| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
|
PolyOne Geon™ Vinyl Rigid Molding M4825 Polyvinyl Chloride, Rigid (PVC, Rigid)
** NOTE: UL REGULATORY LISTING PENDINGInformation provided by PolyOne
|
|||
| Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
|
PolyOne LubriOne™ NN-000/10T-2S Black Polyamide 66 (Nylon 66)
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
|
|||
| Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
|
Oxford Polymers 20GF 20% Glass Fiber Reinforced ABS, Flame Retardant
20% Glass Fiber Reinforced ABS, Flame RetardantInformation provided by Oxford Polymers.
|
|||
| Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
|
Polymer Resources PC-GP1-[color]-LF Polycarbonate, General Purpose, Food Contact
Polycarbonate, General Purpose, Low FlowFeatures: • Food Contact AcceptableProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, ..
|
|||
| Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
|
Polymer Resources PC-UV1-D Polycarbonate, UV-stabilized, Low Flow
Polycarbonate, UV-stabilized, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Po..
|
|||
| Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
|
Polymer Resources PC-UV1-D-[color]-1 Polycarbonate, UV-stabilized, Low Flow with Mold Release
Polycarbonate, UV-stabilized, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat..
|
|||
| Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
|
Polymer Resources TP-FR2-[color]-WR Polybutylene Terephthalate, Flame Retardant, Wear Resistant
Polybutylene Terephthalate, Flame Retardant, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor..
|
|||
| Flexural Strength | 96.5 - 110 MPa | 14000 - 16000 psi | ASTM D790 |
|
Mar-Bal MB1000-10 Thermoset Polyester Composite Molding Compound
A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro..
|
|||
| Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
|
Techmer ES HiFill® ABS GF3 3% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 3% Filler by WeightInformation provided by TP Composites, Inc.
|
|||
| Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
|
Techmer ES Luriblend® PA6/12 01430 Nylon 612
Availability: North AmericaForms: PelletsAdditive: Molybdenum Disulfide LubricantFeatures: Lubricated, Low Friction and Good Wear ResistanceInformation provided by TP Composites, Inc.
|
|||
| Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
|
Techmer ES Plaslube® NY-1/TF/15 NAT PA66 |
|||
| Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
|
Techmer ES Plaslube® NY-1/TF/20 NAT PA66 |
|||
| Flexural Strength | 96.5 MPa | 14000 psi | ASTM D 790 |
|
Styrolution PS 1600 GPPS
Foam extrusion; Injection moldingGood balanced of strength, flow and heat resistanceFree of zinc and oil additivesInformation provided by Styrolution
|
|||
| Flexural Strength | 96.5 MPa | 14000 psi | Method I (3 point load), 2.0 mm/min; ASTM D790 |
|
Styron CALIBREâ„¢ 200-3 Polycarbonate Resin
Overview: CALIBREâ„¢ 200-3 polycarbonate resin is produced in compliance with the US Food and Drugs Administration (FDA) and EU food contact regulation. This resin provides excellent impact resis..
|
|||
| Flexural Strength | 96.5 MPa | 14000 psi | Method I (3 point load), 2.0 mm/min; ASTM D790 |
|
Styron CALIBREâ„¢ 2060-6 Polycarbonate Resin
Overview: CALIBRE™ 2060-6 polycarbonate resin is used in medical applications involving steam or ethylene oxide sterilization – through suitability for use in these applications is depende..
|
|||
| Flexural Strength | 96.5 MPa | 14000 psi | 0.125 in, injection molded, unannealed; ASTM D790 |
|
Styron EMERGEâ„¢ 4310-22 Polycarbonate
EMERGEâ„¢ PC 4310-22 advanced resin is high-performance polycarbonate resin offering high heat resistance, toughness, and superior flow. Applications: Consumer Electronics and Information Techn..
|
|||
| Flexural Strength | 96.5 MPa | 14000 psi | 0.125 in, injection molded, unannealed; ASTM D790 |
|
Styron EMERGEâ„¢ 4330-15 Polycarbonate
EMERGEâ„¢ PC 4330-15 advanced resin is a polycarbonate resin offering ultraviolet light stability, high heat resistance and maximum toughness. Applications: Consumer Electronics and Information..
|
|||
| Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
|
Styron CALIBREâ„¢ 201-15 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
|
|||
| Flexural Strength | 96.5 MPa | 14000 psi | Method I (3 point load), 2.0 mm/min; ASTM D790 |
|
Styron CALIBREâ„¢ 300-6 Polycarbonate Resin
Overview: CALIBREâ„¢ 300-6 polycarbonate resin offer exceptional impact resistance, heat distortion resistance, and optical clarity as high melt strength for blow molding and sheet applications. ..
|
|||
| Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
|
Styron CALIBREâ„¢ 302-06 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
|
|||
| Flexural Strength | 96.5 MPa | 14000 psi | 0.125 in, injection molded, unannealed; ASTM D790 |
|
Styron EMERGEâ„¢ 4310-15 Polycarbonate
EMERGEâ„¢ PC 4310-15 advanced resin is high-performance polycarbonate resin offering high heat resistance and maximum toughness. Applications: Consumer Electronics and Information Technology Eq..
|
|||
| Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
|
Chase Plastics CP Pryme® PC300RHF Polycarbonate, Recycled Content
Features: Good flowHigh rigidityGood toughnessHigh strengthLow viscosityGood mold releaseRecycled contentForm: PelletsInformation provided by Chase Plastics.
|
|||
| Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
|
Total PSC 529 Polystyrene
Polystyrene 529 is a medium flow crystal specially formulated for mar resistance. The easy to process crystal minimizes visual defects from ejection and automated part handling. Typical applications..
|
|||
| Flexural Strength | 96.5 MPa | 14000 psi | |
|
TriStar Ultracomp UC-300 Composite Bearing
Ultracomp UC-300 - Similar in construction to UC-200. Containing special fillers that reduce its coefficient of friction, UC-300 is designed to handle higher rotational and linear speeds.This family..
|
|||
| Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
|
Ensinger Hydex™ 301 Rigid Polyurethane (PU)
Hydex™ 301 is clear totally rigid polyurethane. It combines excellent clarity when polished with a broad range of chemical resistance and outstanding practical toughness.
|
|||
| Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
|
Entec Hylex® P1007L1 HB Polycarbonate
Available in North America Agency Ratings: FDA 21 CFR 177.1580 RoHS Compliant Form: Pellets Information provided by Entec
|
|||