| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Strength | 86.9 MPa | 12600 psi | ASTM D-790 |
|
Plaskolite Optix® CP - 51 KC General Purpose Acrylic Resin
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli..
|
|||
| Flexural Strength | 86.9 MPa | 12600 psi | ASTM D-790 |
|
Plaskolite West Optix® CP - 51 KC General Purpose Acrylic Resin
Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av..
|
|||
| Flexural Strength | 87.0 MPa | 12600 psi | ISO 178 |
|
PTS POM-90 Acetal Copolymer
Information provided by PTS LLC.
|
|||
| Flexural Strength | 87.0 MPa | 12600 psi | ISO 178 |
|
NOVA Chemicals DYLARK® 238 Impact Grade Engineering Resin
Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn..
|
|||
| Flexural Strength | 87.0 MPa | 12600 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics LNP LUBRICOMP BX02715 SAN
LNP* LUBRICOMP* BX02715 is a compound based on SAN containing proprietary fillers. Added features of this grade include: Wear Resistant, Tight Dimensional Tolerance, Good for Water Meter Applicati..
|
|||
| Flexural Strength | 87.0 MPa | 12600 psi | ASTM D790 |
|
Kolon KOCETAL® LW701 Wear Modified Acetal Resin
Special polymer added, improved wear property. Applications: Products for low noise and precision gear. Information provided by API-Kolon.
|
|||
| Flexural Strength | 87.0 MPa | 12600 psi | ASTM D790 |
|
SABIC Innovative Plastics LNP LUBRILOY D20009 PC
LNP LUBRILOY* D20009 is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Flame Retardant, Wear Resistant.
|
|||
| Flexural Strength | 87.0 MPa | 12600 psi | ASTM D790 |
|
SABIC Innovative Plastics LNP LUBRILOY D20009 PC (Asia Pacific)
LNP LUBRILOY* D20009 is a compound based on Polycarbonate resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Flame Retardant.
|
|||
| Flexural Strength | 87.0 MPa | 12600 psi | ASTM D790 |
|
SABIC Innovative Plastics LNP LUBRILOY RA2 PA 66
LNP* LUBRILOY* RA2 is a compound based on Nylon 66 resin containing Aramid Fiber. Added feature of this material is: Wear Resistant.
|
|||
| Flexural Strength | 87.0 MPa | 12600 psi | ASTM D790 |
|
SABIC Innovative Plastics LNP STAT-KON DX93500 PC
LNP STAT-KON* DX93500 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
|
|||
| Flexural Strength | 87.0 MPa | 12600 psi | ISO 178 |
|
SABIC Innovative Plastics LNP THERMOCOMP MF741XXH PP
LNP* THERMOCOMP* MF741XXH is a compound based on Polypropylene reain containing Glass Fiber and proprietay antimicrobial additives. Designed for touch surfaces in patient critical healthcare applic..
|
|||
| Flexural Strength | 87.0 MPa | 12600 psi | ISO 178 |
|
SABIC Innovative Plastics LNP Thermocomp OX92080 PPS - LINEAR
LNP* Thermocomp* OX92080 is a compound based on Linear PPS containing Proprietary Fillers.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Flexural Strength | 87.0 MPa | 12600 psi | ASTM D 790 |
|
SABIC Innovative Plastics Noryl GTX CRN500 PPE+PA6 (Asia Pacific)
Pa6 based unfilled GTX for Non-Auto marketThis data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Flexural Strength | 87.0 MPa | 12600 psi | ISO 178 |
|
SABIC Innovative Plastics LNP THERMOCOMP 2F005 ETFE
LNP* Thermocomp* 2F005 is a fluoropolymer compound based on ETFE containing 25% Glass Fiber.
|
|||
| Flexural Strength | 86.9 MPa | 12600 psi | ASTM D790 |
|
Chase Plastics CP Pryme® N110GL (COND, 50% RH) Nylon 6, 10% Glass Fiber Reinforced, Internally Lubricated
Information provided by Chase Plastics.
