| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Stress |
2.90
MPa @Strain 300 % |
421
psi @Strain 300 % |
Flow; ISO 37 |
|
PolyOne OnFlex™ HT 50A-3S2099 Thermoplastic Elastomer (TPE)
OnFlex™ HT thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds is specially formulated to deliver very good compression set performance at..
|
|||
| Tensile Stress |
2.90
MPa @Strain 300 % |
421
psi @Strain 300 % |
ISO 37 |
|
PolyOne OnFlex™ S EF 60A-3S1967 Thermoplastic Elastomer (TPE)
OnFlex™-S EF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver good mechanical properties together with excell..
|
|||
| Tensile Stress |
2.90
MPa @Strain 300 % |
421
psi @Strain 300 % |
ASTM D412 |
|
Polymax® Maxelast® P2865 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
|
|||
| Tensile Stress |
2.90
MPa @Strain 300 %, Temperature 23.0 °C |
421
psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
|
PolyOne Dynaflex™ G7650-1 (Natural) Thermoplastic Elastomer (TPE)
Dynaflex™ G7650-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop..
|
|||
| Tensile Stress |
2.90
MPa @Strain 300 % |
420
psi @Strain 300 % |
ASTM D412 |
|
Teknor Apex Monprene® MP-1881B Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Tensile Stress |
2.90
MPa @Strain 300 % |
420
psi @Strain 300 % |
ASTM D412 |
|
Teknor Apex Telcar® TL-1522G Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
|
|||
| Tensile Stress |
2.90
MPa @Strain 6.00 %, Temperature 23.0 °C |
421
psi @Strain 6.00 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
|
DuPont Performance Polymers Hytrel® 4056 Polyester Elastomer TPC-ET
(Unverified Data**)
40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
|
|||
| Tensile Stress |
2.90
MPa @Strain 0.100 %, Temperature 200 °C |
421
psi @Strain 0.100 %, Temperature 392 °F |
DAM; ISO 11403-1/-2 |
|
DuPont Performance Polymers Zytel® PLUS PLS93G35DH1 BK261 Nylon 6
(Unverified Data**)
Zytel® PLS93G35DH1 BK261 is a 35% glass reinforced PA6 using SHIELD Technology, only from DuPont, it provides exceptional welding resistance & retention over time thanks to excellent Heat Resistanc..
|
|||
| Tensile Stress |
2.90
MPa @Strain 0.100 %, Temperature 0.000 °C |
421
psi @Strain 0.100 %, Temperature 32.0 °F |
50%RH; ISO 11403-1 -2 |
|
DuPont Performance Polymers Zytel® RS 3061HSL BK039A Nylon 610
(Unverified Data**)
Unreinforced Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3061HSL BK039A is a renewably sourced polyamide 610 resin containing a minimum of 60% renewably sourced ingredie..
|
|||
| Tensile Stress |
2.90
MPa @Strain 0.280 %, Temperature 23.0 °C |
421
psi @Strain 0.280 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 |
|
DuPont Performance Polymers Zytel® RS 3261TL NC010 Nylon 610
(Unverified Data**)
Toughened Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3261TL NC010 is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient by..
|
|||
| Tensile Stress |
2.90
MPa @Strain 38.83 %, Temperature 120 °C |
421
psi @Strain 38.83 %, Temperature 248 °F |
ISO 527 |
|
DuPont Performance Polymers Hytrel® G4078W TPC-ET
(Unverified Data**)
Hytrel® G4078W is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like inject..
|
|||
| Tensile Stress |
2.90
MPa @Strain 14.63 %, Temperature 90.0 °C |
421
psi @Strain 14.63 %, Temperature 194 °F |
ISO 527 |
|
DuPont Performance Polymers Hytrel® G4078W TPC-ET
(Unverified Data**)
Hytrel® G4078W is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like inject..
|
|||
| Tensile Stress |
2.90
MPa @Strain 300 % |
421
psi @Strain 300 % |
ISO 37 |
|
Alliance Polymers Viprene™ G44A-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G44A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
|
|||
| Tensile Stress |
2.90
MPa @Strain 100 % |
421
psi @Strain 100 % |
ISO 37 |
|
Alliance Polymers Viprene™ G75A-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G75A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
|
|||
| Tensile Stress |
2.90
MPa @Strain 100 % |
421
psi @Strain 100 % |
ISO 37 |
|
Alliance Polymers Viprene™ G75A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G75A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
|
|||
| Tensile Stress |
2.90
MPa @Strain 300 % |
421
psi @Strain 300 % |
ISO 37 |
|
Alliance Polymers Viprene™ G44A-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G44A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
|
|||