Gulf becam..
|
|||
| Izod Impact, Notched |
2.67
J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
5.00
ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D-256 |
|
Axiall Suprel® 9422 Rigid PVC, Molding
Georgia Gulf Suprel® 9422 Alloy is engineered for injection molding applications that require outstanding impact resistance or toughness, particularly at low temperatures. This alloy complies with..
|
|||
| Izod Impact, Notched |
2.67
J/cm @Thickness 6.35 mm |
5.00
ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
|
Axiall ProTherm® 4345 Rigid PVC, Extrusion
Georgia Gulf ProTherm® 4345 is a CPVC powder blend designed for extrusion applications requiring high heat deflection temperatures. Processing and stability along with overall physical properties ..
|
|||
| Izod Impact, Notched |
2.67
J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
5.00
ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
|
Techmer ES Plastiblend® ABS 922 NAT
Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc.
|
|||
| Izod Impact, Notched |
2.67
J/cm @Temperature 23.0 °C |
5.00
ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
|
SABIC Innovative Plastics LNP Verton RX93407D PA 66