|
|||
| Flexural Strength | 87.0 MPa | 12600 psi | ISO 178 |
|
Polyplastics Tepcon M130 Acetal-copolymer (POM), High Fluidity
Information provided by PolyPlastics.
|
|||
| Flexural Strength |
87.0
MPa <br>@Strain 3.50 %
|
12600
psi <br>@Strain 3.50 %
|
ISO 178 |
|
DuPont Performance Polymers Delrin® FG511DP NC010 Acetal (POM)
(Unverified Data**)
Nucleated Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for mo..
|
|||
| Flexural Strength | 87.0 MPa | 12600 psi | ASTM Test |
|
BASF Ultramid® 8253 HS PA6 (Dry)
Ultramid 8253 HS is a heat stabilized, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications requiring improved dry as molded toughness and increased..
|
|||
| Flexural Strength | 87.0 - 101 MPa | 12600 - 14600 psi | ASTM D790 |
|
3D Systems Accura® 60 Plastic for SLA® Systems
Simulate the properties and appearance of polycarbonate. For use with solid-state stereolithography (SLA®) systems.ApplicationsTough functional prototypesAutomotive design componentsConsumer electr..
|
|||
| Flexural Strength | 87.0 - 125 MPa | 12600 - 18100 psi | ASTM D790 |
|
3D Systems Accura® Amethyst™ Plastic for Viper™ SLA® Systems
Optimized for the rapid and automated production of patterns and master molds for jewelry manufacturing. For use with Viper™ SLA® systems.ApplicationsPatterns for use with low and high vulcanizing..
|
|||
| Flexural Strength | 86.9 MPa | 12600 psi | GB9341 |
|
Beijing Evergrow Resources Enylon®
Information provided by Beijing Evergrow Resources.
|
|||
| Flexural Strength |
87.0
MPa <br>@Strain 3.50 %,<br> Temperature 23.0 °C
|
12600
psi <br>@Strain 3.50 %,<br> Temperature 73.4 °F
|
ISO 178 |
|
DuPont Performance Polymers Delrin® 511DP NC010 Acetal Homopolymer
(Unverified Data**)
Delrin® 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided..
|
|||
| Flexural Strength | 87.0 MPa | 12600 psi | ISO 178 |
|
Ascend Performance Materials Vydyne® 22WSP Nylon 66, Weather Resistant, DAM
Vydyne® 25WSP is a black, weather resistant injection molding grade Nylon 66 resin. These resins offer a well-balanced combination of engineering properties characterized by high strength, rigidity..
|
|||
| Flexural Strength | 87.0 MPa | 12600 psi | ISO 178 |
|
Polyplastics Duracon® CP-15X Acetal Co-polymer (POM), Creep resistant, Creep resistant
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
|
|||
| Flexural Strength | 87.0 MPa | 12600 psi | ISO 178 |
|
Polyplastics Duracon® M140-44/M140S Acetal Co-polymer (POM), Standard, High flow
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
|
|||
| Flexural Strength | 87.0 MPa | 12600 psi | ISO 178 |
|
Polyplastics Duracon® M90-45 Acetal Co-polymer (POM), Weather resistance, General
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
|
|||
| Flexural Strength | 87.0 MPa | 12600 psi | ISO 178 |
|
Polyplastics Duracon® M90-71 Acetal Co-polymer (POM), Heat resistance
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
|
|||
| Flexural Strength | 87.0 MPa | 12600 psi | ISO 178 |
|
Ascend Performance Materials Vydyne® 25WSP Nylon 66, Dry as Molded
Vydyne® 25WSP is a black, weather-resistant injection-molding grade PA66 resin. This resin offers a well-balanced combination of engineering properties characterized by high strength, rigidity, goo..
|
|||
| Flexural Strength | 87.0 MPa | 12600 psi | ISO 178 |
|
Polyplastics Duracon® M90-44/M90S Acetal Co-polymer (POM), Standard, General