| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Strength | 120 - 140 MPa | 17400 - 20300 psi | Injection; ISO 178 |
|
Raschig Group 2567 AMC
Glass fiber-reinforced and inorganically filled polyester molding compound (UP) in various colors. Outstanding mechanical strength similar to BMC/SMC, very good electrical isolation properties and ..
|
|||
| Flexural Strength | 120 - 140 MPa | 17400 - 20300 psi | Injection and Compression; ISO 178 |
|
Raschig Group 3505 Epoxy
Glass-fiber reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. This product meets the allowed..
|
|||
| Flexural Strength | 120 - 140 MPa | 17400 - 20300 psi | Injection and Compression; ISO 178 |
|
Raschig Group 3535 Epoxy
Glass fiber-reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties adn dimensional stability even at high temperatures. Form: Low dust granulate pack..
|
|||
| Flexural Strength | 120 - 140 MPa | 17400 - 20300 psi | Injection and Compression; ISO 178 |
|
Raschig Group 3536 Epoxy
Glass-fiber reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. This product meets the allowed..
|
|||
| Flexural Strength | 100 - 140 MPa | 14500 - 20300 psi | Injection; ISO 178 |
|
Raschig Group 6502 DAIP Diallyl Phthalate (DAP), Cast, Mineral Filler
Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi..
|
|||
| Flexural Strength | 120 - 140 MPa | 17400 - 20300 psi | Injection and Compression; ISO 178 |
|
Raschig Group EPOXIDUR® 3581 S ZC EP Epoxy Molding Compound
Inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Very good sealing connection on ..
|
|||
| Flexural Strength | 110 - 140 MPa | 16000 - 20300 psi | Injection; ISO 178 |
|
Raschig Group MELOPLAS® 2500 MF
Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al..
|
|||
| Flexural Strength | 130 - 140 MPa | 18900 - 20300 psi | ASTM D790, ISO 178 |
|
EPICHEM Epilon G4-PC 20% GF Polycarbonate, 20% Glass Fiber
Characteristics: 20% glass fibre filled, excellent mechanical properties
|
|||
| Flexural Strength | 100 - 140 MPa | 14500 - 20300 psi | ISO 178 |
|
Bulk Molding Compounds tetra-DUR F 4308 Bulk Molding Compound
UL-licensedTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion protection), thermal stabilit..
|
|||
| Flexural Strength | 100 - 140 MPa | 14500 - 20300 psi | ISO 178 |
|
Bulk Molding Compounds tetra-DUR F 4401 Bulk Molding Compound
UL-licensed, general purpose productTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion prot..
|
|||
| Flexural Strength | 100 - 140 MPa | 14500 - 20300 psi | ISO 178 |
|
Bulk Molding Compounds tetra-DUR N 4303 Bulk Molding Compound
Mechanical high grade standard product.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion p..
|
|||
| Flexural Strength | 100 - 140 MPa | 14500 - 20300 psi | Injection; ISO 178 |
|
Raschig Group 5567 DAP Diallyl Phthalate (DAP), Cast, Mineral Filler
Glass-fiber reinforced diallyl phthalate molding compound free from halogens. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exc..
|
|||
| Flexural Strength | 110 - 140 MPa | 16000 - 20300 psi | Compression; ISO 178 |
|
Raschig Group DECAL® 152CL Phenolic
Glass-fiber and mineral reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meet..
|
|||
| Flexural Strength | 120 - 140 MPa | 17400 - 20300 psi | Compression; ISO 178 |
|
Raschig Group RALUPOL® 8605 UP Polyester
Glass fiber reinforced polyester molding compound. Resistant to hydrolysis. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU dire..
|
|||
| Flexural Strength | 120 - 140 MPa | 17400 - 20300 psi | Compression; ISO 178 |
|
Raschig Group RESINOL® 400 EPF Phenolic
Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets ..
|
|||